CPC分类号: C22C26/00 , B22F7/02 , C04B35/5831 , C04B35/6261 , C04B35/62675 , C04B35/62685 , C04B35/6303 , C04B35/645 , C04B37/026 , C04B41/009 , C04B41/4529 , C04B41/81 , C04B2235/3217 , C04B2235/3804 , C04B2235/3813 , C04B2235/3843 , C04B2235/3847 , C04B2235/3852 , C04B2235/3856 , C04B2235/3865 , C04B2235/3886 , C04B2235/402 , C04B2235/5436 , C04B2235/5445 , C04B2235/5472 , C04B2235/72 , C04B2235/785 , C04B2235/786 , C04B2235/80 , C04B2235/85 , C04B2235/96 , C04B2235/9607 , C04B2237/361 , C04B2237/401 , C22C2026/003 , Y10T428/24975 , Y10T428/25 , Y10T428/265 , C04B41/5061 , C04B41/5068 , C04B41/5062 , C04B41/5063 , C04B41/5066
摘要: A coated cBN sintered body has excellent wear resistance, fracture resistance, adhesiveness between a substrate and a coating, and a tool life of which is elongated as compared with conventional cBN sintered bodies. The coated cBN sintered body has a cBN sintered body substrate and a coating coated on the surface thereof. The cBN sintered body includes 76 to 90% by volume of cBN, and 10 to 24% by volume of a binder phase and inevitable impurities. An average grain size of cBN is 0.5 to 5.0 μm, an average value of the thickness of the binder phase is 0.05 to 0.8 μm, and the standard deviation of the thickness of the binder phase is 0.8 μm or less.
摘要翻译: 涂布的cBN烧结体与传统的cBN烧结体相比具有优异的耐磨性,耐断裂性,基材与涂层之间的粘合性,并且其寿命延长。 涂布的cBN烧结体具有cBN烧结体基材和涂布在其表面上的涂层。 cBN烧结体包含76〜90体积%的cBN,10〜24体积%的粘结相和不可避免的杂质。 cBN的平均粒径为0.5〜5.0μm,粘结相的厚度的平均值为0.05〜0.8μm,粘结相的厚度的标准偏差为0.8μm以下。
-
公开(公告)号:US08999531B2
公开(公告)日:2015-04-07
申请号:US13639994
申请日:2011-04-15
申请人: Takahide Kudoh , Naohiro Kagawa , Takashi Umemura
发明人: Takahide Kudoh , Naohiro Kagawa , Takashi Umemura
CPC分类号: C22C26/00 , B22F7/02 , C04B35/5831 , C04B35/6261 , C04B35/62675 , C04B35/62685 , C04B35/6303 , C04B35/645 , C04B37/026 , C04B41/009 , C04B41/4529 , C04B41/81 , C04B2235/3217 , C04B2235/3804 , C04B2235/3813 , C04B2235/3843 , C04B2235/3847 , C04B2235/3852 , C04B2235/3856 , C04B2235/3865 , C04B2235/3886 , C04B2235/402 , C04B2235/5436 , C04B2235/5445 , C04B2235/5472 , C04B2235/72 , C04B2235/785 , C04B2235/786 , C04B2235/80 , C04B2235/85 , C04B2235/96 , C04B2235/9607 , C04B2237/361 , C04B2237/401 , C22C2026/003 , Y10T428/24975 , Y10T428/25 , Y10T428/265 , C04B41/5061 , C04B41/5068 , C04B41/5062 , C04B41/5063 , C04B41/5066
摘要: A coated cBN sintered body has excellent wear resistance, fracture resistance, adhesiveness between a substrate and a coating, and a tool life of which is elongated as compared with conventional cBN sintered bodies. The coated cBN sintered body has a cBN sintered body substrate and a coating coated on the surface thereof. The cBN sintered body includes 76 to 90% by volume of cBN, and 10 to 24% by volume of a binder phase and inevitable impurities. An average grain size of cBN is 0.5 to 5.0 μm, an average value of the thickness of the binder phase is 0.05 to 0.8 μm, and the standard deviation of the thickness of the binder phase is 0.8 μm or less.
摘要翻译: 涂布的cBN烧结体与传统的cBN烧结体相比具有优异的耐磨性,耐断裂性,基材与涂层之间的粘合性,并且其寿命延长。 涂布的cBN烧结体具有cBN烧结体基材和涂布在其表面上的涂层。 cBN烧结体包含76〜90体积%的cBN,10〜24体积%的粘结相和不可避免的杂质。 cBN的平均粒径为0.5〜5.0μm,粘结相的厚度的平均值为0.05〜0.8μm,粘结相的厚度的标准偏差为0.8μm以下。
-