Abstract:
The polyester resin for a hot melt adhesive includes polycarboxylic acid residues and polyhydric alcohol residues. The polycarboxylic acid resides contain aliphatic polycarboxylic acid residues in a proportion within the range of 50 to 80 mol %. The polyhydric alcohol residues contain propylene glycol residues in a proportion within the range 5 to 60 mol %.
Abstract:
A protective composition contains a water-soluble polyester resin including a polyvalent carboxylic acid residue and a polyvalent alcohol residue. The polyvalent carboxylic acid residue includes: a polyvalent carboxylic acid residue having a metal sulfonate group; and a naphthalene dicarboxylic acid residue. The proportion of the polyvalent carboxylic acid residue to the polyvalent carboxylic acid residue falls within the range from 25 mol % to 70 mol %. The proportion of the naphthalene dicarboxylic acid residue to the polyvalent carboxylic acid residue falls within the range from 30 mol % to 75 mol %.
Abstract:
The polyester resin for a hot melt adhesive includes polycarboxylic acid residues and polyhydric alcohol residues. The polycarboxylic acid resides contain aliphatic polycarboxylic acid residues in a proportion within the range of 50 to 80 mol %. The polyhydric alcohol residues contain propylene glycol residues in a proportion within the range 5 to 60 mol %.