Abstract:
A cover element for a foldable electronic device that includes a foldable glass element, first and second primary surfaces, and a compressive stress region extending from the first primary surface to a first depth that is defined by a stress σI of at least about 100 MPa in compression at the first primary surface. The device also includes a polymeric layer disposed over the first primary surface. The glass element has a stress profile such that when the glass element is bent to a target bend radius of from 1 mm to 20 mm, to induce a bending stress σB at the first primary surface in tension, σI+σB
Abstract:
A cover element for a foldable electronic device that includes a foldable glass element, first and second primary surfaces, and a compressive stress region extending from the first primary surface to a first depth that is defined by a stress σI of at least about 100 MPa in compression at the first primary surface. The device also includes a polymeric layer disposed over the first primary surface. The glass element has a stress profile such that when the glass element is bent to a target bend radius of from 1 mm to 20 mm, to induce a bending stress σB at the first primary surface in tension, σI+σB
Abstract:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that when the glass element is bent to a target bend radius of from 1 mm to 20 mm, with the center of curvature on the side of the second primary surface so as to induce a bending stress σB at the first primary surface, σI+σB
Abstract translation:一种玻璃元件,其厚度为25μm至125μm,第一主表面,第二主表面和从第一主表面延伸到第一深度的压应力区域,该区域由压缩应力和 在第一主表面处至少约100MPa。 此外,玻璃元件具有应力分布,使得当玻璃元件弯曲到目标弯曲半径为1mm至20mm时,具有在第二主表面侧的曲率中心以引起弯曲应力 &sgr; B在第一个主表面,&sgr; I +&sgr; B <0。 此外,当玻璃元件的第一主表面装载有直径为1.5mm的碳化钨球时,玻璃元件具有≥1.5kgf的耐刺穿性。
Abstract:
A strengthened glass article has a chemically-etched edge and a compressive stress layer formed in a surface region thereof. The compressive stress layer has a compressive stress and a depth of layer. A product of the compressive stress and depth of layer is greater than 21,000 μm-MPa. A method of making the strengthened glass article includes creating the compressive stress layer in a glass sheet, separating the glass article from the glass sheet, and chemically etching at least one edge of the glass article.
Abstract:
A cover element for a foldable electronic device that includes a foldable glass element, first and second primary surfaces, and a compressive stress region extending from the first primary surface to a first depth that is defined by a stress σI of at least about 100 MPa in compression at the first primary surface. The device also includes a polymeric layer disposed over the first primary surface. The glass element has a stress profile such that when the glass element is bent to a target bend radius of from 1 mm to 20 mm, to induce a bending stress σB at the first primary surface in tension, σI+σB
Abstract:
A cover element for a foldable electronic device that includes a foldable glass element, first and second primary surfaces, and a compressive stress region extending from the first primary surface to a first depth that is defined by a stress σI of at least about 100 MPa in compression at the first primary surface. The device also includes a polymeric layer disposed over the first primary surface. The glass element has a stress profile such that when the glass element is bent to a target bend radius of from 1 mm to 20 mm, to induce a bending stress σB at the first primary surface in tension, σI+σB
Abstract:
A cover element for a foldable electronic device that includes a foldable glass element, first and second primary surfaces, and a compressive stress region extending from the first primary surface to a first depth that is defined by a stress σI of at least about 100 MPa in compression at the first primary surface. The device also includes a polymeric layer disposed over the first primary surface. The glass element has a stress profile such that when the glass element is bent to a target bend radius of from 1 mm to 20 mm, to induce a bending stress σB at the first primary surface in tension, σI+σB
Abstract:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that when the glass element is bent to a target bend radius of from 1 mm to 20 mm, with the center of curvature on the side of the second primary surface so as to induce a bending stress σB at the first primary surface, σI+σB
Abstract translation:一种玻璃元件,其厚度为25μm至125μm,第一主表面,第二主表面和从第一主表面延伸到第一深度的压应力区域,该区域由压缩应力和 在第一主表面处至少约100MPa。 此外,玻璃元件具有应力分布,使得当玻璃元件弯曲到目标弯曲半径为1mm至20mm时,曲率中心在第二主表面侧以便引起弯曲应力 &sgr; B在第一个主表面,&sgr; I +&sgr; B <0。 此外,当玻璃元件的第一主表面装载有直径为1.5mm的碳化钨球时,玻璃元件具有≥1.5kgf的耐刺穿性。