摘要:
Methods for gas phase olefin polymerization are provided. The method can include combining a spray dried catalyst system with a diluent to produce a catalyst slurry. The catalyst system can include a metallocene compound. Ethylene, a continuity additive, and the catalyst slurry can be introduced to a gas phase fluidized bed reactor. The reactor can be operated at conditions sufficient to produce a polyethylene. The spray dried catalyst system can have a catalyst productivity of at least 12,000 grams polyethylene per gram of the catalyst system.
摘要:
Methods for gas phase olefin polymerization are provided. The method can include combining a spray dried catalyst system with a diluent to produce a catalyst slurry. The catalyst system can include a metallocene compound. Ethylene, a continuity additive, and the catalyst slurry can be introduced to a gas phase fluidized bed reactor. The reactor can be operated at conditions sufficient to produce a polyethylene. The spray dried catalyst system can have a catalyst productivity of at least 12,000 grams polyethylene per gram of the catalyst system.
摘要:
A process for the production of an ethylene alpha-olefin copolymer is disclosed, the process including polymerizing ethylene and at least one alpha-olefin by contacting the ethylene and the at least one alpha-olefin with a metallocene catalyst in at least one gas phase reactor at a reactor pressure of from 0.7 to 70 bar and a reactor temperature of from 20° C. to 150° C. to form an ethylene alpha-olefin copolymer. The resulting ethylene alpha-olefin copolymer may have a density D of 0.927 g/cc or less, a melt index (I2) of from 0.1 to 100 dg/min, a MWD of from 1.5 to 5.0. The resulting ethylene alpha-olefin copolymer may also have a peak melting temperature Tmax second melt satisfying the following relation: Tmax second melt>D*398−245.
摘要:
A process for the production of an ethylene alpha-olefin copolymer is disclosed, the process including polymerizing ethylene and at least one alpha-olefin by contacting the ethylene and the at least one alpha-olefin with a metallocene catalyst in at least one gas phase reactor at a reactor pressure of from 0.7 to 70 bar and a reactor temperature of from 20° C. to 150° C. to form an ethylene alpha-olefin copolymer. The resulting ethylene alpha-olefin copolymer may have a density D of 0.927 g/cc or less, a melt index (I2) of from 0.1 to 100 dg/min, a MWD of from 1.5 to 5.0. The resulting ethylene alpha-olefin copolymer may also have a peak melting temperature Tmax second melt satisfying the following relation: Tmax second melt>D*398−245.
摘要:
A process for the production of an ethylene alpha-olefin copolymer is disclosed, the process including polymerizing ethylene and at least one alpha-olefin by contacting the ethylene and the at least one alpha-olefin with a metallocene catalyst in at least one gas phase reactor at a reactor pressure of from 0.7 to 70 bar and a reactor temperature of from 20° C. to 150° C. to form an ethylene alpha-olefin copolymer. The resulting ethylene alpha-olefin copolymer may have a density D of 0.927 g/cc or less, a melt index (I2) of from 0.1 to 100 dg/min, a MWD of from 1.5 to 5.0. The resulting ethylene alpha-olefin copolymer may also have a peak melting temperature Tmax second melt satisfying the following relation: Tmax second melt>D*398−245.
摘要:
Generally, a method of monitoring a polymerization reaction in a fluid bed reactor to generate, in on-line fashion, data indicative of the imminent occurrence of a discontinuity event (for example, sheeting) and optionally also control the reaction to prevent the occurrence of the discontinuity event is provided. Typical embodiments include the steps of generating in on-line fashion at least one of bed static data indicative of static charge in the fluidized bed and carryover static data indicative of carryover static; and generating at least one of temperature data (in on-line fashion using at least one monitored reaction parameter) indicative of a first temperature and acoustic emission data indicative of resin stickiness in the reactor, where the first temperature is indicative of at least one of degree of resin stickiness in the reactor and a characteristic of melting behavior of polymer resin in the reactor in the presence of at least one diluent.
摘要:
A method for controlling sheeting in a gas phase reactor that includes producing a polyolefin with at least one metallocene catalyst and at least one static control agent in at least one gas phase reactor, measuring entrainment static using a static probe, and adjusting the concentration of the static control agent in response to changes in the measured entrainment static is disclosed.
摘要:
Generally, a method of monitoring a polymerization reaction in a fluid bed reactor to generate, in on-line fashion, data indicative of the imminent occurrence of a discontinuity event (for example, sheeting) and optionally also control the reaction to prevent the occurrence of the discontinuity event is provided. Typical embodiments include the steps of generating in on-line fashion at least one of bed static data indicative of static charge in the fluidized bed and carryover static data indicative of carryover static; and generating at least one of temperature data (in on-line fashion using at least one monitored reaction parameter) indicative of a first temperature and acoustic emission data indicative of resin stickiness in the reactor, where the first temperature is indicative of at least one of degree of resin stickiness in the reactor and a characteristic of melting behavior of polymer resin in the reactor in the presence of at least one diluent.
摘要:
A method for controlling sheeting in a gas phase reactor that includes producing a polyolefin with at least one metallocene catalyst and at least one static control agent in at least one gas phase reactor, measuring entrainment static using a static probe, and adjusting the concentration of the static control agent in response to changes in the measured entrainment static is disclosed.
摘要:
Methods for shutting down and restarting polymerization in a gas phase polymerization reactor are provided. The method can include introducing a polymerization neutralizer to the reactor in an amount sufficient to stop polymerization therein. The method can also include stopping recovery of a polymer product from the reactor and stopping introduction of a catalyst feed and a reactor feed to the reactor. The method can also include adjusting a pressure within the reactor from an operating pressure to an idling pressure. The method can also include adjusting a superficial velocity of a cycle fluid through the reactor from an operating superficial velocity to an idling superficial velocity. The method can also include maintaining the reactor in an idled state for a period of time.