METHOD FOR MANUFACTURING A BIOACTIVE GLASS CERAMIC MATERIAL
    8.
    发明申请
    METHOD FOR MANUFACTURING A BIOACTIVE GLASS CERAMIC MATERIAL 审中-公开
    生产玻璃陶瓷材料的方法

    公开(公告)号:US20090325775A1

    公开(公告)日:2009-12-31

    申请号:US12388095

    申请日:2009-02-18

    Applicant: Nan-Hui Yeh

    Inventor: Nan-Hui Yeh

    CPC classification number: C03C14/006 A61L27/10 C03C10/00 C03C12/00

    Abstract: A method for manufacturing a bioactive glass ceramic material is firstly to prepare a calcium phosphate series ceramic material and a nano-scaled titanium dioxide powder with a specific proportion of anatase type titanium dioxide structure. Then, the calcium phosphate series ceramic material and the nano-scaled titanium dioxide powder are mixed according to a specific proportion for obtaining a mixture. The mixture is then melted and quenched to form a biomedical glass. Finally, the biomedical glass can be further ground into a biomedical glass powder, and a heat treatment can be applied to recrystalize the powder so as to obtain the bioactive glass ceramic material. Also, the bioactive glass ceramic material can be further polarized into a electrified bioactive glass ceramic material which can promote the growth of a broken bone.

    Abstract translation: 一种制备生物活性玻璃陶瓷材料的方法首先是制备一种具有特定比例的锐钛矿型二氧化钛结构的磷酸钙系陶瓷材料和纳米级二氧化钛粉末。 然后,根据特定比例将磷酸钙系陶瓷材料和纳米级二氧化钛粉末混合以获得混合物。 然后将混合物熔化并骤冷以形成生物医学玻璃。 最后,生物医学玻璃可以进一步研磨成生物医学玻璃粉末,并且可以进行热处理以使粉末重结晶,从而获得生物活性玻璃陶瓷材料。 此外,生物活性玻璃陶瓷材料可以进一步极化成带电的生物活性玻璃陶瓷材料,其可以促进破骨的生长。

Patent Agency Ranking