SEMICONDUCTIVE POLYMER COMPOSITION FOR ELECTRIC POWER CABLES

    公开(公告)号:US20190136009A1

    公开(公告)日:2019-05-09

    申请号:US16178243

    申请日:2018-11-01

    Applicant: BOREALIS AG

    Abstract: The invention provides a novel semiconductive polymer composition with improved smoothness and dispersibility of carbon black when compounding the polymer composition and feasible balance with other properties such as volume resistivity. The semiconductive polymer composition comprises (a) from 30 to 90 wt % of a polymer component, (b) from 10 to 70 wt % of carbon black and the carbon black (b) has a mass pellet strength (MPS) according to ASTM D1937-13 of from 50 to 250 N. The invention further relates to a process for preparing the semiconductive polymer composition comprising the steps of: i) introducing 30-90 wt % of a polymer component as defined above and 0-8 wt % additives in a mixer device and mixing the polymer component and additives at elevated temperature such that a polymer melt is obtained; ii) adding 10-70 wt % of a carbon black as defined above to the polymer melt and further mixing of the polymer melt.

    SEMICONDUCTIVE POLYMER COMPOSITION FOR ELECTRIC POWER CABLES
    2.
    发明申请
    SEMICONDUCTIVE POLYMER COMPOSITION FOR ELECTRIC POWER CABLES 审中-公开
    电力电缆用半导体聚合物组合物

    公开(公告)号:US20160311998A1

    公开(公告)日:2016-10-27

    申请号:US15106227

    申请日:2014-12-18

    Applicant: BOREALIS AG

    Abstract: The invention provides a novel semiconductive polymer composition with improved smoothness and dispersibility of carbon black when compounding the polymer composition and feasible balance with other properties such as volume resistivity. The semiconductive polymer composition comprises (a) from 30 to 90 wt % of a polymer component, (b) from 10 to 70 wt % of carbon black and the carbon black (b) has a mass pellet strength (MPS) according to ASTM D1937-13 of from 50 to 250 N. The invention further relates to a process for preparing the semiconductive polymer composition comprising the steps of: i) introducing 30-90 wt % of a polymer component as defined above and 0-8 wt % additives in a mixer device and mixing the polymer component and additives at elevated temperature such that a polymer melt is obtained; ii) adding 10-70 wt % of a carbon black as defined above to the polymer melt and further mixing of the polymer melt.

    Abstract translation: 本发明提供了一种新型的半导体聚合物组合物,其在混合聚合物组合物时具有改善的炭黑的平滑性和分散性,并且与诸如体积电阻率的其它性质可行平衡。 半导电聚合物组合物包含(a)30至90重量%的聚合物组分,(b)10至70重量%的炭黑,并且炭黑(b)具有根据ASTM D1937的质量颗粒强度(MPS) -13为50至250N。本发明还涉及一种制备半导体聚合物组合物的方法,包括以下步骤:i)将30-90重量%的上述聚合物组分和0-8重量%的添加剂引入 混合装置,并在升高的温度下混合聚合物组分和添加剂,从而获得聚合物熔体; ii)将10-70重量%的如上定义的炭黑加入到聚合物熔体中并进一步混合聚合物熔体。

    SEMICONDUCTIVE POLYMER COMPOSITION

    公开(公告)号:US20210366631A1

    公开(公告)日:2021-11-25

    申请号:US16771301

    申请日:2018-12-18

    Applicant: BOREALIS AG

    Abstract: The invention relates to a semiconductive polymer composition comprising a polymer component, a conducting component and a crosslinking agent, wherein the polymer component comprises a polar polyethylene and the crosslinking agent comprises an aliphatic mono- or bifunctional peroxide or, alternatively, a monofunctional peroxide containing an aromatic group, and the crosslinking agent is present in an amount which is Z wt %, based on the total amount (100 wt %) of the polymer composition, and Z1≤Z≤Z2, wherein Z1 is 0.01 and Z2 is 5.0, an article being e.g. a cable, e.g. a power cable, and processes for producing a semiconductive polymer composition and an article; useful in different end applications, such as wire and cable (W&C) applications.

    SEMICONDUCTIVE POLYMER COMPOSITION
    5.
    发明公开

    公开(公告)号:US20240112833A1

    公开(公告)日:2024-04-04

    申请号:US18529074

    申请日:2023-12-05

    Applicant: BOREALIS AG

    Abstract: The invention relates to a semiconductive polymer composition comprising a polymer component, a conducting component and a crosslinking agent, wherein the polymer component comprises a polar polyethylene and the crosslinking agent comprises an aliphatic mono- or bifunctional peroxide or, alternatively, a monofunctional peroxide containing an aromatic group, and the crosslinking agent is present in an amount which is Z wt %, based on the total amount (100 wt %) of the polymer composition, and Z1≤Z≤Z2, wherein Z1 is 0.01 and Z2 is 5.0, an article being e.g. a cable, e.g. a power cable, and processes for producing a semiconductive polymer composition and an article; useful in different end applications, such as wire and cable (W&C) applications.

Patent Agency Ranking