IONIC LIQUID-CONTAINING LAMINATE AND METHOD FOR PRODUCING SAME

    公开(公告)号:US20200094195A1

    公开(公告)日:2020-03-26

    申请号:US16613096

    申请日:2018-04-27

    Abstract: This ionic liquid-containing laminate includes a porous layer having affinity with ionic liquids (C), said layer holding an ionic liquid-containing liquid (A) within voids therein, and a porous layer lacking affinity with ionic liquids (B). The porous layer having affinity with ionic liquids (C) may include an inorganic material (e.g., metal oxide particles having an average particle size of 0.001 to 10 μm on a number basis). The ionic liquid-containing liquid (A) may include an ionic liquid containing cations selected from ammonium, imidazolium and phosphonium cations, and anions selected from fluorine-containing anions, cyano-containing anions and amino acid-derived anions. The porous layer having affinity with ionic liquids (C) may include 1 to 100 volume parts of the ionic liquid-containing liquid (A) with respect to 100 volume parts of voids therein. The ionic liquid-containing laminate is easily formable, and is able to stably hold (or fix) the ionic liquid while maintaining said liquid in a liquid state.

    LAMINATED BODY AND FLEXIBLE DEVICE PROVIDED WITH SAID LAMINATED BODY

    公开(公告)号:US20200230925A1

    公开(公告)日:2020-07-23

    申请号:US16634491

    申请日:2018-04-25

    Abstract: The present invention provides a laminated body obtained by bonding a thinned glass plate and a resin film with an adhesive agent, the laminated body having excellent bending resistance. The laminated body according to an embodiment of the present invention comprising a structure having a glass plate with a thickness of 150 μm or less and a resin film laminated with an adhesive layer; the laminated body having a bending resistance based on a test below of 10 or greater. Bending Resistance Test: in the case where a set of operation includes bending a laminated body for 180° from a state where the laminated body is stretched, in a direction that makes a surface of a glass plate concave and a bending radius 3 mm and then stretching the laminated body again, an index of the bending resistance is the number of sets of the operation until the laminated body cracks when the operation was performed at a rate of 43 sets per minute.

    HEAT-TRANSPORT MEDIUM INCLUDING LATENT HEAT STORAGE MATERIAL, MIXTURE FOR HEAT TRANSPORT, AND HEAT TRANSPORT METHOD

    公开(公告)号:US20180187059A1

    公开(公告)日:2018-07-05

    申请号:US15737685

    申请日:2016-06-13

    Abstract: Used as a heat transport medium to be transported with a fluid that is liquid in an operating temperature range is a medium in which a latent heat storage material is penetrated in a porous material, wherein the latent heat storage material is incompatible with the fluid and has a melting point within the operating temperature range, and the porous material has a liquid repellency to the fluid, an affinity for the latent heat storage material, and a sponge hardness of not more than 50. This achieves stable heat transport with a high heat conversion efficiency even by circulating the medium through a pipeline over a long period of time. The porous material may have continuous pores. The porous material may have a void ratio of not less than 50%. The porous material has an apparent density of about 0.05 to 0.5 g/cm3. The ratio of the latent heat storage material is about 100 to 5000 parts by weight relative to 100 parts by weight of the porous material. The porous material may contain a water-repellent lipophilic resin. The porous material may have a polyorganosiloxane skeleton.

    CARBON DIOXIDE SEPARATION MEMBRANE AND METHOD FOR PRODUCING SAME

    公开(公告)号:US20210154622A1

    公开(公告)日:2021-05-27

    申请号:US16612036

    申请日:2018-04-27

    Abstract: A carbon dioxide separation membrane according to the present invention includes: an ionic liquid affinitive porous layer (C) having an ionic liquid-containing liquid (A) retained in voids; and an ionic liquid non-affinitive porous layer (B). The ionic liquid affinitive porous layer (C) may contain inorganic materials (for example, metal oxide particles having an average particle size of about 0.001 to 5 μm on a number basis). An average thickness of the ionic liquid affinitive porous layer (C) may be about from 0.01 to 10 μm. The ionic liquid affinitive porous layer (C) may include the ionic liquid-containing liquid (A) at a ratio from 0.1 to 99 parts by volume with respect to 100 parts by volume of voids. It may be a carbon dioxide separation membrane for fertilizing plants with carbon dioxide. The carbon dioxide separation membrane can reduce a size of the carbon dioxide concentrating device and enables smooth operation of the device.

    ELECTRODE SLURRY, ELECTRODE AND PROCESS FOR PRODUCING THE SAME, AND SECONDARY BATTERY

    公开(公告)号:US20210083275A1

    公开(公告)日:2021-03-18

    申请号:US16474594

    申请日:2018-01-10

    Abstract: An electrode slurry contains (A) a cellulose fiber and (C) an electrode active material, the electrode active material (C) contains at least a silicon particle and may contain a silicon particle and a carbonaceous particle. The slurry may further contain (B) a carboxymethyl-group-containing cellulose ether or a salt thereof. The average fiber length L (1 to 750 μm) of the cellulose fiber (A) is larger than the average particle size DSi (1 nm to 1 μm) of the silicon particle as the electrode active material (C). The average particle size ratio L/DSi is 5 to 15000. The electrode slurry can improve a discharge capacity and is useful for forming an electrode of a non-aqueous secondary battery (lithium-ion secondary battery) that can maintain a high discharge capacity after repeated charging and discharging.

    ELECTRODE SLURRY, ELECTRODE AND PROCESS FOR PRODUCING THE SAME, AND SECONDARY BATTERY

    公开(公告)号:US20190334175A1

    公开(公告)日:2019-10-31

    申请号:US16476929

    申请日:2018-01-10

    Abstract: An electrode slurry contains (A) a cellulose fiber, (B) a carboxymethyl-group-containing cellulose ether or a salt thereof, and a particulate material containing at least (C) an electrode active material, and the cellulose fiber (A) has an average fiber length of 1 to 750 μm. The amount of the carboxymethyl-group-containing cellulose ether or the salt thereof (B) is 0.1 to 3 parts by weight based on 100 parts by weight of the total amount of the cellulose fiber (A), the carboxymethyl-group-containing cellulose ether or the salt thereof (B), and the electrode active material (C), in terms of solid content. The present invention provides an electrode slurry that allows an improved surface smoothness (coating uniformity) of an electrode and an improved coating property, a process for producing the electrode slurry, an electrode, a process for producing the electrode, a non-aqueous secondary battery, and a lithium-ion secondary battery.

    NOVEL ORGANIC POLYMER AND METHOD FOR PRODUCING SAME

    公开(公告)号:US20190112417A1

    公开(公告)日:2019-04-18

    申请号:US16089831

    申请日:2017-03-24

    Abstract: Provided are a novel organic polymer useful for forming an organic semiconductor and a use of the novel organic polymer. A compound represented by the following formula (Ia) is subjected to a coupling reaction to give an organic polymer: wherein a ring A and a ring B represent an aromatic hydrocarbon ring or an aromatic heterocyclic ring, n denotes an integer of 0 or 1 to 6, R1 to R2+n represent a substituent (such as an alkyl group), a1 to a (2+n) denote an integer of 0 to 2, a ring C represents a benzene ring ortho-fused sequentially and nonlinearly to an adjacent benzene ring depending on the number of n, X represents a hydrogen atom, a halogen atom, a lithium atom, or —MgX1 (wherein X1 represents a halogen atom).

    SECONDARY BATTERY
    9.
    发明申请
    SECONDARY BATTERY 审中-公开

    公开(公告)号:US20190036094A1

    公开(公告)日:2019-01-31

    申请号:US16072801

    申请日:2016-11-30

    Abstract: The present invention provides a secondary battery including a separator which is better in heat resistance than conventional polyolefin-based separators for secondary batteries so that safety can be improved, and which has a low electric resistance while maintaining insulation. It is also an object of the present invention to provide a secondary battery that is excellent in wettability for electrolytic solution, and excellent in productivity in an assembling step of the secondary battery.The secondary battery of the present invention is a secondary battery comprising: a negative electrode; a positive electrode; a separator disposed between the electrodes; and an electrolytic solution, wherein the separator is a porous film, or a porous film laminate having a porous film integrated with a support, a main component of the porous film is a polyetherimide-based resin, and in the configuration of the secondary battery described in this specification, an ion resistance value of the separator as determined by a measuring method described in this specification is 0.18 Ω or less. The secondary battery of the present invention is also a secondary battery comprising: a negative electrode; a positive electrode; a separator disposed between the electrodes; and an electrolytic solution, wherein the separator is a porous film, or a porous film laminate having a porous film integrated with a support, a main component of the porous film is a polyetherimide-based resin, and the separator has an electrolytic solution penetration rate value of 10 to 30 mm/30 minutes in an MD direction.

Patent Agency Ranking