Molecular, inorganic glasses
    4.
    发明授权
    Molecular, inorganic glasses 有权
    分子,无机眼镜

    公开(公告)号:US06503859B1

    公开(公告)日:2003-01-07

    申请号:US09894587

    申请日:2001-06-28

    申请人: Bruce G. Aitken

    发明人: Bruce G. Aitken

    IPC分类号: C03C332

    CPC分类号: C03C3/321 C03C4/10

    摘要: The invention resides in a molecular, inorganic glass and a method of making the glass, the glass being vitreous and resistant to devitrification, that is composed, in substantial part at least, of thermally-stable, zero-dimensional clusters or molecules, composed of four atoms of arsenic and three atoms of sulfur, the glass further containing up to 12 atomic percent of germanium, adjoining clusters being bonded to each other primarily by van der Waals forces, and at least 95% of the glass composition consisting of 42-60% arsenic, 37-48% sulfur plus selenium, the selenium being 0-14%.

    摘要翻译: 本发明在于一种分子,无机玻璃和一种制造玻璃,玻璃是玻璃体并且耐失透的方法,其至少部分地由热稳定的零维簇或分子组成,其由 四个原子的砷和三个原子的硫,玻璃还含有最多12原子%的锗,相邻的簇主要通过范德华力彼此结合,并且至少95%的玻璃组合物由42-60 %砷,37-48%硫加硒,硒为0-14%。

    Fluorine-free phosphate glasses
    5.
    发明授权
    Fluorine-free phosphate glasses 失效
    无氟磷酸盐玻璃

    公开(公告)号:US5021366A

    公开(公告)日:1991-06-04

    申请号:US599751

    申请日:1990-10-19

    申请人: Bruce G. Aitken

    发明人: Bruce G. Aitken

    IPC分类号: C03C3/16 C03C3/17

    摘要: This invention is drawn particularly to the production of glasses having essentially fluorine-free compositions consisting essentially, in mole percent, of:______________________________________ Li.sub.2 O 5-10 P.sub.2 O.sub.5 30-36 Na.sub.2 O 5-15 Al.sub.2 O.sub.3 0-5 K.sub.2 O 0-6 CeO.sub.2 0-2 Li.sub.2 O + Na.sub.2 O + K.sub.2 O 15-25 SnO 0-20 ZnO 10-33 PbO 0-20 CaO 0-20 Sb.sub.2 O.sub.3 0-12 SrO 0-20 Bi.sub.2 O.sub.3 0-6 BaO 0-20 SnO + PbO + 0-20. Sb.sub.2 O.sub.3 + Bi.sub.2 O.sub.3 CaO + SrO + BaO 12-25 ______________________________________

    Hermetically sealed glass package and method of fabrication
    6.
    发明授权
    Hermetically sealed glass package and method of fabrication 有权
    密封玻璃包装及其制造方法

    公开(公告)号:US08148179B2

    公开(公告)日:2012-04-03

    申请号:US12725648

    申请日:2010-03-17

    IPC分类号: H01L21/00

    摘要: A hermetically sealed glass package and method for manufacturing the hermetically sealed glass package are described herein using an OLED display as an example. In one embodiment, the hermetically sealed glass package is manufactured by providing a first substrate plate and a second substrate plate. The second substrate contains at least one transition or rare earth metal such as iron, copper, vanadium, manganese, cobalt, nickel, chromium, neodymium and/or cerium. A sensitive thin-film device that needs protection is deposited onto the first substrate plate. A laser is then used to heat the doped second substrate plate in a manner that causes a portion of it to swell and form a hermetic seal that connects the first substrate plate to the second substrate plate and also protects the thin film device. The second substrate plate is doped with at least one transition metal such that when the laser interacts with it there is an absorption of light from the laser in the second substrate plate, which leads to the formation of the hermetic seal while avoiding thermal damage to the thin-film device. Another embodiment of the hermetically sealed glass package and a method for manufacturing that hermetically sealed glass package are also described herein.

    摘要翻译: 这里使用OLED显示器作为示例来描述气密密封的玻璃封装和制造密封玻璃封装的方法。 在一个实施例中,通过提供第一基板和第二基板制造密封的玻璃封装。 第二基板包含至少一种过渡金属或稀土金属,例如铁,铜,钒,锰,钴,镍,铬,钕和/或铈。 需要保护的敏感薄膜器件沉积到第一衬底板上。 然后使用激光器以使其一部分膨胀并形成将第一衬底板连接到第二衬底板的气密密封件并且还保护薄膜器件的方式来加热掺杂的第二衬底板。 第二衬底板掺杂有至少一种过渡金属,使得当激光与其相互作用时,吸收来自第二衬底板中的激光的光,这导致气密密封的形成,同时避免对 薄膜装置。 本文还描述了密封玻璃封装的另一个实施例以及密封玻璃封装的制造方法。

    High strain point glasses
    7.
    发明授权
    High strain point glasses 有权
    高应变点眼镜

    公开(公告)号:US07612004B2

    公开(公告)日:2009-11-03

    申请号:US11505205

    申请日:2006-08-16

    IPC分类号: C03C3/095 C03C3/068

    CPC分类号: C03C3/095

    摘要: A family of glasses from the rare earth alumino-silicate (RE2O3—Al2O3—SiO2) ternary system exhibiting high strain point and low liquidus temperatures; preferably the La2O3—Al2O3—SiO2 ternary system. The glasses are excellent candidates for electronics applications and have the following composition, expressed in mole percent and calculated from the glass batch on an oxide basis: 60-85% SiO2, 10-25% Al2O3, and 4-15% RE2O3.

    摘要翻译: 来自稀土铝硅酸盐(RE2O3-Al2O3-SiO2)三元体系的一系列玻璃显示出高应变点和低液相线温度; 优选La2O3-Al2O3-SiO2三元体系。 该玻璃是电子应用的理想候选物,并且具有以摩尔百分比表示的以下组成,并且以氧化物为基准从玻璃批料计算:60-85%SiO 2,10-25%Al 2 O 3和4-15%RE 2 O 3。

    Aluminum silicophosphate glasses
    9.
    发明授权
    Aluminum silicophosphate glasses 有权
    铝硅磷酸盐玻璃

    公开(公告)号:US07189672B2

    公开(公告)日:2007-03-13

    申请号:US11026364

    申请日:2004-12-30

    IPC分类号: C03C3/062 C03C3/064 C03C3/097

    摘要: A substrate for flat panel display glasses comprising a glass the P2O5—SiO2—Al2O3 ternary system which yields stable glasses exhibiting high strain point temperatures, resistance to devitrification, good chemical durability, excellent dielectric properties, coefficients of thermal expansion that can be tailored to match that of silicon, and having liquidus viscosities that enable forming by conventional methods. The glass comprises the following composition as calculated in weight percent on an oxide basis: P2O5 33–75%, SiO2 2–52%, Al2O3 8–35%.

    摘要翻译: 一种用于平板显示器玻璃的基板,包括玻璃P 2 O 5 -SiO 2 -Al 2 O 2 产生显示出高应变点温度的稳定玻璃,耐失透性,良好的化学耐久性,优异的介电性能,可以适应于硅的热膨胀系数以及具有液相线粘度的稳定玻璃的三元体系 这可以通过常规方法形成。 玻璃包含以氧化物为基准的重量百分比计算的以下组成:P 2 O 3 33-75%,SiO 2 2- 52%,Al 2 O 3 3-35%。

    Durable Sb-stabilized Mo+W phosphate glasses
    10.
    发明授权
    Durable Sb-stabilized Mo+W phosphate glasses 有权
    耐久的Sb稳定的Mo + W磷酸盐玻璃

    公开(公告)号:US06432851B1

    公开(公告)日:2002-08-13

    申请号:US09583600

    申请日:2000-05-31

    申请人: Bruce G. Aitken

    发明人: Bruce G. Aitken

    IPC分类号: C03C804

    CPC分类号: C03C3/21

    摘要: A durable low Tg Sb-stabilized Mo+W phosphate based glass composition exhibiting superior resistance to attack by boiling water, humidity and acids resulting from the addition of Sb to Mo+W phosphate based glass compositions. Specifically, the present invention discloses a glass composition comprising in mol % on the oxide basis, of 0-40% R2O where R includes the alkali metals (Li, Na, K, Rb or Cs) as well as Ag and Tl, 0-20% XO where X includes the alkaline earth metals (Mg, Ca, Sr or Ba) as well as Cu, Zn, Cd and Pb, 15-80% MoO3+WO3, 0.5-60% Sb2O3, and 10-40% P2O5. Additionally, the Sb-stabilized Mo+W phosphate based glass composition can contain a total of 0-5%, in mole percent (mol %) on the oxide basis, of glass forming oxides including, but not limited to, B2O3, Al2O3, SiO2, TeO2, Ga2O3, GeO2, transition metal and rare earth metal oxides, or mixtures thereof. The resulting durable Sb-stabilized Mo+W phosphate based glass compositions are particularly useful as refractory adhesives, sealing glass frits, and overcladding material for glass fiber.

    摘要翻译: 耐久的低Tg Sb稳定的Mo + W磷酸盐基玻璃组合物,其显示出优异的抗沸水,湿度和由添加Sb至Mo + W磷酸盐基玻璃组合物产生的酸所引起的酸的抵抗力。 具体地说,本发明公开了一种玻璃组合物,其以氧化物的摩尔%计含有0-40%的R 2 O,其中R包括碱金属(Li,Na,K,Rb或Cs)以及Ag和Tl, 20%XO,其中X包括碱土金属(Mg,Ca,Sr或Ba)以及Cu,Zn,Cd和Pb,15-80%MoO3 + WO3,0.5-60%Sb2O3和10-40%P2O5 。 另外,Sb稳定化的Mo + W磷酸盐系玻璃组合物可以含有以氧化物为基准的0-5%(摩尔%)的玻璃形成氧化物,包括但不限于B2O3,Al2O3, SiO 2,TeO 2,Ga 2 O 3,GeO 2,过渡金属和稀土金属氧化物,或其混合物。 得到的耐久的Sb稳定的Mo + W磷酸盐基玻璃组合物特别可用作耐火粘合剂,密封玻璃料和用于玻璃纤维的外包装材料。