METHODS FOR PRODUCING AND PURIFYING 2-HYDROCARBYL-3,3-BIS(4-HYDROXYARYL)PHTHALIMIDINE MONOMERS AND POLYCARBONATES DERIVED THEREFROM
    3.
    发明申请
    METHODS FOR PRODUCING AND PURIFYING 2-HYDROCARBYL-3,3-BIS(4-HYDROXYARYL)PHTHALIMIDINE MONOMERS AND POLYCARBONATES DERIVED THEREFROM 审中-公开
    2-烃基-3,3-双(4-羟基)苯基咪唑单体和衍生自其的聚碳酸酯的生产和纯化方法

    公开(公告)号:US20080033123A1

    公开(公告)日:2008-02-07

    申请号:US11848009

    申请日:2007-08-30

    IPC分类号: C08G64/04 C07D209/44 C08F6/00

    CPC分类号: C08G64/12 C07D209/34

    摘要: Disclosed herein is a method for producing a 2-hydrocarbyl-3,3-bis(4-hydroxyaryl)phthalimidine. The method comprises forming a reaction mixture comprising at least one substituted or unsubstituted phenolphthalein, at least one substituted or unsubstituted primary hydrocarbyl amine, and an acid catalyst; and heating the reaction mixture to a temperature of less than 180° C. to remove a distillate comprising water and form a crude 2-hydrocarbyl-3,3-bis(4-hydroxyaryl)phthalimidine product; where the 2-hydrocarbyl-3,3-bis(4-hydroxyaryl)phthalimidine has a formula: where R1 is selected from the group consisting of a hydrogen and a hydrocarbyl group, and R2 is selected from the group consisting of a hydrogen, a hydrocarbyl group, and a halogen.

    摘要翻译: 本文公开了一种2-烃基-3,3-双(4-羟基芳基)苯并二氮吡啶的制备方法。 该方法包括形成包含至少一种取代或未取代的酚酞,至少一种取代或未取代的伯烃基胺和酸催化剂的反应混合物; 并将反应混合物加热至低于180℃的温度以除去包含水的馏出物并形成粗2-烃基-3,3-双(4-羟基芳基)苯并二氮嘧啶产物; 其中2-烃基-3,3-双(4-羟基芳基)苯并二氮嘧啶具有下式:其中R 1选自氢和烃基, 2 H选自氢,烃基和卤素。

    Dimensionally stable polycarbonate articles
    9.
    发明授权
    Dimensionally stable polycarbonate articles 失效
    尺寸稳定的聚碳酸酯制品

    公开(公告)号:US06552158B1

    公开(公告)日:2003-04-22

    申请号:US10064348

    申请日:2002-07-03

    IPC分类号: C08G6400

    CPC分类号: G11B7/2534 C08G64/06

    摘要: The disclosure relates to articles using polycarbonates produced by a melt transesterification polymerization method using bis(hydroxyaryl)cyclohexanes. Such polycarbonates have suitable glass transition temperatures and outstanding dimensional stabilities, thus making them particularly useful for making articles possessing high temperature stability, particularly for use in optical articles such as high density optical data storage and recordable media.

    摘要翻译: 本公开涉及使用通过使用双(羟基芳基)环己烷的熔融酯交换聚合方法制备的聚碳酸酯的制品。 这种聚碳酸酯具有合适的玻璃化转变温度和优异的尺寸稳定性,因此使其特别适用于具有高温稳定性的制品,特别适用于光学制品如高密度光学数据存储和可记录介质。

    Polysiloxane-polycarbonate compositions, method of manufacture, and articles formed therefrom
    10.
    发明授权
    Polysiloxane-polycarbonate compositions, method of manufacture, and articles formed therefrom 有权
    聚硅氧烷 - 聚碳酸酯组合物,制造方法和由其形成的制品

    公开(公告)号:US08389648B2

    公开(公告)日:2013-03-05

    申请号:US13196599

    申请日:2011-08-02

    IPC分类号: C08L83/06 C08L85/00

    摘要: A composition, comprising, based on the total weight of the polymer components in the composition, 1 to 40 wt. % of an aromatic polycarbonate, 30 to 98.8 wt. % of a polysiloxane-polycarbonate block copolymer, and 0.1 to 10 wt. % of a polysiloxane-polyimide block copolymer comprising more than 20 wt. % polysiloxane blocks, based on the total weight of the polysiloxane-polyimide copolymer. The compositions provide articles with low haze, high luminous transmittance, and good hydro-aging properties. The articles can further be formulated to have excellent flame retardance, particularly when KSS is used.