摘要:
A nitrogen gas tank, a rotary pump and a mechanical booster pump are connected to a bonding vessel that constitutes a bonding apparatus for carrying out diffusion bonding, the apparatus further comprising a pressure sensor. A nitrogen gas atmosphere is formed inside the bonding vessel, and under control operations of a control circuit, a nitrogen introduction rate is controlled so that a pressure is substantially fixed at a predetermined pressure between 3-105 Pa. At such a state, under the action of a rod of a hydraulic cylinder, a second electrode is brought into proximity with a first electrode, so that ultimately, a first object to be bonded and a second object to be bonded on the first electrode are pressed. Further, current is applied through the first electrode and the second electrode with respect to the first object to be bonded and the second object to be bonded.
摘要:
A nitrogen gas tank, a rotary pump and a mechanical booster pump are connected to a bonding vessel that constitutes a bonding apparatus for carrying out diffusion bonding, the apparatus further comprising a pressure sensor. A nitrogen gas atmosphere is formed inside the bonding vessel, and under control operations of a control circuit, a nitrogen introduction rate is controlled so that a pressure is substantially fixed at a predetermined pressure between 3-105 Pa. At such a state, under the action of a rod of a hydraulic cylinder, a second electrode is brought into proximity with a first electrode, so that ultimately, a first object to be bonded and a second object to be bonded on the first electrode are pressed. Further, current is applied through the first electrode and the second electrode with respect to the first object to be bonded and the second object to be bonded.
摘要:
A voltage non-linearity type resistor and a process for the preparation of a voltage non-linearity type resistor wherein pre-sintering is effected at a temperature of no lower than 700.degree. C. with a basic composition including X mole % of ZnO and (100-X) mole % of Fe.sub.2 O.sub.3 (wherein 40.ltoreq.X.ltoreq.60), and sintering is then effected with the resulting pre-sintered body to which at least one of V.sub.2 O.sub.5, Bi.sub.2 O.sub.3, MgO, Al.sub.2 O.sub.3, MoO.sub.3, Sb.sub.2 O.sub.3, SiO.sub.2, NiO, SrO.sub.2 and PbO is further added in a proportion of 0.01-40% by weight.
摘要翻译:一种电压非线性型电阻器和用于制备电压非线性型电阻器的方法,其中预烧结在不低于700℃的温度下进行,其碱性组成包括X摩尔%的ZnO和( 100-X)摩尔%的Fe2O3(其中40≤X= 60),然后用所得的预烧结体进行烧结,其中V 2 O 5,Bi 2 O 3,MgO,Al 2 O 3,MoO 3,Sb 2 O 3中的至少一种 ,进一步以0.01-40重量%的比例加入SiO 2,NiO,SrO 2和PbO。
摘要:
A calcium sulfoaluminate clinker having a calcium sulfoaluminate compound 3CaO.3Al.sub.2 O.sub.3. CaSO.sub.4 as a main component, a Portland cement and a blast furnace granulated slag are mixed to produce cements which prevent the formation of efflorescence.
摘要翻译:具有磺酸铝酸钙化合物3CaO·3Al 2 O 3的磺硅铝酸钙熟料。 以CaSO4为主要成分,将波特兰水泥和高炉颗粒状矿渣混合制成防止形成风化的水泥。
摘要:
A fluid flow passage structure and a manufacturing method therefor are provided, in which fluid flow passages can be easily produced employing a simple structure and process, while also being suitable for reducing the weight thereof. Wire members having a predetermined pattern are disposed between a first block member and a second block member. Airtight and fluidtight hermetic fluid flow passages are formed between such members, by forming the first block member, the second block member, and the wire members together as an integral structure.
摘要:
A manufacturing method for a fluid pressure device and a fluid pressure device are provided, in which joints are diffusion bonded to a valve body. In the fluid pressure device, the joints are inserted into an inlet port and an outlet port formed in the valve body, and heating is performed to generate a temperature difference between the valve body and the joints, whereupon by diffusion bonding of the joints into a wall of the valve body in which the inlet port and the outlet port are formed, both members are bonded.
摘要:
A material for destroying concrete structures, rock formations and the like comprises a mixture of 20 to 80 parts by weight of coarse-grained quicklime adjusted to a particle size of from 88 to 3000 microns, and 20 to 80 parts by weight of cement. The cement may contain calcium sulfoaluminate as a hydraulic component, and a retardant may be added to the mixture to retard the hydration of the calcium sulfoaluminate. The material is blended with water and then injected into holes formed in the body to be destroyed, the material expanding as it hydrates to crack and fracture the body.
摘要:
A laminated structure is formed by stacking a first block member, an intermediate member, and a second block member together in this order, and then mutually joining each of the members. Further, by setting the elastic constant of the intermediate member to be greater than the elastic constants of the first block member and the second block member, deformation of grooves, which are formed in the first block member, is minimized.
摘要:
A laminated structure is formed by stacking a first block member, an intermediate member, and a second block member together in this order, and then mutually joining each of the members. Further, by setting the elastic constant of the intermediate member to be greater than the elastic constants of the first block member and the second block member, deformation of grooves, which are formed in the first block member, is minimized.
摘要:
A fluid flow passage structure and a manufacturing method therefor are provided, in which fluid flow passages can be easily produced employing a simple structure and process, while also being suitable for reducing the weight thereof. Wire members having a predetermined pattern are disposed between a first block member and a second block member. Airtight and fluidtight hermetic fluid flow passages are formed between such members, by forming the first block member, the second block member, and the wire members together as an integral structure.