公开(公告)号:US20140093416A1
公开(公告)日:2014-04-03
申请号:US14033613
申请日:2013-09-23
申请人: Lutz Dekker , Guido Günther , Stefan Janssen , Susanne Michel , Alfred Scholz , Shilun Sheng , Babette Tonn , Mark Vierbaum , Stefan Wanjura
发明人: Lutz Dekker , Guido Günther , Stefan Janssen , Susanne Michel , Alfred Scholz , Shilun Sheng , Babette Tonn , Mark Vierbaum , Stefan Wanjura
CPC分类号: C22C37/10 , C22C37/04 , C22C37/08 , F01D25/24 , F05D2300/111
摘要: An alloy is provided. The alloy comprises (in % by weight): silicon2.0%-4.5%, in particular 2.3%-3.9%, carbon2.9%-4.0%, in particular 3.2%-3.7%, niobium0.05%-0.7%, in particular 0.05%-0.6%, molybdenum 0.3%-1.5%, in particular 0.4%-1.0%, and optionally cobalt0.1%-2.0%, in particular 0.1%-1.0%, manganese≦0.3%, in particular 0.15-0.30%, nickel≦0.5%, in particular ≦0.3%, magnesium≦0.07%, in particular at least 0.03%, phosphorus≦0.05%, in particular 0.02%-0.035%, sulfur≦0.012%, in particular ≦0.005%, chromium≦0.1%, in particular ≦0.05%, antimony≦0.004%, in particular ≦0.003%, and iron.
摘要翻译: 提供合金。 该合金包含(重量%):硅2.0%-4.5%,特别是2.3%-3.9%,碳2.9%-4.0%,特别是3.2%-3.7%,铌0.05%-0.7%,特别是0.05 %-0.6%,钼0.3%-1.5%,特别是0.4%-1.0%,和任选的钴0.1%-2.0%,特别是0.1%-1.0%的锰和镍; 0.3%,特别是0.15-0.30% 镍和镍; 0.5%,特别是nlE; 0.3%,镁&nIE; 0.07%,特别是至少0.03%的磷和更多; 0.05%,特别是0.02%-0.035%的硫和镍; 0.012%,特别是nlE; 0.005%,铬< 0.1%,特别是< nlE; 0.05%,锑&NlE; 0.004%,特别是nlE; 0.003%和铁。
-
公开(公告)号:US09494046B2
公开(公告)日:2016-11-15
申请号:US14233514
申请日:2012-07-23
申请人: Stefan Janssen , Michael Kursch
发明人: Stefan Janssen , Michael Kursch
CPC分类号: F01D25/16 , F01D3/04 , F01D25/168 , F05D2240/53 , F16C17/04 , F16C17/243 , F16C25/02 , F16C2360/23
摘要: A method for operating a rotary machine with a rotor that is mounted in a bearing is provided. The rotor is subjected to a thrust that acts substantially in only an axial direction during the operating time. The thrust is received and dissipated by a first thrust bearing of the bearing via sliding means, the bearing having a second thrust bearing. The axial vibrations of the rotor are damped or completely prevented by means of the second thrust bearing generating a force that acts on the first thrust bearing in the direction of the thrust at least temporarily at the same time as the thrust occurs.
摘要翻译: 提供一种用于操作具有安装在轴承中的转子的旋转机器的方法。 转子受到在操作时间内基本上只在轴向作用的推力。 推力由轴承的第一推力轴承通过滑动装置接收和消散,该轴承具有第二止推轴承。 转子的轴向振动通过第二推力轴承被阻尼或完全防止,该第二推力轴承至少在推力发生的同时产生在推力方向上作用在第一止推轴承上的力。
-
公开(公告)号:US20140147247A1
公开(公告)日:2014-05-29
申请号:US14233514
申请日:2012-07-23
申请人: Stefan Janssen , Michael Kursch
发明人: Stefan Janssen , Michael Kursch
IPC分类号: F01D25/16
CPC分类号: F01D25/16 , F01D3/04 , F01D25/168 , F05D2240/53 , F16C17/04 , F16C17/243 , F16C25/02 , F16C2360/23
摘要: A method for operating a rotary machine with a rotor that is mounted in a bearing is provided. The rotor is subjected to a thrust that acts substantially in only an axial direction during the operating time. The thrust is received and dissipated by a first thrust bearing of the bearing via sliding means, the bearing having a second thrust bearing. The axial vibrations of the rotor are damped or completely prevented by means of the second thrust bearing generating a force that acts on the first thrust bearing in the direction of the thrust at least temporarily at the same time as the thrust occurs.
摘要翻译: 提供一种用于操作具有安装在轴承中的转子的旋转机器的方法。 转子受到在操作时间内基本上只在轴向作用的推力。 推力由轴承的第一推力轴承通过滑动装置接收和消散,该轴承具有第二止推轴承。 转子的轴向振动通过第二推力轴承被阻尼或完全防止,该第二推力轴承至少在推力发生的同时产生在推力方向上作用在第一止推轴承上的力。
-
公开(公告)号:US20110194969A1
公开(公告)日:2011-08-11
申请号:US13123001
申请日:2009-09-04
申请人: Stefan Janssen , Shilun Sheng
发明人: Stefan Janssen , Shilun Sheng
IPC分类号: C22C37/10
摘要: Known cast iron alloys have application limits with regard to temperature. A cast iron including cobalt is provided. Through the use of cobalt, an optimal ferritic microstructure is achieved such that with an alloy having silicon 2.0-4.5 wt %, cobalt 0.5-5 wt %, carbon 2.0-4 wt %, molybdenum 0.3-1.48 wt %, manganese ≦0.5 wt %, nickel ≦0.5 wt %, the remainder iron, wherein the proportion of silicon, cobalt, and molybdenum is preferably less than 7.5 wt %, the application limits are shifted to high temperatures.
摘要翻译: 已知的铸铁合金在温度方面有应用限制。 提供了包括钴的铸铁。 通过使用钴,可以获得最佳的铁素体组织,使得使用2.0-4.5重量%的硅,0.5-5重量%的钴,2.0-4重量%的碳,0.3-1.48重量%的钼,锰和镍 wt%,镍和镍; 0.5wt%,余量为铁,其中硅,钴和钼的比例优选小于7.5wt%,施加极限转移到高温。
-
公开(公告)号:US20070295471A1
公开(公告)日:2007-12-27
申请号:US11667575
申请日:2005-11-04
申请人: Stefan Janssen
发明人: Stefan Janssen
摘要: Thick-walled parts made by means of a casting method often exhibit, in those thick zones, the worst mechanical properties since the solidification speed in said zones is reduced relative to the thin-walled zone and frequently induces the worst mechanical properties. There is described a method incorporating control elements in a melting charge, said elements increase locally the solidification speed of the melting charge.
摘要翻译: 通过铸造方法制成的厚壁部件在这些厚区域中经常表现出最差的机械性能,因为所述区域中的凝固速度相对于薄壁区域减小并且经常引起最差的机械性能。 描述了一种在熔化电荷中并入控制元素的方法,所述元素局部地增加熔融电荷的凝固速度。
-
公开(公告)号:US20100178192A1
公开(公告)日:2010-07-15
申请号:US12087797
申请日:2007-01-03
申请人: Stefan Janssen , Shilun Sheng
发明人: Stefan Janssen , Shilun Sheng
摘要: Cast iron alloys have application limits with regard to temperature. By means of the use of cobalt an optimal ferritic structure can be achieved such that with an alloy containing silicon 2.0-4.5 wt. %, cobalt 0.5-5 wt. %, carbon 2.5-4 wt. %, molybdenum≦1 wt. %, manganese≦0.25 wt. %, nickel≦0.3 wt. %, the remainder iron where the proportion of silicon cobalt and molybdenum is less than 7.5 wt. % the application limits are shifted to higher temperatures.
摘要翻译: 铸铁合金在温度方面有应用限制。 通过使用钴,可以实现最佳的铁素体结构,使得使用含有2.0-4.5wt。 %,钴0.5-5wt。 %,碳2.5-4wt。 %,钼≦̸ 1wt。 %,锰≦̸ 0.25wt。 %,镍和镍; 0.3wt。 %,剩余的铁,其中硅钴和钼的比例小于7.5wt。 应用限制转移到更高的温度。
-
公开(公告)号:US07681623B2
公开(公告)日:2010-03-23
申请号:US11667575
申请日:2005-11-04
申请人: Stefan Janssen
发明人: Stefan Janssen
摘要: Thick-walled parts made via a casting method often exhibit, in those thick zones, the worst mechanical properties since the solidification speed in the zones is reduced relative to the thin-walled zone and frequently induces the worst mechanical properties. There is described a method incorporating solidification control elements in a melting charge, the elements increase locally the solidification speed of the melting charge.
摘要翻译: 通过铸造方法制成的厚壁部件在这些厚区域中通常表现出最差的机械性能,因为区域中的凝固速度相对于薄壁区域减小,并且经常引起最差的机械性能。 描述了一种在熔融电荷中结合固化控制元素的方法,该元素局部地增加熔融电荷的固化速度。
-
公开(公告)号:US20140030133A1
公开(公告)日:2014-01-30
申请号:US14110498
申请日:2012-03-21
申请人: Lutz Dekker , Guido Günther , Stefan Janssen , Susanne Lange , Alfred Scholz , Shilun Sheng , Babette Tonn , Mark Vierbaum , Stefan Wanjura
发明人: Lutz Dekker , Guido Günther , Stefan Janssen , Susanne Lange , Alfred Scholz , Shilun Sheng , Babette Tonn , Mark Vierbaum , Stefan Wanjura
摘要: Known cast iron alloys have use limits in respect of the temperature. An alloy (in a weight percentage) including silicon 2.0%-4.5%, carbon 2.9%-4.0%, niobium 0.05%-0.7%, molybdenum 0.3%-1.5%, optionally cobalt 0.1%-2.0%, manganese≦0.3%, nickel≦0.5%, magnesium≦0.07%, phosphorus≦0.05%, sulphur≦0.012%, chromium≦0.1%, antimony≦0.004%, and, iron, is provided.
摘要翻译: 已知的铸铁合金在温度方面有使用限制。 合金(重量百分比)包括硅2.0%-4.5%,碳2.9%-4.0%,铌0.05%-0.7%,钼0.3%-1.5%,任选钴0.1%-2.0%,锰锰0.3% 镍@0.5%,镁@ 0.07%,磷@ 0.05%,硫化值@ 0.012%,铬@ 0.1%,锑@ 0.004%和铁。
-
-
-
-
-
-
-