摘要:
The invention relates to the use of polyalkyl(meth)acrylate bead polymers with an average particle size V50 that ranges between 30 and 70 μm for improving the stress cracking resistance of moulding materials containing polyalkyl(meth)acrylate. The invention also relates to moulding materials comprising: a) at least 50 wt. % of an impact resistance modifying agent, which contains at least one polyalkyl(meth)acrylate phase; b) at least 8 wt. % of a polyalkyl(meth)acrylate bead polymer with an average particle size V50 that ranges between 30 and 70 μm; and c) between 0 and 42 wt. % of a polyalkyl(meth)acrylate with a molecular weight ranging between 20,000 and 350,000 g/mol, whereby the wt. % of the components a) to c) amounts to 100 wt. %, and to moulded bodies that can be obtained from said materials.
摘要:
The invention relates to the use of polyalkyl(meth)acrylate bead polymers with an average particle size V50 that ranges between 30 and 70 μm for improving the stress cracking resistance of moulding materials containing polyalkyl(meth)acrylate. The invention also relates to moulding materials comprising: a) at least 50 wt. % of an impact resistance modifying agent, which contains at least one polyalkyl(meth)acrylate phase; b) at least 8 wt. % of a polyalkyl(meth)acrylate bead polymer with an average particle size V50 that ranges between 30 and 70 μm; and c) between 0 and 42 wt. % of a polyalkyl(meth)acrylate with a molecular weight ranging between 20,000 and 350,000 g/mol, whereby the wt. % of the components a) to c) amounts to 100 wt. %, and to moulded bodies that can be obtained from said materials.
摘要:
The present invention relates to a plastics mixture comprising at least one thermoplastic polyurethane A) and at least one impact-modified poly(meth)acrylate B), where the impact-modified poly(meth)acrylate comprises a hard phase whose glass transition temperature is at least 70° C. and a tough phase whose glass transition temperature is at most −10° C., the average particle size of the tough phase is at most 130 nm, and at least a portion of the tough phase has covalent linkage to the hard phase.
摘要:
The present invention relates to a concentrator for focusing solar radiation, having surface structuring in the form of one or more Fresnel lenses on the lower side, and to the production thereof from polymeric materials by means of a specific extrusion process. The inventive concentrator can be employed in plants utilizable for photovoltaic or solar heating purposes, and has the required durability and performance in demanding climatic zones. The inventive concentrator enables particularly economic production and efficient concentration of solar radiation onto objects such as solar cells or absorber units, irrespective of the geometry thereof. The inventive concentrator has high longevity and—combined with this—high optical performance when employed in extreme and demanding climatic zones. This relates, for example, to the area of a high-performance solar cell used in concentrating photovoltaics, and likewise to an absorber tube which finds use in concentrating solar thermal collector, for example in the context of parabolic trough technology.
摘要:
The invention relates to the use of a) at least one polyalkyl(meth)acrylate and b) at least one compound according to formula (I), where the groups R1 and R2 independently represent an alkyl or cycloalkyl group with 1 to 20 carbon atoms, for the production of solar cell modules, particularly for the production of light concentrators for solar cell modules.
摘要:
The invention describes transparent plastics mixtures having low-temperature impact resistance composed of a thermoplastic polyurethane (TPU) and of an impact-modified poly(meth)acrylate (PMMA).
摘要:
The invention relates to the use of a) at least one (poly)alkyl(meth)acrylate and b) at least one compound according to formula (I), wherein the radicals R1 and R2 independently represent an alkyl or cycloalkyl radical having 1 to 20 carbon atoms, for producing solar cell modules, in particular for producing light concentrators for solar cell modules.
摘要:
The present invention relates to a plastics mixture comprising at least one thermoplastic polyurethane A) and at least one impact-modified poly(meth)acrylate B), where the impact-modified poly(meth)acrylate comprises a hard phase whose glass transition temperature is at least 70° C. and a tough phase whose glass transition temperature is at most −10° C., the average particle size of the tough phase is at most 130 nm, and at least a portion of the tough phase has covalent linkage to the hard phase.
摘要:
Moulding composition, encompassing a) at least one polyalkyl (meth)acrylate, and b) at least one compound according to formula (I) in which the moieties R1 and R2 are independently an alkyl or cycloalkyl moiety having from 1 to 20 carbon atoms, where the moulding composition further comprises c) at least one infrared absorber, where the transmittance of the moulding composition at 500 nm is smaller than 89%, at 1000 nm is smaller than 80%, at 1150 nm is smaller than 70% and at 1600 nm is smaller than 77%, in each case measured by means of infrared spectroscopy at 25° C. on 3 mm plaques. The moulding composition is in particular used for the production of solar-cell modules.
摘要:
The invention describes transparent plastics mixtures having low-temperature impact resistance composed of a thermoplastic polyurethane (TPU) and of an impact-modified poly(meth)acrylate (PMMA).