摘要:
The present invention relates to articles prepared from novel anionic block copolymers of mono alkenyl arenes and conjugated dienes, and to blends of such block copolymers with other polymers. The block copolymers are selectively hydrogenated and have mono alkenyl arene end blocks and controlled distribution blocks of mono alkenyl arenes and conjugated dienes. The block copolymer may be blended with at least one other polymer selected from the group consisting of olefin polymers, styrene polymers, amorphous resins and engineering thermoplastic resins.
摘要:
The present invention relates to articles prepared from novel anionic block copolymers of mono alkenyl arenes and conjugated dienes, and to blends of such block copolymers with other polymers. The block copolymers have mono alkenyl arene end blocks and controlled distribution blocks of mono alkenyl arenes and conjugated dienes. The block copolymer may be blended with at least one other polymer selected from the group consisting of olefin polymers, styrene polymers, amorphous resins and engineering thermoplastic resins.
摘要:
The present invention relates to articles prepared from novel anionic block copolymers of mono alkenyl arenes and conjugated dienes, and to blends of such block copolymers with other polymers. The block copolymers are selectively hydrogenated and have mono alkenyl arene end blocks and conjugated diene mid blocks. The block copolymer may be blended with at least one other polymer selected from the group consisting of olefin polymers, styrene polymers, amorphous resins and engineering thermoplastic resins.
摘要:
The present invention provides a thermofusible elastomer composition comprising:(a) 100 phr of a selectively hydrogenated block copolymer component comprising an A'B' block copolymer and a multiblock copolymer having at least two end blocks A and at least one mid block B wherein the A' and A blocks are monoalkenyl arene polymer blocks and the B' and B blocks are substantially completely hydrogenated conjugated diene polymer blocks, the number average molecular weight of the A' and A blocks are between about 3,000 and about 7,000 and the monoalkenyl arene content of the multiblock copolymer is between about 7% and about 22% by weight;(b) 20 to 50 phr of at least one high melt flow polyolefin;(c) 0 to 19 phr of a plasticizing oil selected from naphthenic oils and paraffinic oils; and(d) 0 to 40 phr of at least one poly(conjugated diene) block compatible resin wherein the elastomer composition has a particle size of 1400 .mu.m or less.This composition is used in low shear processes.