Abstract:
A spot welded joint of at least two steel sheets is provided. At least one of the steel sheets presents yield strength above or equal to 600 MPa, an ultimate tensile strength above or equal to 1000 MPa, uniform elongation above or equal to 15%. The base metal chemical composition includes 0.05≤C≤0.21%, 4.0≤Mn≤7.0%, 0.5≤Al≤3.5%, Si≤2.0%, Ti≤0.2%, V≤0.2%, Nb≤0.2%, P≤0.025%, B≤0.0035%, and the spot welded joint contains a molten zone microstructure containing more than 0.5% of Al and containing a surface fraction of segregated areas lower than 1%, said segregated areas being zones larger than 20 μm2 and containing more than the steel nominal phosphorus content.
Abstract:
The present invention provides a spot welded joint of at least two steel sheets. At least one of the steel sheets presents yield strength above or equal to 600 MPa, an ultimate tensile strength above or equal to 1000 MPa, uniform elongation above or equal to 15%. The base metal chemical composition includes 0.05≤C≤0.21%, 4.0≤Mn≤7.0%, 0.5≤Al≤3.5%, Si≤2.0%, Ti≤0.2%, V≤0.2%, Nb≤0.2%, P≤0.025%, B≤0.0035%, and the spot welded joint contains a molten zone microstructure containing more than 0.5% of Al and containing a surface fraction of segregated areas lower than 1%, said segregated areas being zones larger than 20 μm2 and containing more than the steel nominal phosphorus content.
Abstract:
A cold-rolled and heat-treated steel sheet having a microstructure consisting of, in surface fraction: between 10% and 30% of retained austenite, the retained austenite being present as films having an aspect ratio of at least 3 and as Martensite Austenite islands, less than 8% of the Martensite Austenite islands having a size above 0.5 μm, at most 1% of fresh martensite, at most 50% of tempered martensite, and recovered martensite containing precipitates of at least one element chosen among niobium, titanium and vanadium. A method for manufacturing the cold-rolled and heat-treated steel sheet is also described.
Abstract:
A spot welded joint of at least two steel sheets is provided. At least one of the steel sheets presents yield strength above or equal to 600 MPa, an ultimate tensile strength above or equal to 1000 MPa, uniform elongation above or equal to 15%. The base metal chemical composition includes 0.05≤C≤0.21%, 4.0≤Mn≤7.0%, 0.5≤Al≤3.5%, Si≤2.0%, Ti≤0.2%, V≤0.2%, Nb≤0.2%, P≤0.025%, B≤0.0035%, and the spot welded joint contains a molten zone microstructure containing more than 0.5% of Al and containing a surface fraction of segregated areas lower than 1%, said segregated areas being zones larger than 20 μm2 and containing more than the steel nominal phosphorus content.
Abstract:
A spot welded joint of at least two steel sheets is provided. At least one of the steel sheets presents yield strength above or equal to 600 MPa, an ultimate tensile strength above or equal to 1000 MPa, uniform elongation above or equal to 15%. The base metal chemical composition includes 0.05≤C≤0.21%, 4.0≤Mn≤7.0%, 0.5≤Al≤3.5%, Si≤2.0%, Ti≤0.2%, V≤0.2%, Nb≤0.2%, P≤0.025%, B≤0.0035%, and the spot welded joint contains a molten zone microstructure containing more than 0.5% of Al and containing a surface fraction of segregated areas lower than 1%, said segregated areas being zones larger than 20 μm2 and containing more than the steel nominal phosphorus content.
Abstract:
A cold-rolled and heat-treated steel sheet having a microstructure of, in surface fraction: between 10% and 30% of retained austenite, said retained austenite being present as films having an aspect ratio of at least 3 and as Martensite Austenite islands, less than 8% of such Martensite Austenite islands having a size above 0.5 μm, at most 10% of fresh martensite and recovered martensite containing precipitates of at least one element chosen among niobium, titanium and vanadium. A manufacturing method thereof is also provided.
Abstract:
A spot welded joint of at least two steel sheets is provided. At least one of the steel sheets presents yield strength above or equal to 600 MPa, an ultimate tensile strength above or equal to 1000 MPa, uniform elongation above or equal to 15%. The base metal chemical composition includes 0.05≤C≤0.21%, 4.0≤Mn≤7.0%, 0.5≤Al≤3.5%, Si≤2.0%, Ti≤0.2%, V≤0.2%, Nb≤0.2%, P≤0.025%, B≤0.0035%, and the spot welded joint contains a molten zone microstructure containing more than 0.5% of Al and containing a surface fraction of segregated areas lower than 1%, said segregated areas being zones larger than 20 μm2 and containing more than the steel nominal phosphorus content.
Abstract:
The present invention provides a spot welded joint of at least two steel sheets. At least one of the steel sheets presents yield strength above or equal to 600 MPa, an ultimate tensile strength above or equal to 1000 MPa, uniform elongation above or equal to 15%. The base metal chemical composition includes 0.05≦C≦0.21%, 4.0≦Mn≦7.0%, 0.5≦Al≦3.5%, Si≦2.0%, Ti≦0.2%, V≦0.2%, Nb≦0.2%, P≦0.025%, B≦0.0035%, and the spot welded joint contains a molten zone microstructure containing more than 0.5% of Al and containing a surface fraction of segregated areas lower than 1%, said segregated areas being zones larger than 20 μm2 and containing more than the steel nominal phosphorus content.