Abstract:
An example turbomachine shroud assembly includes an annular shroud configured to receive a rotating component. A radially outer surface of the annular shroud establishes positioning slots and relief slots. The positioning slots are configured to receive a support finger that limits radial movement of the annular shroud. The relief slots are different than the positioning slots.
Abstract:
An example turbomachine shroud assembly includes an annular shroud configured to receive a rotating component. A radially outer surface of the annular shroud establishes positioning slots and relief slots. The positioning slots are configured to receive a support finger that limits radial movement of the annular shroud. The relief slots are different than the positioning slots.
Abstract:
A composite article includes a substrate, at least one protective layer on the substrate and an intermediate layer between the at least one protective layer and the substrate. The intermediate layer includes dense silicon oxycarbide.
Abstract:
A composition for manufacturing a composite of a non-oxide ceramic matrix and a refractory phase within the non-oxide ceramic matrix includes a preceramic polymer for forming a non-oxide ceramic matrix and a refractory material dispersed within the preceramic polymer.
Abstract:
A method of manufacturing a composite article includes pyrolyzing a preceramic polymer to form a non-oxide ceramic matrix and a byproduct, and reacting the refractory material with the byproduct to form a refractory phase within the non-oxide ceramic matrix.
Abstract:
A process for applying an oxidation resistant coating to an article includes the steps of mixing at least about 10% by volume to up to about 99% by volume of a slurry at least one silica based material having a viscosity of about 1×102 poise to about 1×107 poise at a temperature of about 1,292° F. (700° C.) to about 3,272° F. (1,800° C.) at least about 1% by volume to up to about 90% by volume of the slurry at least one oxygen scavenger, and a liquid medium to form the slurry; coating an article with the slurry to form a slurry coated article; and heat treating under an inert atmosphere the slurry coated article to form an article having at least one oxidation resistant coating layer containing the at least one oxygen scavenger.
Abstract:
A process for applying an oxidation resistant coating to an article includes the steps of mixing at least about 10% by volume to up to about 99% by volume of a slurry at least one silica based material having a viscosity of about 1×102 poise to about 1×107 poise at a temperature of about 1,292° F. (700° C.) to about 3,272° F. (1,800° C.) at least about 1% by volume to up to about 90% by volume of the slurry at least one oxygen scavenger, and a liquid medium to form the slurry; coating an article with the slurry to form a slurry coated article; and heat treating under an inert atmosphere the slurry coated article to form an article having at least one oxidation resistant coating layer containing the at least one oxygen scavenger.
Abstract:
A catalytic device for removal of airborne volatile compounds from air includes a substrate and an electrodeposited catalytic coating. The substrate has a surface. The electrodeposited catalytic coating is on the surface of the substrate. The electrodeposited catalytic coating includes a catalyst that is capable of interacting with airborne volatile compounds. The electrodeposited catalytic coating has a multimodal porosity distribution.