摘要:
The present invention relates to a thermoplastic elastomer composition having a three-dimensional network structure which is not formed by a chemical crosslinking and having an excellent elasticity recovery and flexibility, a foam having a highly closed cell, an uniform cell shape, an excellent elasticity recovery, flexibility and appearance, and a process for producing the same. A thermoplastic elastomer of the invention is obtained by mixing in a predetermined ratio an EPDM (1), a crystalline polyethylenic resin (2) and a block copolymer (3) having a crystalline ethylenic polymeric block and a block which is more compatible with said EPDM than with said crystalline polyethylenic resin together with an anti-aging agent followed by kneading in a pressurized kneader. A foam of the invention is obtained by adding 1 part by mass of a wetting agent to 100 parts by mass of the thermoplastic elastomer composition described above together with a foaming agent, agitating and then performing an extrusion foaming.
摘要:
A thermoplastic elastomer composition of the invention, formed by dynamically crosslinking a polymer composition including a rubber and an olefinic resin and having an average particle size of rubber particles within a specific range, shows an excellent balance of mechanical properties such as flexibility and elastic recovery, and a moldability. Also an inclusion of a (meth)acrylate resin and a hydrogenated diene polymer provides a composition particularly excellent in scratch resistance. Also an inclusion of a maleimide compound provides a composition particularly excellent in injection fusibility. Also an inclusion of an undenatured organopolysiloxane of a specific viscosity and a denatured organopolysiloxane provides a composition particularly excellent in initial slidability and durable slidability.
摘要:
The thermoplastic elastomer composition in the present invention comprises an ethylene.&agr;-olefinic copolymeric rubber (A) whose intrinsic viscosity [&eegr;] determined at 135° C. in decalin solvent is 3.5 to 6.8 dl/g, a mineral oil-based softener (B), an &agr;-olefinic crystalline polymer (C) whose degree of crystallinity is 50% or higher and an &agr;-olefinic amorphous polymer (D) whose melt viscosity at 190° C. is 50,000 cPs or less and whose degree of crystallinity is less than 50%, and at least a part of a mixture containing 20 to 63% by mass of the (A), 35 to 78% by mass of the (B), 1 to 12% by mass of the (C) and 1 to 12% by mass of the (D), based on 100% by mass of the total of the components (A), (B), (C) and (D), is crosslinked.
摘要:
An olefin thermoplastic elastomer containing an olefin random copolymer formed by copolymerizing ethylene, an &agr;-olefin having 3 to 10 carbon atoms and an unsaturated monomer having a functional group, and optionally a non-conjugated diene, and metal ions crosslinking the olefin random copolymer, has the same or similar rubber elasticity, flexibility and molding and processability as the conventional olefin thermoplastic elastomers, and has good mechanical properties, wear resistance, in particular scratch resistance.
摘要:
A thermoplastic elastomer composition of the invention, formed by dynamically crosslinking a polymer composition including a rubber and an olefinic resin and having an average particle size of rubber particles within a specific range, shows an excellent balance of mechanical properties such as flexibility and elastic recovery, and a moldability. Also an inclusion of a (meth)acrylate resin and a hydrogenated diene polymer provides a composition particularly excellent in scratch resistance. Also an inclusion of a maleimide compound provides a composition particularly excellent in injection fusibility. Also an inclusion of an undenatured organopolysiloxane of a specific viscosity and a denatured organopolysiloxane provides a composition particularly excellent in initial slidability and durable slidability.
摘要:
The thermoplastic elastomer composition of the present invention comprises a thermoplastic elastomer which includes an ethylene•α-olefin copolymer and a crystalline polyethylene resin, wherein the crystalline polyethylene resin constitutes a three-dimensional network structure in a matrix formed by the ethylene•α-olefin copolymer, an organic or inorganic blowing agent and a nucleating agent, wherein the thermoplastic elastomer has a melt flow rate of 5 g/10 min or more at a temperature of 230° C. and a load of 10 kg, and a melt tension of 3.0 gf or more at a temperature of 210° C. and a pulling rate of 2 m/min. Also the foam injection molding method of the present invention is a method including injecting the above-mentioned composition into a cavity space of a metal mold and then expanding the cavity space to foam by opening the metal mold at a mold opening rate of 0.05 to 0.4 mm/sec.
摘要:
Disclosed herein are an olefinic thermoplastic elastomer sheet which has the same rubber elasticity, flexibility and molding or forming and processing ability as those of the conventional olefinic thermoplastic elastomer sheets and is good in mechanical properties and excellent in mar resistance in particular, a production process thereof, and a laminate having a surface layer composed of this sheet. The olefinic thermoplastic elastomer sheet according to the present invention is composed of an elastomer material comprising an olefin random copolymer obtained by copolymerizing ethylene, an α-olefin having 3 to 10 carbon atoms and an unsaturated monomer having a functional group, and optionally a non-conjugated diene, and a metal ion for crosslinking the olefin random copolymer.
摘要:
Disclosed herein is an automotive molding, which is excellent in scratching resistance, has high gloss and moreover is excellent in weathering resistance. The automotive molding of the invention has a part composed of an elastomer material containing an olefinic random copolymer obtained by copolymerizing ethylene, an α-olefin having 3 to 10 carbon atoms and an unsaturated monomer having a functional group, and optionally a non-conjugated diene, and a metal ion for crosslinking the olefinic random copolymer.
摘要:
The thermoplastic elastomer composition of the present invention comprises a thermoplastic elastomer which includes an ethylene•α-olefin copolymer and a crystalline polyethylene resin, wherein the crystalline polyethylene resin constitutes a three-dimensional network structure in a matrix formed by the ethylene•α-olefin copolymer, an organic or inorganic blowing agent and a nucleating agent, wherein the thermoplastic elastomer has a melt flow rate of 5 g/10 min or more at a temperature of 230° C. and a load of 10 kg, and a melt tension of 3.0 gf or more at a temperature of 210° C. and a pulling rate of 2 m/min. Also the foam injection molding method of the present invention is a method comprising of injecting the above-mentioned composition into a cavity space of a metal mold and then expanding the cavity space to foam by opening the metal mold at a mold opening rate of 0.05 to 0.4 mm/sec.
摘要:
The thermoplastic elastomer composition of the present invention comprises a thermoplastic elastomer which includes an ethylene.α-olefin copolymer and a crystalline polyethylene resin, wherein the crystalline polyethylene resin constitutes a three-dimensional network structure in a matrix formed by the ethylene.α-olefin copolymer, an organic or inorganic blowing agent and a nucleating agent, wherein the thermoplastic elastomer has a melt flow rate of 5 g/10 min or more at a temperature of 230° C. and a load of 10 kg, and a melt tension of 3.0 gf or more at a temperature of 210° C. and a pulling rate of 2 m/min. Also the foam injection molding method of the present invention is a method including injecting the above-mentioned composition into a cavity space of a metal mold and then expanding the cavity space to foam by opening the metal mold at a mold opening rate of 0.05 to 0.4 mm/sec.