Abstract:
The present disclosure relates to a polypropylene composition for the production of molded articles, such as finished parts for the automotive industry, has melt flow rate (230° C., 2.16 kg) of at least 25 g/10 min and comprising: (A) 50-95% of a composition having an intrinsic viscosity of the fraction soluble in xylene at 25° C. of 3.0-5.0 dl/g; and (A1) 70-95% of a propylene homopolymer having a polydispersity index (PI) of 4.3-10, a fraction insoluble in xylene at 25° C. higher than 90% and an MFR (230° C., 2.16 kg) of 100-250 g/10 min; (A2) 5-30% of a copolymer of propylene with 36-44% of ethylene-derived units; (B) optionally up to 45% of a heterophasic propylene polymer, having an MFR (230° C., 2.16 kg) of 10-25 g/10 min, a flexural modulus higher than 1400 MPa, comprising 5-20% of a copolymer rubber component and 80-95% of a matrix propylene polymer component; (C) 2-10% of an ethylene based elastoplastic copolymer; and (D) optionally up to 20% of talc.
Abstract:
The present invention relates to a new polypropylene composition for molded articles, such as finished parts for the automotive industry. A composition comprising: (A) from 40 to 85% by weight of a first propylene-based component being selected from propylene homopolymers, propylene copolymers and heterophasic propylene polymer, such first propylene-based component having a flexural modulus higher than 800 MPa; (B) from 5 to 20% by weight of a second propylene-based component being a heterophasic propylene polymer comprising: (B1) from 20 to 90% by weight of a crystalline polypropylene, and (B2) from 10 to 80% by weight of a copolymer of ethylene and at least one C3-C10 alpha-olefin, such copolymer containing from 10 to 70% by weight of ethylene, being soluble in xylene at room temperature, and having an intrinsic viscosity in tetrahydronaphtalene at 135° C. of higher than 3.5 dl/g; and (C) from 10 to 40% by weight of glass fibers.
Abstract:
The present invention relates to low density polypropylene compositions for the production of molded articles, such as finished parts for the automotive industry.
Abstract:
Polyolefin compositions suitable for injection moulded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A); and from 10% to 70% by weight of a multimodal ethylene/C6-C12 alpha olefin copolymer (B); having density from 0.850 to 0.920 g/cm3, total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135° C. from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE % wt) up to 30% wt; further comprising up to 50% by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component (D) consisting of a ultra-soft heterophasic copolymer component.
Abstract:
The present invention relates to a new polypropylene composition for molded articles, such as finished parts for the automotive industry. A composition comprising: (A) from 40 to 85% by weight of a first propylene-based component being selected from propylene homopolymers, propylene copolymers and heterophasic propylene polymer, such first propylene-based component having a flexural modulus higher than 800 MPa; (B) from 5 to 20% by weight of a second propylene-based component being a heterophasic propylene polymer comprising: (B1) from 20 to 90% by weight of a crystalline polypropylene, and (B2) from 10 to 80% by weight of a copolymer of ethylene and at least one C3-C10 alpha-olefin, such copolymer containing from 10 to 70% by weight of ethylene, being soluble in xylene at room temperature, and having an intrinsic viscosity in tetrahydronaphtalene at 135° C. of higher than 3.5 dl/g; and (C) from 10 to 40% by weight of glass fibers.
Abstract:
Polyolefin compositions suitable for injection molded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A); and from 10% to 70% by weight of a multimodal ethylene/butene-1 copolymer (B); having density from 0.850 to 0.935 g/cm3, total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135° C. from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE % wt) up to 30% wt; further comprising from 0 to 50% by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component D consisting of an ultra-soft heterophasic copolymer component.
Abstract:
The present disclosure relates to a composition comprising: (A) 30-60% by weight of a soft polyolefin composition comprising 10-50% by weight of a copolymer (a) of propylene, which contains from 1-8% by weight of comonomer; 50-90% by weight of a copolymer (b) of ethylene and other alpha-olefin(s) and from 57-80% of ethylene; where the weight ratio of the content of copolymer component (b) to the fraction XS (soluble in xylene) at room temperature (about 25° C.), both (b and XS) referred to the total weight of (a)+(b), is 1.5 or less, and the intrinsic viscosity [η] of the XS fraction is 3 dl/g or more; and the total quantity of copolymerized ethylene is 30-65% by weight; (B) 5-30% of glass fiber filler; (C) 0.5%-3% by weight of a compatibilizer; and (D) 10-40% by weight of a polypropylene component selected from propylene homopolymers, propylene copolymers containing up to 5% by moles of ethylene and/or C4-C10 α-olefin(s) and combinations of such homopolymers and copolymers, with a MFR from 0.3 to 2500 g/10 min.
Abstract:
The present invention relates to a new polypropylene composition for molded articles, such as finished parts for the automotive industry. A composition comprising: (A) from 40 to 85% by weight of a first propylene-based component being selected from propylene homopolymers, propylene copolymers and heterophasic propylene polymer, such first propylene-based component having a flexural modulus higher than 800 MPa; (B) from 5 to 20% by weight of a second propylene-based component being a heterophasic propylene polymer comprising: (B1) from 20 to 90% by weight of a crystalline polypropylene, and (B2) from 10 to 80% by weight of a copolymer of ethylene and at least one C3-C10 alpha-olefin, such copolymer containing from 10 to 70% by weight of ethylene, being soluble in xylene at room temperature, and having an intrinsic viscosity in tetrahydronaphtalene at 135° C. of higher than 3.5 dl/g; and (C) from 10 to 40% by weight of glass fibers.
Abstract:
Polyolefin compositions suitable for injection moulded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A); and from 10% to 70% by weight of a multimodal ethylene/C6-C12 alpha olefin copolymer (B); having density from 0.850 to 0.920 g/cm3, total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135° C. from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE % wt) up to 30% wt; further comprising up to 50% by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component (D) consisting of a ultra-soft heterophasic copolymer component.
Abstract:
The present invention relates to a new polypropylene composition for molded articles, such as finished parts for the automotive industry. A composition comprising: (A) from 40 to 85% by weight of a first propylene-based component being selected from propylene homopolymers, propylene copolymers and heterophasic propylene polymer, such first propylene-based component having a flexural modulus higher than 800 MPa; (B) from 5 to 20% by weight of a second propylene-based component being a heterophasic propylene polymer comprising: (B1) from 20 to 90% by weight of a crystalline polypropylene, and (B2) from 10 to 80% by weight of a copolymer of ethylene and at least one C3-C10 alpha-olefin, such copolymer containing from 10 to 70% by weight of ethylene, being soluble in xylene at room temperature, and having an intrinsic viscosity in tetrahydronaphtalene at 135° C. of higher than 3.5 dl/g; and (C) from 10 to 40% by weight of glass fibers.