    摘要: A process for regenerating one or more deactivated cobalt comprising Fischer-Tropsch catalyst particle(s), comprising the steps of: (i) oxidising the catalyst particle(s) at a temperature between 20 and 400° C.; (ii) treating the catalyst particle(s) for more than 5 minutes, (iii) drying the catalyst particle(s); and (iv) optionally reducing the catalyst particle(s) with hydrogen or a hydrogen comprising gas. This process may be preceded by a step in which Fischer-Tropsch product is removed from the catalyst particle(s). The treatment is performed using carbon dioxide and a liquid comprising ammonia.

    摘要翻译: 一种用于再生一种或多种包含费 - 托催化剂颗粒的失活的钴的方法,包括以下步骤:(i)在20-400℃的温度下氧化催化剂颗粒; (ii)处理催化剂颗粒超过5分钟,(iii)干燥催化剂颗粒; 和(iv)任选地用氢或包含气体的氢还原催化剂颗粒。 此过程之前可以是从催化剂颗粒中除去费 - 托产物的步骤。 使用二氧化碳和包含氨的液体进行处理。

    Process for regenerating a catalyst
    3.
    发明授权
    Process for regenerating a catalyst 有权
    再生催化剂的方法

    公开(公告)号:US08729140B2

    公开(公告)日:2014-05-20

    申请号:US13333409

    申请日:2011-12-21

    IPC分类号: C07C27/00 B01J20/34

    摘要: A process for regenerating one or more deactivated cobalt comprising Fischer-Tropsch catalyst particle(s), comprising the steps of: (i) oxidizing the catalyst particle(s) at a temperature between 20 and 400° C.; (ii) treating the catalyst particle(s) for more than 5 minutes, (iii) drying the catalyst particle(s); and (iv) optionally reducing the catalyst particle(s) with hydrogen or a hydrogen comprising gas. This process may be preceded by a step in which Fischer-Tropsch product is removed from the catalyst particle(s). The treatment is performed using carbon dioxide and a liquid comprising ammonia.

    摘要翻译: 一种用于再生一种或多种包含费 - 托催化剂颗粒的失活的钴的方法,包括以下步骤:(i)在20-400℃的温度下氧化催化剂颗粒; (ii)处理催化剂颗粒超过5分钟,(iii)干燥催化剂颗粒; 和(iv)任选地用氢或包含气体的氢还原催化剂颗粒。 此过程之前可以是从催化剂颗粒中除去费 - 托产物的步骤。 使用二氧化碳和包含氨的液体进行处理。

    Process for regenerating a catalyst
    5.
    发明授权
    Process for regenerating a catalyst 有权
    再生催化剂的方法

    公开(公告)号:US08431507B2

    公开(公告)日:2013-04-30

    申请号:US12411464

    申请日:2009-03-26

    IPC分类号: B01J38/18

    摘要: A process for regenerating a fixed bed of Fischer-Tropsch catalyst particles, of which at least 40 wt % of the catalyst particles have a size of at least 1 mm, in situ in a Fischer-Tropsch reactor tube. The process comprises the steps of: (i) optionally oxidizing the catalyst at a temperature between 200 and 400° C.; (ii) oxidizing the catalyst at a temperature above 580° C. and below 670° C.; and (iii) reducing the catalyst with hydrogen or a hydrogen comprising gas. This process may be preceded by a step in which Fischer-Tropsch product is removed from the catalyst.

    摘要翻译: 在费 - 托反应器管中原位再生固定床的费 - 托催化剂颗粒的方法,其中至少40重量%的催化剂颗粒的尺寸至少为1mm。 该方法包括以下步骤:(i)任选地在200-400℃的温度下氧化催化剂; (ii)在高于580℃和低于670℃的温度下氧化催化剂; 和(iii)用氢或包含气体的氢还原催化剂。 此过程之前可以是从催化剂中除去费 - 托产物的步骤。

    PROCESS FOR REGENERATING A CATALYST
    6.
    发明申请
    PROCESS FOR REGENERATING A CATALYST 有权
    再生催化剂的方法

    公开(公告)号:US20110143917A1

    公开(公告)日:2011-06-16

    申请号:US12969082

    申请日:2010-12-15

    摘要: A process for regenerating one or more deactivated cobalt comprising Fischer-Tropsch catalyst particle(s), comprising the steps of: (i) oxidising the catalyst particle(s) at a temperature between 20 and 400° C.; (ii) treating the catalyst particle(s) for more than 5 minutes with a solvent, which solvent comprises an amine, (iii) drying the catalyst particle(s); and (iv) optionally reducing the catalyst particle(s) with hydrogen or a hydrogen comprising gas. This process may be preceded by a step in which Fischer-Tropsch product is removed from the catalyst particle(s).

    摘要翻译: 一种用于再生一种或多种包含费 - 托催化剂颗粒的失活的钴的方法,包括以下步骤:(i)在20-400℃的温度下氧化催化剂颗粒; (ii)用溶剂处理催化剂颗粒超过5分钟,该溶剂包括胺,(iii)干燥催化剂颗粒; 和(iv)任选地用氢或包含气体的氢还原催化剂颗粒。 此过程之前可以是从催化剂颗粒中除去费 - 托产物的步骤。

    PROCESS FOR REGENERATING A CATALYST
    7.
    发明申请
    PROCESS FOR REGENERATING A CATALYST 有权
    再生催化剂的方法

    公开(公告)号:US20090247393A1

    公开(公告)日:2009-10-01

    申请号:US12411464

    申请日:2009-03-26

    IPC分类号: B01J38/18 B01J38/10

    摘要: A process for regenerating a fixed bed of Fischer-Tropsch catalyst particles, of which at least 40 wt % of the catalyst particles have a size of at least 1 mm, in situ in a Fischer-Tropsch reactor tube. The process comprises the steps of: (i) optionally oxidising the catalyst at a temperature between 200 and 400° C.; (ii) oxidising the catalyst at a temperature above 580° C. and below 670° C.; and (iii) reducing the catalyst with hydrogen or a hydrogen comprising gas. This process may be preceded by a step in which Fischer-Tropsch product is removed from the catalyst.

    摘要翻译: 在费 - 托反应器管中原位再生固定床的费 - 托催化剂颗粒的方法,其中至少40重量%的催化剂颗粒的尺寸至少为1mm。 该方法包括以下步骤:(i)任选地在200-400℃的温度下氧化催化剂; (ii)在高于580℃和低于670℃的温度下氧化催化剂; 和(iii)用氢或包含气体的氢还原催化剂。 此过程之前可以是从催化剂中除去费 - 托产物的步骤。