摘要:
A method of producing a hard magnetic alloy compact at low cost, in which an alloy that contains not less than 50% by weight of an amorphous phase and exhibits hard magnetism in a crystallized state is solidified and molded at around its crystallization temperature under applied pressure by utilizing the softening phenomenon occurring during a crystallization process. The resulting compact has high hard magnetic characteristics and can be applied as permanent magnet members such as in motors, actuators, and speakers.
摘要:
Hard magnetic materials of the present invention contain at least one element of Fe, Co and Ni as a main component, at least one element M of Zr, Nb, Ta and Hf, at least one rare earth element R and B. The texture of the materials has at least 70% of fine crystalline phase having an average grain size of 100 nm or less, and the residue having an amorphous phase, the fine crystalline phase mainly composed of bcc-Fe or bcc-Fe compound, Fe--B compound and/or R.sub.2 Fe.sub.14 B.sub.1.
摘要:
An Fe-based soft magnetic alloy having a high saturated magnetic flux density and having a composition represented by formula (I) below: (Fe.sub.1-a Q.sub.a).sub.b B.sub.x T.sub.y T'.sub.z (I) wherein Q represents at least one element selected from the group consisting of Co and Ni; T represents at least one element selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, Mo and W, with Zr and/or Hf being always included; T' represents at least one element selected from the group consisting of Cu, Ag, Au, Ni, Pd and Pt; a, b, x, y and z are real numbers satisfying relationships below: 0.ltoreq.a.ltoreq.0.05, 0.ltoreq.b.ltoreq.93 atomic %, 0.5.ltoreq.x.ltoreq.16 atomic %, 4.ltoreq.y.ltoreq.10 atomic %, 0.ltoreq.z.ltoreq.4.5 atomic % provided that when 0
摘要翻译:具有高饱和磁通密度且具有由下式(I)表示的组成的Fe基软磁合金:(Fe1-aQa)bBxTyT'z(I)其中Q表示选自以下的至少一种元素: Co和Ni; T表示选自Ti,Zr,Hf,V,Nb,Ta,Mo和W中的至少一种元素,其中始终包括Zr和/或Hf; T'表示选自Cu,Ag,Au,Ni,Pd和Pt中的至少一种元素; a,b,x,y和z是满足以下关系的实数:0 = a = 0.05,0
摘要:
A noise filter includes an annular magnetic core made of a soft magnetic alloy ribbon mainly made of Fe and containing B and at least one element selected from a group consisting of Ti, Zr, Hf, Nb, Ta, Mo and W, at least 50% of the soft magnetic alloy structure being composed of body-centered cubic structured fine grains having an average grain size of 30 nm or below, a casing for accommodating the magnetic core and having an insulating plate, a pair of coils separated from each other by the insulating plate, and an electronic circuit for connecting a core element made up of the magnetic core, the casing and the coils.
摘要:
The present invention relates to a method of stably manufacturing a Fe-base soft magnetic alloy having steps of subjecting an amorphous alloy mainly composed of Fe to heat treatment in which the amorphous alloy is heated to 400.degree. to 750.degree. C. at a heating rate of 1.0.degree. C./minute or higher so that at least 50% or more of the structure of the amorphous alloy is made of fine crystalline grains formed into a body-centered cubic structure and having an average grain size of crystal of 30 nm or smaller as to have a high magnetic permeability and saturation magnetic flux density.
摘要:
A soft magnetic bulky alloy according to the present invention is obtained by forming under pressure a powder and granule material mainly made of a Fe-M-B based amorphous alloy containing Fe, B and M where M is at least one element selected from a group consisting of Ti, Zr, Hf, V, Nb, Ta, Mo and W. In the soft magnetic bulky alloy, an amorphous alloy phase and a bcc phase with fine grain sizes of 30 nm or below are present in a mixed state, or the bcc phase with fine grain sizes of 30 nm or below is mainly present. The present invention also discloses a method of manufacturing such a soft magnetic bulky alloy.
摘要:
A magneto-impedance element comprises an alloy composed of at least one of Fe, Co and Ni. The alloy has a mixed texture of an amorphous phase and a fine crystalline phase having an average crystal grain size of 50 nm or less. The magneto-impedance element shows a change in impedance in response to an external magnetic field by applying an alternating current. The magneto-impedance element is applied to an azimuth sensor, an autocanceler, or a magnetic head.
摘要:
The present invention provides an Fe-base soft magnetic alloy and a laminated magnetic core formed by using the alloy which contains Fe as a main component and at least one element M and B selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, Mo and W, in which at least 50% of the crystalline structure comprises fine crystalline grains having an average crystal grain size of 30 nm or less and a body-centered cubic structure, and the fracture strain at 300.degree. C. or less is 1. The ratios of the components Fe, and elements M and B are 75 to 93 atomic %, 4 to 9 atomic % and 0.5 to 18 atomic %, respectively. The alloy may contain other additive elements such as Cr, Ru, Hr, Ir, Si, Al, Ge, Ga and the like.
摘要:
A method for making a Fe-based soft magnetic alloy where an alloy melt is injected onto a moving cooling unit to form an amorphous alloy ribbon. The alloy melt contains Fe as a main component, B and at least one metallic element M selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, Mo and W, the composition of the alloy melt being selected such that the resulting amorphous alloy ribbon is characterized by a first crystallization temperature at which fine grain bcc Fe crystallites precipitate, and a second crystallization temperature at which a compound phase containing Fe--B and/or Fe--M precipitates. The amorphous alloy ribbon is then annealed at a temperature which is higher that the first crystallization temperature and less than the second crystallization temperature for an annealing time in the range of 0 minutes to 20 minutes.
摘要:
Alloy powder which is low in price and is unlikely to be oxidized on the surface, and a dispersion-type conductor using the alloy powder in which electromigration is not likely to occur. Melt of copper and silver is cooled at a high cooling speed of 10.sup.5 .degree.C./s or higher. Alloy powder having a composition expressed by a chemical formula Cu.sub.x Ag.sub.1-x (where 0.80.ltoreq..times..ltoreq.0.99) is obtained. Also, a dispersion-type conductor is produced by dispersing 100 parts by weight of the alloy powder in between 5-100 parts by weight of a binder. Thus, the low-priced alloy powder and the dispersion-type conductor of high quality and high reliability can be obtained.