Method for making Mo.sub.4 S.sub.4 L.sub.6 (C-2386)
    1.
    发明授权
    Method for making Mo.sub.4 S.sub.4 L.sub.6 (C-2386) 失效
    制备Mo4S4L6(C-2​​386)的方法

    公开(公告)号:US5110963A

    公开(公告)日:1992-05-05

    申请号:US708020

    申请日:1991-05-24

    IPC分类号: C07F11/00

    CPC分类号: C07F11/005

    摘要: The present invention is predicated on the discovery that Mo(III) containing compounds will react with salts of a 1,1-dithioacid to form Mo.sub.4 S.sub.4 L.sub.6. Accordingly, there is provided a method for preparing compounds of the formula Mo.sub.4 S.sub.4 L.sub.6 wherein L is a 1,1-dithioacid ligand comprising:contacting a Mo(III) containing compound with the salt of a 1,1-dithioacid at temperatures and for a time sufficient to form the Mo.sub.4 S.sub.4 L.sub.6 compound. Preferably, the Mo(III) containing compound is dissolved in an organic solvent and the solution is heated at temperatures above about 25.degree. C. up to the boiling point of the solvent and, preferably, at temperatures in the range of about 25.degree. C. to about 250.degree. C.

    摘要翻译: 本发明基于以下发现:含有Mo(III)的化合物将与1,1-二硫酸的盐反应形成Mo 4 S 4 L 6。 因此,提供了制备式Mo 4 S 4 L 6的化合物的方法,其中L是1,1-二硫酸配体,其包括:使含Mo(III)的化合物与1,1-二硫酸的盐在温度和时间 足以形成Mo4S4L6化合物。 优选地,将含Mo(III)的化合物溶解在有机溶剂中,并将溶液在高于约25℃的温度下加热至溶剂的沸点,优选在约25℃的温度 至约250℃

    Method for making Mo.sub.4 S.sub.4 L.sub.6
    3.
    发明授权
    Method for making Mo.sub.4 S.sub.4 L.sub.6 失效
    制备Mo4S4L6的方法

    公开(公告)号:US5126465A

    公开(公告)日:1992-06-30

    申请号:US688212

    申请日:1991-04-22

    IPC分类号: C07F11/00

    CPC分类号: C07F11/005

    摘要: There is provided an improved method for preparing compounds of the formula Mo.sub.4 S.sub.4 L.sub.6 comprising:heating a solution of a compound having the formula MoL.sub.4, wherein L is a 1,1-dithioacid ligand, at a temperature and for a time sufficient to form the Mo.sub.4 S.sub.4 L.sub.6 compound. Preferably, the MoL.sub.4 compound is dissolved in an organic solvent and the solution is heated at temperatures above 25.degree. C., up to the boiling point of the solvent and, more preferably, at temperatures in the range of from about 50.degree. C. to about 250.degree. C.

    摘要翻译: 提供了制备式Mo4S4L6化合物的改进方法,其包括:在足以形成Mo4S4L6化合物的温度和时间下,加热具有式MoL4的化合物(其中L为1,1-二硫酸配体)的溶液 。 优选地,将MoL 4化合物溶解在有机溶剂中,并将溶液在高于25℃的温度下加热至溶剂的沸点,更优选在约50℃至约50℃至 约250℃

    Crude oil pre-heat train with improved heat transfer and method of improving heat transfer
    8.
    发明申请
    Crude oil pre-heat train with improved heat transfer and method of improving heat transfer 失效
    具有改善传热的原油预热列车和改善传热的方法

    公开(公告)号:US20090090613A1

    公开(公告)日:2009-04-09

    申请号:US12232946

    申请日:2008-09-26

    IPC分类号: C10B43/14 F28G7/00

    CPC分类号: C10G75/04 C10G9/16

    摘要: Targeted application of anti-fouling mechanisms in a heat exchange system produces higher rates of energy recovery. The anti-fouling mechanisms with high mitigation rates can be deployed at only the hottest portions of a pre-heat train that experience the highest rates of fouling and heat loss. In application, bundles of corrosion resistant smoothed tubes are deployed in the late pre-heat train to significantly reduce the formation of harder deposits. Vibration can be used as an adjunct approach in conjunction with the corrosion resistant, smooth tubes, or deployed alone on existing bundles. The use of high performing, more durable exchangers in select locations justifies the increased cost of these components.

    摘要翻译: 防污机构在热交换系统中的目标应用产生更高的能量回收率。 具有高缓解率的防污机制只能部署在经受最高污染和热损失率的预热列车的最热部分。 在应用中,在后期预热火车中部署了耐腐蚀平滑管束,以显着减少较硬沉积物的形成。 振动可以作为辅助方法与耐腐蚀,光滑的管一起使用,或单独部署在现有的束上。 在选择的位置使用高性能,更耐用的交换器证明了这些部件的成本增加。