A method of biaxially stretching a polymeric film along an overbias stretch profile having the steps of (a) imparting a sufficiently high temperature to the film to allow a significant amount of biaxial stretch; and (b) biaxial tenter stretching the film to a final first direction stretch parameter and a final second direction stretch parameter, wherein at least 75% of the final first direction stretch parameter is attained before no more than 50% of the final second direction stretch parameter is attained, and wherein the final first direction stretch parameter is no greater than the final second direction stretch parameter.
摘要:
A method of biaxially stretching a polymeric film according to an overbias or overstretch stretch profile to a final first direction stretch parameter and a final second direction stretch parameter to provide a film having uniform properties. First, a sufficiently high temperature is imparted to the film to allow a significant amount of biaxial stretch. The film is then biaxially tenter stretched to a peak first direction stretch parameter that is at least 1.3 times the final first direction stretch parameter wherein the final first direction stretch parameter is no larger than the final second direction stretch parameter. Finally, the film is retracted in the first direction from the peak first direction stretch parameter to the final first direction stretch parameter to produce a film having uniformity of properties in the first direction.
摘要:
A method of stretching films in which all or a portion of the width of the film is cooled during or just after stretching so as to improve the uniformity of the film. The includes stretching a polymeric film in a tenter that grasps the film with a plurality of clips along the opposing edges of the film and propels the clips to thereby stretch the film. The tenter includes driven clips and idler clips, with at least one idler clip between respective pairs of driven clips. The cooling is done so as to improve the uniformity of the clip spacing relative to the spacing obtained at otherwise identical process conditions without such cooling.
摘要:
A process for making an optical film includes stretching a polyolefin film in a first direction and stretching the polyolefin film in a second direction different than the first direction forming a biaxially stretched polyolefin film. At least a portion of the stretching of the polyolefin film in the second direction occurs simultaneous with the stretching of the polyolefin film in the first direction. The biaxially stretched polyolefin film has a length and a width and substantially non-absorbing and non-scattering for at least one polarization state of visible light. The biaxially stretched polyolefin film has x, y, and z orthogonal indices of refraction where at least two of the orthogonal indices of refraction are not equal, an in-plane retardance being 100 nm or less and an out-of-plane retardance being 50 nm or greater.
摘要:
An optical stack includes a first liquid crystal layer and a j-retarder disposed on the liquid crystal layer. The j-retarder includes a simultaneous biaxally stretched polymeric film being substantially non-absorbing and non-scattering for at least one polarization state of visible light. The j-retarder has x, y, and z orthogonal indices of refraction where at least two of the orthogonal indices of refraction are not equal, an in-plane retardance being 100 nm or less and an out-of-plane retardance being 50 nm or greater.
摘要:
An optical stack includes a first liquid crystal layer and a j-retarder disposed on the liquid crystal layer. The j-retarder includes a simultaneous biaxially stretched polymeric film being substantially non-absorbing and non-scattering for at least one polarization state of visible light. The j-retarder has x, y, and z orthogonal indices of refraction where at least two of the orthogonal indices of refraction are not equal, an in-plane retardance being 100 nm or less and an absolute value for an out-of-plane retardance being 55 nm or greater.
摘要:
An optical film includes a layer of simultaneous biaxially stretched polyolefin film that is substantially non-absorbing and non-scattering for at least one polarization state of visible light. The layer has x, y, and z orthogonal indices of refraction where at least two of the orthogonal indices of refraction are not equal. The layer has an in-plane retardance of 100 nm or less and an absolute value of an out-of-plane retardance being 55 nm or greater.
摘要:
An optical film includes a layer of simultaneous biaxially stretched polyolefin film that is substantially non-absorbing and non-scattering for at least one polarization state of visible light. The layer has x, y, and z orthogonal indices of refraction where at least two of the orthogonal indices of refraction are not equal. The layer has an in-plane retardance of 100 nm or less and an out-of-plane retardance of 50 nm or greater.
摘要:
An assembly comprising a film bounded by a frame, the film having a first thermal expansion coefficient along a first direction parallel to the film and a second thermal expansion coefficient along a second direction parallel to the film, wherein thermal expansion of the film compared to that of the frame is greater along the first direction than along the second direction, and wherein the film has a shape at an ambient reference temperature different from that of the frame, the shape of the film being selected to reduce clearance while allowing sufficient room between the film and the frame for thermal expansion in the first direction for temperatures up to a predetermined elevated reference temperature.
摘要:
The invention provides a two-step process for increasing the modulus of a film in a desired direction, by drawing the film at between about 10.degree. C. above T.sub.g and 40.degree. C. below T.sub.m at a draw ratio of between 1.05 and 5.5 and then drawing the film in the same direction at between about 5.degree. C. and 35.degree. C. below T.sub.m at a draw ratio of between about 1.05 and 2.5.