Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and a second ethylene-based polymer, formed by a high pressure, free-radical polymerization process, such composition comprising the following properties: a) a melt index (I2) from 2.0 to 10 dg/min; b) a density from 0.922 to 0.935 g/cc; and wherein the second ethylene-based polymer is present in an amount from 60 to 95 weight percent, based on the sum of the weight of the first polymer and the second polymer; and wherein the second ethylene-based polymer has a density greater than, or equal to, 0.924 g/cc; and wherein the first ethylene-based polymer has a melt index less than 2.5 dg/min.
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)
Abstract:
A multi-layered structure comprising an induction activation layer comprising a blend of (a) a first thermoplastic polymer, (b) a plurality of first particles, each said first particle comprising (i) a core comprising one or more magnetic materials and (ii) a shell comprising silicon dioxide; and (c) optionally a plurality of second particles, each said second particle comprising heat conducting particles; and a sealant, wherein the sealant exhibits a melting point equal to or lower than any other layer in the multi-layered structure, wherein the induction activation layer and sealant are in direct or indirect thermal contact is provided.
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and a second ethylene-based polymer, formed by a high pressure, free-radical polymerization process, such composition comprising the following properties: a) a melt index (12) from 2.0 to 10 dg/min; b) a density from 0.922 to 0.935 g/cc; and wherein the second ethylene-based Hyper polymer is present in an amount from 60 to 95 weight percent, based on the sum of the weight of the first polymer and the second polymer; and wherein the second ethylene-based polymer has a density greater than, or equal to, 0.924 g/cc; and wherein the first ethylene-based polymer has a melt index less than 2.5 dg/min
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus 12 relationship: Mw(abs)
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and comprising the following properties: a) a Mw(abs) versus I2 relationship: Mw(abs)
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and a second ethylene-based polymer, formed by a high pressure, free-radical polymerization process, such composition comprising the following properties: a) a melt index (I2) from 2.0 to 10 dg/min; b) a density from 0.922 to 0.935 g/cc; and wherein the second ethylene-based polymer is present in an amount from 60 to 95 weight percent, based on the sum of the weight of the first polymer and the second polymer; and wherein the second ethylene-based polymer has a density greater than, or equal to, 0.924 g/cc; and wherein the first ethylene-based polymer has a melt index less than 2.5 dg/min.
Abstract:
The invention provides a composition comprising a first ethylene-based polymer, formed by a high pressure, free-radical polymerization process, and a second ethylene-based polymer, formed by a high pressure, free-radical polymerization process, such composition comprising the following properties: a) a melt index (12) from 2.0 to 10 dg/min; b) a density from 0.922 to 0.935 g/cc; and wherein the second ethylene-based polymer is present in an amount from 60 to 95 weight percent, based on the sum of the weight of the first polymer and the second polymer; and wherein the second ethylene-based polymer has a density greater than, or equal to, 0.924 g/cc; and wherein the first ethylene-based polymer has a melt index less than 2.5 dg/min.