摘要:
There are provided a phosphor, a light emitting device, a surface light source device, a display device and an illumination device. The phosphor includes an α-type Si3N4 crystal structure and includes oxynitride represented by an empirical formula CaxEuyMzSi12-(m+n)Aln+mOnN16-n, wherein M is at least one selected from a group consisting of Sr, Lu, La and Ba, and satisfies 0.5≦x≦1.1, 0.00005≦y≦0.09, 1.0≦m≦3.6, 0.001≦n≦0.2, and 0.00001≦z≦0.1.
摘要:
There are provided a phosphor, a light emitting device, a surface light source device, a display device and an illumination device. The phosphor includes an α-type Si3N4 crystal structure and includes oxynitride represented by an empirical formula CaxEuyMzSi12−(m+n)Aln+mOnN16−n, wherein M is at least one selected from a group consisting of Sr, Lu, La and Ba, and satisfies 0.5≦x≦1.1, 0.00005≦y≦0.09, 1.0≦m≦3.6, 0.001≦n≦0.2, and 0.00001≦z≦0.1.
摘要:
Disclosed is a method for preparing a fluorescent substance, which is represented by the formula M1-zEuzSiaObNc (M=Sr1-x-yBaxCay, 0 x 0.5, 0 y 0.2, 0
摘要:
Disclosed is a method for preparing a fluorescent substance, which is represented by the formula M1-zEuzSiaObNc (M=Sr1-x-yBaxCay, 0 x 0.5, 0 y 0.2, 0
摘要:
An insulation structure for a storage tank and a method of constructing the insulation structure. Angle plates to which expansion joints and wires are assembled are vertically disposed around the storage tank, tensions of the wires, which are horizontally disposed around the storage tank, are adjusted, and then insulation panels having insulating materials attached thereto are disposed to thermally insulate the storage tank in order to protect a kind of oil that is contained in the storage tank.
摘要:
Disclosed is a method for preparing an oxide nano phosphor. A metal precursor solution is prepared. The metal precursor solution is impregnated into a porous polymer material. A heat treatment is performed on the porous polymer material having the metal precursor solution impregnated therein. The heat treatment is performed by heating the porous polymer material having the metal precursor impregnated therein up to a temperature of higher than 500° C. solution at a temperature elevating rate of higher than 100° C. per minute.
摘要:
Disclosed herein is a method for preparing nanophosphor powders. The method includes impregnating an aqueous solution of one or more metal salts into a fine crystalline polymeric material, drying the impregnated polymeric material, and subjecting the polymeric material to heat-treatment.