摘要:
Provided are bulk homogeneous polymerization processes for producing ethylene propylene random copolymers. The process includes contacting in a reactor or in a series of reactors propylene monomer, ethylene comonomer with one or more catalyst systems and optional solvent (present at less than 40 wt %), wherein the reactor train is at a temperature of between 65° C. and 180° C. and at a pressure no lower than 10 MPa below the cloud point pressure of the polymerization system and less than 1500 MPa, and wherein the polymerization system for the reactor train is in its dense fluid state to form a polymer reactor effluent including a homogeneous fluid phase polymer-monomer mixture in the reactor train; and wherein the resultant copolymer product comprises between 10 wt % and 20 wt % randomly distributed ethylene and the concentration of total region defects in the continuous propylene segments of the random EP copolymer is between 40 and 150% greater than in a copolymer of equivalent melt flow rate and wt % ethylene polymerized by a solution polymerization process.
摘要:
Provided are bulk homogeneous polymerization processes for producing ethylene propylene random copolymers. The process includes contacting in a reactor or in a series of reactors propylene monomer, ethylene comonomer with one or more catalyst systems and optional solvent (present at less than 40 wt %), wherein the reactor train is at a temperature of between 65° C. and 180° C. and at a pressure no lower than 10 MPa below the cloud point pressure of the polymerization system and less than 1500 MPa, and wherein the polymerization system for the reactor train is in its dense fluid state to form a polymer reactor effluent including a homogeneous fluid phase polymer-monomer mixture in the reactor train; and wherein the resultant copolymer product comprises between 10 wt % and 20 wt % randomly distributed ethylene and the concentration of total region defects in the continuous propylene segments of the random EP copolymer is between 40 and 150% greater than in a copolymer of equivalent melt flow rate and wt % ethylene polymerized by a solution polymerization process.
摘要:
Provided are methods of producing polymers with broadened molecular weight and/or composition distribution in a continuous homogeneous polymerization system utilizing reactor temperature gradients, reactor polymer concentration gradients, monomer concentration gradients, catalyst concentration gradients, and combinations thereof in the polymerization reactor. Such methods are particularly suitable when utilizing metallocene catalysts and other single-site catalysts, which generally produce polymers with narrow molecular weight and composition distribution.
摘要:
Provided are methods of producing polymers with broadened molecular weight and/or composition distribution in a continuous homogeneous polymerization system utilizing reactor temperature gradients, reactor polymer concentration gradients, monomer concentration gradients, catalyst concentration gradients, and combinations thereof in the polymerization reactor. Such methods are particularly suitable when utilizing metallocene catalysts and other single-site catalysts, which generally produce polymers with narrow molecular weight and composition distribution.
摘要:
Provided are methods of producing polymers with broadened molecular weight and/or composition distribution in a continuous homogeneous polymerization system utilizing reactor temperature gradients, reactor polymer concentration gradients, monomer concentration gradients, catalyst concentration gradients, and combinations thereof in the polymerization reactor. Such methods are particularly suitable when utilizing metallocene catalysts and other single-site catalysts, which generally produce polymers with narrow molecular weight and composition distribution.
摘要:
A process for feeding ethylene into a polymerization system includes providing a low-pressure ethylene stream, one or more low-pressure C3 to C20 monomer streams, an optional low-pressure inert solvent/diluent stream, and one or more reactors; metering the low-pressure ethylene stream, the one or more low-pressure C3 to C20 monomer streams, and the optional low-pressure inert solvent/diluent stream; blending the metered low-pressure ethylene stream, the metered one or more low-pressure C3 to C20 monomer streams, and the metered low-pressure optional inert solvent/diluent stream to form an ethylene-carrying low-pressure blended liquid feed stream; pressurizing the ethylene-carrying low-pressure blended liquid feed stream to the polymerization system pressure with one or more high-pressure pumps to thrm an ethylene-carrying high-pressure blended reactor feed stream; and feeding the ethylene-carrying high-pressure blended reactor feed stream to the one or more reactors.
摘要:
Provided are methods of producing polymers with broadened molecular weight and/or composition distribution in a continuous homogeneous polymerization system utilizing reactor temperature gradients, reactor polymer concentration gradients, monomer concentration gradients, catalyst concentration gradients, and combinations thereof in the polymerization reactor. Such methods are particularly suitable when utilizing metallocene catalysts and other single-site catalysts, which generally produce polymers with narrow molecular weight and composition distribution.
摘要:
Provided are methods of producing polymers with broadened molecular weight and/or composition distribution in a continuous homogeneous polymerization system utilizing reactor temperature gradients, reactor polymer concentration gradients, monomer concentration gradients, catalyst concentration gradients, and combinations thereof in the polymerization reactor. Such methods are particularly suitable when utilizing metallocene catalysts and other single-site catalysts, which generally produce polymers with narrow molecular weight and composition distribution.
摘要:
Isotactic polypropylene ethylene-propylene copolymer blends and in-line processes for producing. The blends may have between 1 and 50 wt % of isotactic polypropylene with a melt flow rate of between 0.5 and 20,000 g/10 min and a melting peak temperature of 145° C. or higher, and wherein the difference between the DSC peak melting and the peak crystallization temperatures is less than or equal to 0.5333 times the melting peak temperature minus 41.333° C., and between 50 and 99 wt % of ethylene-propylene copolymer including between 10 wt % and 20 wt % randomly distributed ethylene with a melt flow rate of between 0.5 and 20,000 g/10 min, wherein the copolymer is polymerized by a bulk homogeneous polymerization process, and wherein the total regio defects in the continuous propylene segments of the copolymer is between 40 and 150% greater than a copolymer of equivalent melt flow rate and wt % ethylene polymerized by a solution polymerization process.
摘要:
Isotactic polypropylene ethylene-propylene copolymer blends and in-line processes for producing them. The blends may have between 1 and 50 wt % of isotactic polypropylene with a melt flow rate of between 0.5 and 20,000 g/10 min and a melting peak temperature of 145° C. or higher, and wherein the difference between the DSC peak melting and the peak crystallization temperatures is less than or equal to 0.5333 times the melting peak temperature minus 41.333° C., and between 50 and 99 wt % of ethylene-propylene copolymer including between 10 wt % and 20 wt % randomly distributed ethylene with a melt flow rate of between 0.5 and 20,000 g/10 min, wherein the copolymer is polymerized by a bulk homogeneous polymerization process, and wherein the total regio defects in the continuous propylene segments of the copolymer is between 40 and 150% greater than a copolymer of equivalent melt flow rate and wt % ethylene polymerized by a solution polymerization process.