1.
公开(公告)号:US10365411B2
公开(公告)日:2019-07-30
申请号:US15655183
申请日:2017-07-20
Applicant: FUJIFILM Corporation
Inventor: Katsuyuki Takada , Keigo Ueki
IPC: G02F1/1335 , G02B1/14 , B32B27/30 , B32B27/38 , B05D1/18 , B05D1/26 , B05D1/28 , B05D1/30 , C08J7/04 , G02B5/30 , G02B27/00
Abstract: A hardcoat film including a support and a hardcoat layer, in which the support contains a resin as a main component, a film thickness of the hardcoat layer exceeds 20 μm, the hardcoat layer contains a structure derived from a compound which has one alicyclic epoxy group and one ethylenically unsaturated double bond group and has a molecular weight equal to or less than 300, and a structure derived from a compound which has 3 or more ethylenically unsaturated double bond groups, a radical polymerization initiator and a cationic polymerization initiator.
-
公开(公告)号:US20230085579A1
公开(公告)日:2023-03-16
申请号:US17874520
申请日:2022-07-27
Applicant: FUJIFILM Corporation
Inventor: Keigo Ueki , Kentaro Toyooka , Masaya Suzuki
IPC: G03F7/033 , C08F220/18 , C08F212/08 , G03F7/11 , B32B5/02 , B32B5/26 , G06F3/044
Abstract: The present invention relates to: a photosensitive composition including a binder polymer, a polymerizable compound, a photopolymerization initiator, and at least one of a compound A having a group capable of coordinating to a metal or a hygroscopic material; a cured film; a photosensitive transfer material and a method of producing the same; a film; a touch panel; a method of suppressing deterioration; and a laminate and a method of producing the same.
-
公开(公告)号:US11016223B2
公开(公告)日:2021-05-25
申请号:US16013464
申请日:2018-06-20
Applicant: FUJIFILM Corporation
Inventor: Keigo Ueki , Katsuyuki Takada
IPC: G02B1/14 , B32B27/30 , G02B5/30 , G02F1/1335 , H05B33/02 , G06F3/045 , B32B7/023 , G06F3/041 , B05D7/00 , B05D3/06 , G06F3/044 , G09F9/30 , H01L27/32 , H01L51/50 , H01L51/52
Abstract: A hardcoat film has a support, a first cured layer, and a second cured layer in this order in which the first cured layer is formed of a curable composition for forming a first cured layer containing a polymerizable compound 1 having a radically polymerizable group and a polymerizable compound 2 having a cationically polymerizable group and a radically polymerizable group, the second cured layer is formed of a curable composition for forming a second cured layer containing a polymerizable compound 3 having at least two radically polymerizable groups, and a content of the polymerizable compound 2 with respect to a total content of the polymerizable compounds contained in the curable composition for forming a first cured layer is equal to or greater than 51% by mass.
-
公开(公告)号:US09829606B2
公开(公告)日:2017-11-28
申请号:US14747463
申请日:2015-06-23
Applicant: FUJIFILM Corporation
Inventor: Masaaki Suzuki , Keigo Ueki , Taketo Otani , Katsuyuki Takada , Ryo Nakamura
IPC: C09K19/00 , G02B1/14 , C09D135/02 , C09D133/06 , C09D4/00 , G02F1/1335
CPC classification number: G02B1/14 , C08L2312/00 , C09D4/00 , C09D133/066 , C09D135/02 , G02F1/133528 , G02F2201/50 , Y10T428/10 , Y10T428/1036 , C08F2220/325
Abstract: There is provided a method of manufacturing a hard coat film having a hard coat layer on at least one side of a transparent support, the method includes curing a hard coat layer forming composition containing (a) a compound having one alicyclic epoxy group and one ethylenically unsaturated double bond group in a molecule and having a molecular weight of 300 or less, (b) a compound having three or more ethylenically unsaturated double bond groups in a molecule, (c) a radical polymerization initiator, and (d) a cationic polymerization initiator in a specific amount.
-
公开(公告)号:US11435502B2
公开(公告)日:2022-09-06
申请号:US16522030
申请日:2019-07-25
Applicant: FUJIFILM Corporation
Inventor: Yuki Nakazawa , Yutaka Nozoe , Keigo Ueki
Abstract: An optical film, a front panel of an image display apparatus, the image display apparatus, a mirror with an image display function, a resistive film-type touch panel, and a capacitance-type touch panel which have the optical film can be provided. The optical film includes at least a first resin film, an adhesive layer disposed on one side of the first resin film, and a second resin film disposed on the adhesive layer, and the adhesive layer contains a polysaccharide.
-
公开(公告)号:US11300712B2
公开(公告)日:2022-04-12
申请号:US16786167
申请日:2020-02-10
Applicant: FUJIFILM Corporation
Inventor: Makoto Uchimura , Keigo Ueki , Takashi Tamada , Yuichi Fukushige
IPC: G02B1/14
Abstract: A laminate includes a shock absorbing layer, a support, and a hard coat layer, in which the shock absorbing layer has a maximum value of tan δ in a frequency range of 104 to 1013 Hz at 25° C. The tan δ is a ratio of a loss modulus with respect to a storage modulus.
-
公开(公告)号:US10479908B2
公开(公告)日:2019-11-19
申请号:US15782248
申请日:2017-10-12
Applicant: FUJIFILM Corporation
Inventor: Akio Tamura , Katsuyuki Takada , Takayasu Yamazaki , Keisuke Oku , Keigo Ueki
IPC: C09D133/14 , C09D4/00 , B05D7/02 , B05D3/00 , C08F222/10
Abstract: An aspect of the present invention relates to method of manufacturing a hard coat film, wherein the hard coat film comprises a plastic substrate and a hard coat layer, the method comprises forming the hard coat layer by subjecting a photopolymerizable hard coating composition to photopolymerization processing, and the photopolymerizable hard coating composition comprises a radical polymerizable compound having two or more radical polymerizable groups selected from the group consisting of acryloyloxy groups, acryloyl groups, methacryloyloxy groups, and methacryloyl groups per molecule, a cationic polymerizable compound, a radical photopolymerization initiator, and a cationic photopolymerization initiator.
-
公开(公告)号:US20180157111A1
公开(公告)日:2018-06-07
申请号:US15875261
申请日:2018-01-19
Applicant: FUJIFILM Corporation
Inventor: Keigo Ueki , Katsuyuki Takada
IPC: G02F1/1335 , G02F1/1333 , G06F3/041
CPC classification number: G02F1/133528 , G02B5/3033 , G02F1/133305 , G02F1/13338 , G02F1/133602 , G02F2001/133331 , G02F2001/133562 , G02F2202/28 , G06F3/0412
Abstract: The liquid crystal panel has a front-surface plate, a front-side polarizing plate, a liquid crystal display element, and a rear-side polarizing plate in an integrally laminated state, in which the front-surface plate and the front-side polarizing plate are in the state of being laminated with each other via an adhesive layer having a thickness of 2 μm or more, and the liquid crystal panel satisfies Formula A-1: 2020>ECp×dCp×εCp×(100−P)+(Ef×df×εf)−(Er×dr×εr)>0 (ECp is the modulus of elasticity, dCp is the thickness, and εCp is the humidity dimensional change rate, of the front-surface plate, Ef is the modulus of elasticity, df is the thickness, and εf is the humidity dimensional change rate, of the front-side polarizing plate, Er is the modulus of elasticity, dr is the thickness, and εr is the humidity dimensional change rate, of the rear-side polarizing plate, P is the stress relaxation rate of the adhesive layer).
-
9.
公开(公告)号:US11353738B2
公开(公告)日:2022-06-07
申请号:US17038931
申请日:2020-09-30
Applicant: FUJIFILM Corporation
Inventor: Keigo Ueki , Yuichi Fukushige
IPC: G02F1/1335 , G02F1/1333
Abstract: An optical film includes a resin film, and a shock absorbing layer disposed on at least one surface of the resin film, in which a storage elastic modulus E′ of the shock absorbing layer at 25° C., and a frequency of 106 Hz is 1 GPa or less.
-
公开(公告)号:US11092845B2
公开(公告)日:2021-08-17
申请号:US17161002
申请日:2021-01-28
Applicant: FUJIFILM Corporation
Inventor: Keigo Ueki , Yuichi Fukushige
IPC: G02F1/1335 , G02F1/1333
Abstract: A liquid crystal panel and an image display device include a front-side polarizing plate in which a resin film, a shock absorbing layer, and a hard coat layer are disposed in this order; and a rear-side polarizing plate in which a resin film and a shock absorbing layer are disposed in this order, in which a storage elastic modulus E′f of the shock absorbing layer of the front-side polarizing plate at 25° C. and a frequency of 106 Hz is more than 1 GPa, and a relationship between the E′f and a storage elastic modulus E′r of the shock absorbing layer of the rear-side polarizing plate at 25° C. and a frequency of 106 Hz satisfies the expression E′f−E′r>0.
-
-
-
-
-
-
-
-
-