公开(公告)号:US08122583B2
公开(公告)日:2012-02-28
申请号:US11758160
申请日:2007-06-05
CPC分类号: B23P17/02 , B22C9/04 , B22C9/12 , B22D29/00 , B22D29/001 , B22D31/002 , Y10T29/4981 , Y10T29/49812 , Y10T29/49982 , Y10T29/49989 , Y10T29/49993
摘要: Removing of a casting core from a metal casting leaves at least one opening in a surface of the metal. The opening is filled with a sacrificial material. The metal and sacrificial material are machined at the opening. After the machining, a remainder of the sacrificial material is removed.
摘要翻译: 从金属铸件中去除铸芯使金属表面中的至少一个开口离开。 开口充满牺牲材料。 金属和牺牲材料在开口处加工。 在加工之后,除去剩余的牺牲材料。
-
公开(公告)号:US20130318771A1
公开(公告)日:2013-12-05
申请号:US13405876
申请日:2012-02-27
IPC分类号: B23P17/02
CPC分类号: B23P17/02 , B22C9/04 , B22C9/12 , B22D29/00 , B22D29/001 , B22D31/002 , Y10T29/4981 , Y10T29/49812 , Y10T29/49982 , Y10T29/49989 , Y10T29/49993
摘要: Removing of a casting core from a metal casting leaves at least one opening in a surface of the metal. The opening is filled with a sacrificial material. The metal and sacrificial material are machined at the opening. After the machining, a remainder of the sacrificial material is removed.
-
公开(公告)号:US20090095435A1
公开(公告)日:2009-04-16
申请号:US11758160
申请日:2007-06-05
CPC分类号: B23P17/02 , B22C9/04 , B22C9/12 , B22D29/00 , B22D29/001 , B22D31/002 , Y10T29/4981 , Y10T29/49812 , Y10T29/49982 , Y10T29/49989 , Y10T29/49993
摘要: Removing of a casting core from a metal casting leaves at least one opening in a surface of the metal. The opening is filled with a sacrificial material. The metal and sacrificial material are machined at the opening. After the machining, a remainder of the sacrificial material is removed.
摘要翻译: 从金属铸件中去除铸芯使金属表面中的至少一个开口离开。 开口充满牺牲材料。 金属和牺牲材料在开口处加工。 在加工之后,除去剩余的牺牲材料。
-
公开(公告)号:US07882884B2
公开(公告)日:2011-02-08
申请号:US11770071
申请日:2007-06-28
IPC分类号: B22D29/00
CPC分类号: B22D29/002
摘要: To destructively remove a casting core from a cast part, the part is exposed to a combination of nitric acid and sulfuric acid. The combination may have, by volume, a nitric acid concentration of 4-20 times the sulfuric acid concentration. The combination may be an aqueous solution including, by volume, 40-60% nitric acid and 3-10% sulfuric acid. The method may remove a ceramic casting core and a refractory metal-based casting core. A first leaching step may remove a major portion of the ceramic casting core and may comprise alkaline leaching. A second leaching step may remove a major portion of the refractory metal-based casting core and may comprise acid leaching. The acid leaching may comprise the combination of nitric acid and sulfuric acid.
摘要翻译: 为了从铸造件中破坏性地去除铸造芯,该部件暴露于硝酸和硫酸的组合。 该组合可以具有体积的硝酸浓度为硫酸浓度的4-20倍。 该组合可以是水溶液,其包含体积比为40-60%的硝酸和3-10%的硫酸。 该方法可以移除陶瓷铸造芯和难熔金属基铸造芯。 第一浸出步骤可以去除陶瓷浇铸芯的主要部分并且可以包括碱浸液。 第二浸出步骤可以除去耐火金属基铸造芯的主要部分,并且可以包括酸浸。 酸浸可以包括硝酸和硫酸的组合。
-
公开(公告)号:US07243700B2
公开(公告)日:2007-07-17
申请号:US11261164
申请日:2005-10-27
IPC分类号: B22D29/00
CPC分类号: B22D29/002
摘要: To destructively remove a refractory metal casting core from a cast part the part is exposed to a combination of nitric acid and sulfuric acid.
摘要翻译: 为了从铸件中破坏性地去除难熔金属铸造芯,该部分暴露于硝酸和硫酸的组合。
-
公开(公告)号:US07753104B2
公开(公告)日:2010-07-13
申请号:US11582592
申请日:2006-10-18
申请人: Blake J. Luczak , Eric A. Hudson , James T. Beals , Eric L. Couch
发明人: Blake J. Luczak , Eric A. Hudson , James T. Beals , Eric L. Couch
摘要: A method involves forming a core assembly. The forming includes molding a first ceramic core over a first refractory metal core to form a core subassembly. The subassembly is assembled to a second ceramic core.
摘要翻译: 一种方法包括形成芯组件。 成型包括在第一耐火金属芯上形成第一陶瓷芯以形成芯子组件。 将组件组装到第二陶瓷芯。
-
公开(公告)号:US20100116452A1
公开(公告)日:2010-05-13
申请号:US11582592
申请日:2006-10-18
申请人: Blake J. Luczak , Eric A. Hudson , James T. Beals , Eric L. Couch
发明人: Blake J. Luczak , Eric A. Hudson , James T. Beals , Eric L. Couch
摘要: A method involves forming a core assembly. The forming includes molding a first ceramic core over a first refractory metal core to form a core subassembly. The subassembly is assembled to a second ceramic core.
-
公开(公告)号:US20120045701A1
公开(公告)日:2012-02-23
申请号:US13144006
申请日:2009-01-09
申请人: Robert J. Braun , Sean C. Emerson , Justin R. Hawkes , Ellen Y. Sun , Jean Yamanis , Tobias H. Sienel , Balbir Singh Bal , Stuart Anthony Astley , Thomas D. Radcliffe , James T. Beals , Walter H. Borst, JR. , May L. Corn , Louis Chiappetta, JR. , John T. Costello , Robert R. Hebert , Thomas Henry Vanderspurt
发明人: Robert J. Braun , Sean C. Emerson , Justin R. Hawkes , Ellen Y. Sun , Jean Yamanis , Tobias H. Sienel , Balbir Singh Bal , Stuart Anthony Astley , Thomas D. Radcliffe , James T. Beals , Walter H. Borst, JR. , May L. Corn , Louis Chiappetta, JR. , John T. Costello , Robert R. Hebert , Thomas Henry Vanderspurt
CPC分类号: H01M8/0618 , H01M8/04014 , H01M8/04022 , H01M8/04089 , H01M8/0612 , H01M8/1246 , H01M2008/1293 , Y02E60/50 , Y02E60/525
摘要: A system and method satisfies temperature and pressure requirements of solid oxide fuel cell system 10 in a manner that increases the overall efficiency and decreases the overall weight of system 10. The system and method include a secondary blower 30 for boosting air stream pressure level sufficient for operation of a reformer 12 that is designed to minimize pressure drop; an integrated heat exchanger 18 for recovering heat from exhaust 36 and comprising multiple flow fields 18A, 18B, 18C for ensuring inlet temperature requirements of a solid oxide fuel cell 14 are met; and a thermal enclosure 46 for separating hot zone 48 components from cool zone 50 components for increasing thermal efficiency of the system and better thermal management.
摘要翻译: 系统和方法以固体氧化物燃料电池系统10的温度和压力要求满足,从而提高整体效率并降低系统10的整体重量。该系统和方法包括二次鼓风机30,用于将空气流压力水平提升到足以 设计用于最小化压降的重整器12的操作; 满足用于从排气36回收热并且包括用于确保固体氧化物燃料电池14的入口温度要求的多个流场18A,18B,18C的集成热交换器18; 以及用于将热区48组件与冷区50组件分离的热封套46,用于提高系统的热效率和更好的热管理。
-
公开(公告)号:US07240718B2
公开(公告)日:2007-07-10
申请号:US11225512
申请日:2005-09-13
IPC分类号: B22D29/00
CPC分类号: B22D29/002 , B22C9/04 , B22C9/103 , B22D29/003
摘要: A thermal-oxidative process is used to remove a casting core from a cast part.
摘要翻译: 使用热氧化方法从铸造部件去除铸造芯。
-
公开(公告)号:US06742698B2
公开(公告)日:2004-06-01
申请号:US10167679
申请日:2002-06-10
IPC分类号: B23K900
CPC分类号: B23P6/007 , B23K9/044 , B23K10/027 , B23K26/32 , B23K26/342 , B23K35/3033 , B23K35/3046 , B23K35/327 , B23K37/06 , B23K2101/001 , B23K2101/34 , B23K2103/08 , B23K2103/18 , B23K2103/26 , F01D5/005 , Y10T29/49318
摘要: The present invention relates to a method for repairing components such as blades used in turbine engines. The method comprises the steps of placing a piece of refractory metal material over an area of the component to be repaired and depositing a repair filler metal material over the piece of refractory material in an amount sufficient to repair the component and welding the repair filler metal material in place. The refractory metal material may be selected from the group consisting of niobium, tantalum, molybdenum, tungsten, a metal having a melting point higher than the melting point of nickel, and alloys thereof and may be uncoated or coated.