Glass fiber forming composition, glass fibers obtained from the
composition and substrate for circuit board including the glass fibers
as reinforcing material
    1.
    发明授权
    Glass fiber forming composition, glass fibers obtained from the composition and substrate for circuit board including the glass fibers as reinforcing material 失效
    玻璃纤维形成组合物,由组合物获得的玻璃纤维和用于电路板的基板,包括玻璃纤维作为增强材料

    公开(公告)号:US5407872A

    公开(公告)日:1995-04-18

    申请号:US148539

    申请日:1993-11-08

    IPC分类号: C03C13/00 H05K1/03 G03C13/02

    摘要: A glass fiber forming composition exhibits a remarkably high dielectric constant .epsilon..sub..GAMMA. as well as superior chemical resistance, yet it is readily spun into glass fibers. The composition is characterized to show a devitrification temperature which is lower than a spinning temperature at which the glass composition exhibits a viscosity of 10.sup.2.5 poise, so as to be readily spun into corresponding glass fibers. The composition consists essentially of 40 to 65 mol % of SiO.sub.2 ; 20 to 45 mol % of at least one component selected from the group consisting of MgO, CaO, SrO and BaO; 5 to 25 mol % of at least one component selected from the group consisting of TiO.sub.2 and ZrO.sub.2 ; and 0.5 to 15 mol % of NbO.sub.5/2 as calculated from an incorporated amount of Nb.sub.2 O.sub.5. Alternately, the composition consist essentially of 40 to 65 mol % of SiO.sub.2 ; 20 to 45 mol % of at least one component selected from the group consisting of CaO, SrO and BaO; 5 to 25 mol % of at least one component selected from the group consisting of TiO.sub.2 and ZrO.sub.2 ; 0.5 to 15 mol % of NbO.sub.5/2 as calculated from an incorporated amount of Nb.sub.2 O.sub.5 ; and 0.5 to 15 mol % of AlO.sub.3/2 as calculated from an incorporated amount of Al.sub.2 O.sub.3. The composition is also characterized to incorporate at least 85 mol % of a total amount of the oxides and have a dielectric constant [.epsilon..sub..GAMMA. ] of 9 or more at 1 MHz and 25.degree. C.

    摘要翻译: 玻璃纤维形成组合物显示出非常高的介电常数εGAMMA以及优异的耐化学性,但易于纺成玻璃纤维。 该组合物的特征在于显示出低于玻璃组合物的粘度为102.5泊的纺丝温度的失透温度,以便容易地纺丝成相应的玻璃纤维。 该组合物基本上由40至65mol%的SiO 2组成; 20〜45摩尔%的选自MgO,CaO,SrO和BaO的至少一种成分; 5〜25摩尔%的选自TiO 2和ZrO 2的至少一种成分; 和0.5〜15mol%的NbO 5/2,由Nb 2 O 5的掺入量计算。 或者,组合物基本上由40至65mol%的SiO 2组成; 20〜45摩尔%的选自CaO,SrO和BaO的至少一种成分; 5〜25摩尔%的选自TiO 2和ZrO 2的至少一种成分; 由Nb 2 O 5的掺入量计算的NbO 5/2为0.5〜15摩尔% 和由Al 2 O 3的掺入量计算的0.5〜15摩尔%的AlO 3/2。 该组合物的特征还在于,在1MHz和25℃下,所含的氧化物总量至少为85mol%,其介电常数εε为9或更大。

    Substrate for circuit board including the glass fibers as reinforcing
material
    2.
    发明授权
    Substrate for circuit board including the glass fibers as reinforcing material 失效
    电路板基板,包括玻璃纤维作为增强材料

    公开(公告)号:US5334645A

    公开(公告)日:1994-08-02

    申请号:US148330

    申请日:1993-11-08

    摘要: A glass fiber forming composition exhibits a remarkably high dielectric constant .epsilon..sub.r as well as superior chemical resistance, yet it is readily spun into glass fibers. The composition is characterized to show a devitrification temperature which is lower than a spinning temperature at which the glass composition exhibits a viscosity of 10.sup.2.5 poise, so as to be readily spun into corresponding glass fibers. The composition consists essentially of 40 to 65 mol % of SiO.sub.2 ; 20 to 45 mol % of at least one component selected from the group consisting of MgO, CaO, SrO and BaO; 5 to 25 mol % of at least one component selected from the group consisting of TiO.sub.2 and ZrO.sub.2 ; and 0.5 to 15 mol % of NbO.sub.5/2 as calculated from an incorporated amount of Nb.sub.2 O.sub.5. Alternately, the composition consist essentially of 40 to 65 mol % of SiO.sub.2 ; 20 to 45 mol % of at least one component selected from the group consisting of CaO, SrO and BaO; 5 to 25 mol % of at least one component selected from the group consisting of TiO.sub.2 and ZrO.sub.2 ; 0.5 to 15 mol % of NbO.sub.5/2 as calculated from an incorporated amount of Nb.sub.2 O.sub.5 ; and 0.5 to 15 mol % of AlO.sub.3/2 as calculated from an incorporated amount of Al.sub.2 O.sub.3. The composition is also characterized to incorporate at least 85 mol % of a total amount of the oxides and have a dielectric constant [.epsilon..sub.r ] of 9 or more at 1 MHz and 25.degree. C.

    摘要翻译: 玻璃纤维形成组合物显示出非常高的介电常数ε以及优异的耐化学性,但易于纺成玻璃纤维。 该组合物的特征在于显示出低于玻璃组合物的粘度为102.5泊的纺丝温度的失透温度,以便容易地纺丝成相应的玻璃纤维。 该组合物基本上由40至65mol%的SiO 2组成; 20〜45摩尔%的选自MgO,CaO,SrO和BaO的至少一种成分; 5〜25摩尔%的选自TiO 2和ZrO 2的至少一种成分; 和0.5〜15mol%的NbO 5/2,由Nb 2 O 5的掺入量计算。 或者,组合物基本上由40至65mol%的SiO 2组成; 20〜45摩尔%的选自CaO,SrO和BaO的至少一种成分; 5〜25摩尔%的选自TiO 2和ZrO 2的至少一种成分; 由Nb 2 O 5的掺入量计算的NbO 5/2为0.5〜15摩尔% 和由Al 2 O 3的掺入量计算的0.5〜15摩尔%的AlO 3/2。 该组合物的特征还在于,在1MHz和25℃下,将总氧化物的总量至少为85mol%,并且其介电常数ε为9以上。

    Glass fiber forming composition, glass fibers obtained from the
composition and substrate for circuit board including the glass fibers
as reinforcing material
    3.
    发明授权
    Glass fiber forming composition, glass fibers obtained from the composition and substrate for circuit board including the glass fibers as reinforcing material 失效
    玻璃纤维形成组合物,由组合物获得的玻璃纤维和用于电路板的基板,包括玻璃纤维作为增强材料

    公开(公告)号:US5284807A

    公开(公告)日:1994-02-08

    申请号:US832267

    申请日:1992-02-07

    IPC分类号: C03C13/00 H05K1/03 C03L13/02

    摘要: A glass fiber forming composition exhibits a remarkably high dielectric constant .epsilon..sub.r as well as superior chemical resistance, yet it is readily spun into glass fibers. The composition is characterized to show a devitrification temperature which is lower than a spinning temperature at which the glass composition exhibits a viscosity of 10.sup.2.5 poise, so as to be readily spun into corresponding glass fibers. The composition consists essentially of 40 to 65 mol % of SiO.sub.2 ; 20 to 45 mol % of at least one component selected from the group consisting of MgO, CaO, SrO and BaO; 5 to 25 mol % of at least one component selected from the group consisting of TiO.sub.2 and ZrO.sub.2 ; and 0.5 to 15 mol % of NbO.sub.5/2 as calculated from an incorporated amount of Nb.sub.2 O.sub.5. Alternately, the composition consist essentially of 40 to 65 mol % of SiO.sub.2 ; 20 to 45 mol % of at least one component selected from the group consisting of CaO, SrO and BaO; 5 to 25 mol % of at least one component selected from the group consisting of TiO.sub.2 and ZrO.sub.2 ; 0.5 to 15 mol % of NbO.sub.5/2 as calculated from an incorporated amount of Nb.sub.2 O.sub.5 ; and 0.5 to 15 mol % of AlO.sub.3/2 as calculated from an incorporated amount of Al.sub.2 O.sub.3. The composition is also characterized to incorporate at least 85 mol % of a total amount of the oxides and have a dielectric constant [.epsilon..sub.r ] of 9 or more at 1 MHz and 25.degree. C.

    摘要翻译: 玻璃纤维形成组合物显示出非常高的介电常数(ε)r以及优异的耐化学性,但易于纺成玻璃纤维。 该组合物的特征在于显示出低于玻璃组合物的粘度为102.5泊的纺丝温度的失透温度,以便容易地纺丝成相应的玻璃纤维。 该组合物基本上由40至65mol%的SiO 2组成; 20〜45摩尔%的选自MgO,CaO,SrO和BaO的至少一种成分; 5〜25摩尔%的选自TiO 2和ZrO 2的至少一种成分; 和0.5〜15mol%的NbO 5/2,由Nb 2 O 5的掺入量计算。 或者,组合物基本上由40至65mol%的SiO 2组成; 20〜45摩尔%的选自CaO,SrO和BaO的至少一种成分; 5〜25摩尔%的选自TiO 2和ZrO 2的至少一种成分; 由Nb 2 O 5的掺入量计算的NbO 5/2为0.5〜15摩尔% 和由Al 2 O 3的掺入量计算的0.5〜15摩尔%的AlO 3/2。 该组合物的特征还在于,在1MHz和25℃下,其总氧化物的总量至少为85mol%,并具有9或更高的介电常数(ε)r)。