Manufacturing method for isothermal evaporation casting process
    2.
    发明授权
    Manufacturing method for isothermal evaporation casting process 有权
    等温蒸发铸造工艺的制造方法

    公开(公告)号:US07648598B2

    公开(公告)日:2010-01-19

    申请号:US11584847

    申请日:2006-10-23

    CPC classification number: C22C19/007 C22C3/00 C22C23/00

    Abstract: A manufacturing method for an isothermal evaporation casting process is disclosed and to design the manufacturing method for the simple atmospheric casting. The present invention can melt the Mg—Ni alloy with the aspect of totally different melting points thereof, and the other elements can be added during melting simultaneously. Through the Mg—Ni alloy with a suitable weight ratio, the eutectic alloy of Mg/Mg2Ni and high purified γ-phase Mg2Ni can be made. Then adding other elements are to produce the composition of Mg/Ni/M. By way of the manufacturing method of the present invention, the melting equipment is simplified; and, through different manufacturing steps, the purposes of time-saving and low cost are reached; further that, a large amount of the eutectic alloy of Mg/Mg2Ni with different kinds of ratios of Mg, high purified γ-phase Mg2Ni, or the composition of Mg/Ni/M can be obtained.

    Abstract translation: 公开了一种等温蒸发铸造工艺的制造方法,并设计了简单大气铸造的制造方法。 本发明可以熔融Mg-Ni合金,其熔点完全不同,其它元素可以在熔融的同时加入。 通过合适重量比的Mg-Ni合金,可以制备Mg / Mg2Ni和高纯γ相Mg2Ni共晶合金。 然后添加其他元素是产生Mg / Ni / M的组成。 通过本发明的制造方法,简化了熔化设备; 通过不同的制造步骤,实现了节省时间和低成本的目的; 此外,可以获得大量的具有不同种类的Mg,高纯度γ相Mg2Ni比的Mg / Mg2Ni或Mg / Ni / M组成的共晶合金。

    HYDROGEN STORAGE DEVICE
    4.
    发明申请
    HYDROGEN STORAGE DEVICE 审中-公开
    氢储存装置

    公开(公告)号:US20120132545A1

    公开(公告)日:2012-05-31

    申请号:US13041446

    申请日:2011-03-07

    CPC classification number: F17C11/005 Y02E60/321

    Abstract: A hydrogen storage device includes a hydrogen storage can, at least one first partition, and at least one second partition. The hydrogen storage can defines a major axis. The at least one first partition is used to partition the space in the hydrogen storage can into at least one compartment. The at least one second partition includes a plurality of sub-compartments. The sub-compartments are arranged linearly in at least one row perpendicular to the major axis.

    Abstract translation: 氢存储装置包括氢存储罐,至少一个第一分区和至少一个第二分区。 储氢器可以限定长轴。 至少一个第一隔板用于将储氢罐中的空间分隔成至少一个隔间。 所述至少一个第二分隔件包括多个子隔室。 子隔间在垂直于长轴的至少一行中线性排列。

    Manufacturing method for isothermal evaporation casting process
    10.
    发明申请
    Manufacturing method for isothermal evaporation casting process 有权
    等温蒸发铸造工艺的制造方法

    公开(公告)号:US20080093046A1

    公开(公告)日:2008-04-24

    申请号:US11584847

    申请日:2006-10-23

    CPC classification number: C22C19/007 C22C3/00 C22C23/00

    Abstract: A manufacturing method for an isothermal evaporation casting process is disclosed and to design the manufacturing method for the simple atmospheric casting. The present invention can melt the Mg—Ni alloy with the aspect of totally different melting points thereof, and the other elements can be added during melting simultaneously. Through the Mg—Ni alloy with a suitable weight ratio, the eutectic alloy of Mg/Mg2Ni and high purified γ-phase Mg2Ni can be made. Then adding other elements are to produce the composition of Mg/Ni/M. By way of the manufacturing method of the present invention, the melting equipment is simplified; and, through different manufacturing steps, the purposes of time-saving and low cost are reached; further that, a large amount of the eutectic alloy of Mg/Mg2Ni with different kinds of ratios of Mg, high purified γ-phase Mg2Ni, or the composition of Mg/Ni/M can be obtained.

    Abstract translation: 公开了一种等温蒸发铸造工艺的制造方法,并设计了简单大气铸造的制造方法。 本发明可以熔融Mg-Ni合金,其熔点完全不同,其它元素可以在熔融的同时加入。 通过具有合适重量比的Mg-Ni合金,可以制备Mg / Mg 2 Ni和高纯度γ相Mg 2 Ni的共晶合金。 然后添加其他元素是产生Mg / Ni / M的组成。 通过本发明的制造方法,简化了熔化设备; 通过不同的制造步骤,实现了节省时间和低成本的目的; 此外,大量Mg / Mg 2 Ni的共晶合金与Mg,高纯度γ相Mg 2 Ni的比例不同,或组合物 的Mg / Ni / M。