Ductile Iron Having Cobalt
    3.
    发明申请
    Ductile Iron Having Cobalt 审中-公开
    具有钴的球墨铸铁

    公开(公告)号:US20110194969A1

    公开(公告)日:2011-08-11

    申请号:US13123001

    申请日:2009-09-04

    IPC分类号: C22C37/10

    CPC分类号: C22C37/10 C22C37/04

    摘要: Known cast iron alloys have application limits with regard to temperature. A cast iron including cobalt is provided. Through the use of cobalt, an optimal ferritic microstructure is achieved such that with an alloy having silicon 2.0-4.5 wt %, cobalt 0.5-5 wt %, carbon 2.0-4 wt %, molybdenum 0.3-1.48 wt %, manganese ≦0.5 wt %, nickel ≦0.5 wt %, the remainder iron, wherein the proportion of silicon, cobalt, and molybdenum is preferably less than 7.5 wt %, the application limits are shifted to high temperatures.

    摘要翻译: 已知的铸铁合金在温度方面有应用限制。 提供了包括钴的铸铁。 通过使用钴,可以获得最佳的铁素体组织,使得使用2.0-4.5重量%的硅,0.5-5重量%的钴,2.0-4重量%的碳,0.3-1.48重量%的钼,锰和镍 wt%,镍和镍; 0.5wt%,余量为铁,其中硅,钴和钼的比例优选小于7.5wt%,施加极限转移到高温。

    Cast Iron Comprising Cobalt and Component
    4.
    发明申请
    Cast Iron Comprising Cobalt and Component 审中-公开
    铸铁包括钴和组分

    公开(公告)号:US20100178192A1

    公开(公告)日:2010-07-15

    申请号:US12087797

    申请日:2007-01-03

    IPC分类号: C22C37/00 C22C37/10

    CPC分类号: C22C37/10 C22C37/04

    摘要: Cast iron alloys have application limits with regard to temperature. By means of the use of cobalt an optimal ferritic structure can be achieved such that with an alloy containing silicon 2.0-4.5 wt. %, cobalt 0.5-5 wt. %, carbon 2.5-4 wt. %, molybdenum≦1 wt. %, manganese≦0.25 wt. %, nickel≦0.3 wt. %, the remainder iron where the proportion of silicon cobalt and molybdenum is less than 7.5 wt. % the application limits are shifted to higher temperatures.

    摘要翻译: 铸铁合金在温度方面有应用限制。 通过使用钴,可以实现最佳的铁素体结构,使得使用含有2.0-4.5wt。 %,钴0.5-5wt。 %,碳2.5-4wt。 %,钼≦̸ 1wt。 %,锰≦̸ 0.25wt。 %,镍和镍; 0.3wt。 %,剩余的铁,其中硅钴和钼的比例小于7.5wt。 应用限制转移到更高的温度。

    Casting process and cast component
    5.
    发明授权
    Casting process and cast component 失效
    铸造工艺和铸件组件

    公开(公告)号:US07681623B2

    公开(公告)日:2010-03-23

    申请号:US11667575

    申请日:2005-11-04

    申请人: Stefan Janssen

    发明人: Stefan Janssen

    IPC分类号: B22D19/00 B22D27/04

    CPC分类号: B22D27/04 B22D19/00

    摘要: Thick-walled parts made via a casting method often exhibit, in those thick zones, the worst mechanical properties since the solidification speed in the zones is reduced relative to the thin-walled zone and frequently induces the worst mechanical properties. There is described a method incorporating solidification control elements in a melting charge, the elements increase locally the solidification speed of the melting charge.

    摘要翻译: 通过铸造方法制成的厚壁部件在这些厚区域中通常表现出最差的机械性能,因为区域中的凝固速度相对于薄壁区域减小,并且经常引起最差的机械性能。 描述了一种在熔融电荷中结合固化控制元素的方法,该元素局部地增加熔融电荷的固化速度。

    Method for operating a rotary machine
    6.
    发明授权
    Method for operating a rotary machine 有权
    操作旋转机器的方法

    公开(公告)号:US09494046B2

    公开(公告)日:2016-11-15

    申请号:US14233514

    申请日:2012-07-23

    摘要: A method for operating a rotary machine with a rotor that is mounted in a bearing is provided. The rotor is subjected to a thrust that acts substantially in only an axial direction during the operating time. The thrust is received and dissipated by a first thrust bearing of the bearing via sliding means, the bearing having a second thrust bearing. The axial vibrations of the rotor are damped or completely prevented by means of the second thrust bearing generating a force that acts on the first thrust bearing in the direction of the thrust at least temporarily at the same time as the thrust occurs.

    摘要翻译: 提供一种用于操作具有安装在轴承中的转子的旋转机器的方法。 转子受到在操作时间内基本上只在轴向作用的推力。 推力由轴承的第一推力轴承通过滑动装置接收和消散,该轴承具有第二止推轴承。 转子的轴向振动通过第二推力轴承被阻尼或完全防止,该第二推力轴承至少在推力发生的同时产生在推力方向上作用在第一止推轴承上的力。

    METHOD FOR OPERATING A ROTARY MACHINE
    7.
    发明申请
    METHOD FOR OPERATING A ROTARY MACHINE 有权
    操作旋转机的方法

    公开(公告)号:US20140147247A1

    公开(公告)日:2014-05-29

    申请号:US14233514

    申请日:2012-07-23

    IPC分类号: F01D25/16

    摘要: A method for operating a rotary machine with a rotor that is mounted in a bearing is provided. The rotor is subjected to a thrust that acts substantially in only an axial direction during the operating time. The thrust is received and dissipated by a first thrust bearing of the bearing via sliding means, the bearing having a second thrust bearing. The axial vibrations of the rotor are damped or completely prevented by means of the second thrust bearing generating a force that acts on the first thrust bearing in the direction of the thrust at least temporarily at the same time as the thrust occurs.

    摘要翻译: 提供一种用于操作具有安装在轴承中的转子的旋转机器的方法。 转子受到在操作时间内基本上只在轴向作用的推力。 推力由轴承的第一推力轴承通过滑动装置接收和消散,该轴承具有第二止推轴承。 转子的轴向振动通过第二推力轴承被阻尼或完全防止,该第二推力轴承至少在推力发生的同时产生在推力方向上作用在第一止推轴承上的力。

    Casting Process and Cast Component
    8.
    发明申请
    Casting Process and Cast Component 失效
    铸造工艺和铸件

    公开(公告)号:US20070295471A1

    公开(公告)日:2007-12-27

    申请号:US11667575

    申请日:2005-11-04

    申请人: Stefan Janssen

    发明人: Stefan Janssen

    IPC分类号: B22D27/04 B22D19/00

    CPC分类号: B22D27/04 B22D19/00

    摘要: Thick-walled parts made by means of a casting method often exhibit, in those thick zones, the worst mechanical properties since the solidification speed in said zones is reduced relative to the thin-walled zone and frequently induces the worst mechanical properties. There is described a method incorporating control elements in a melting charge, said elements increase locally the solidification speed of the melting charge.

    摘要翻译: 通过铸造方法制成的厚壁部件在这些厚区域中经常表现出最差的机械性能,因为所述区域中的凝固速度相对于薄壁区域减小并且经常引起最差的机械性能。 描述了一种在熔化电荷中并入控制元素的方法,所述元素局部地增加熔融电荷的凝固速度。