Platinum-based, bimetallic catalyst, and a second group VIII metal used for the opening of cyclic compounds
    2.
    发明申请
    Platinum-based, bimetallic catalyst, and a second group VIII metal used for the opening of cyclic compounds 失效
    铂金双金属催化剂和用于开环的化合物的第二族Ⅷ族金属

    公开(公告)号:US20080207437A1

    公开(公告)日:2008-08-28

    申请号:US11979637

    申请日:2007-11-06

    摘要: A description is given of a catalyst comprising at least one porous support, at least some platinum, and at least a second group VIII metal which is different from platinum and iridium, said catalyst having been prepared in accordance with a process comprising a) impregnation of the support with at least one solution containing a platinum precursor, b) activation in a neutral or oxidising atmosphere, at a temperature of between 120 and 800° C., c) activation in a reducing medium, at a temperature of between 0 and 800° C., d1) impregnation with an aqueous solution and d2) treatment with at least one hydrogen donor compound, at a temperature of less than 200° C., e) the impregnation of the support, which has already been impregnated with the platinum, with at least one solution containing a precursor of said second group VIII metal, and f) activation in a neutral, reducing, or oxidising atmosphere, at a temperature of between 100 and 800° C.

    摘要翻译: 给出了包含至少一种多孔载体,至少一些铂和至少一种与铂和铱不同的第Ⅷ族金属的催化剂的描述,所述催化剂是按照以下方法制备的:a)将 含有至少一种含有铂前体的溶液的载体,b)在中性或氧化性气氛中在120〜800℃的温度下活化,c)在还原介质中在0〜800℃的温度下进行活化 ℃),d1)用水溶液浸渍,和d2)在低于200℃的温度下用至少一种氢供体化合物处理,e)已经浸渍有铂的载体的浸渍 与至少一种含有所述第二族VIII族金属的前体的溶液,和f)在中性,还原性或氧化性气氛中在100至800℃的温度下活化。

    Platinum-based, bimetallic catalyst, and a second group VIII metal used for the opening of cyclic compounds
    3.
    发明授权
    Platinum-based, bimetallic catalyst, and a second group VIII metal used for the opening of cyclic compounds 失效
    铂金双金属催化剂和用于开环的化合物的第二族Ⅷ族金属

    公开(公告)号:US07700514B2

    公开(公告)日:2010-04-20

    申请号:US11979637

    申请日:2007-11-06

    摘要: A catalyst comprising at least one porous support, at least some platinum, and at least a second group VIII metal which is different from platinum and iridium, said catalyst having been prepared in accordance with a process comprising a) impregnation of the support with at least one solution containing a platinum precursor, b) activation in a neutral or oxidizing atmosphere, at a temperature of between 120 and 800° C., c) activation in a reducing medium, at a temperature of between 0 and 800° C., d1) impregnation with an aqueous solution and d2) treatment with at least one hydrogen donor compound, at a temperature of less than 200° C., e) the impregnation of the support, which has already been impregnated with the platinum, with at least one solution containing a precursor of said second group VIII metal, and f) activation in a neutral, reducing, or oxidizing atmosphere, at a temperature of between 100 and 800° C.

    摘要翻译: 一种催化剂,其包含至少一种多孔载体,至少一些铂和至少一种不同于铂和铱的第Ⅷ族金属,所述催化剂是根据以下方法制备的,所述方法包括:a)至少浸渍载体 一种含有铂前体的溶液,b)在中性或氧化性气氛中在120-800℃的温度下活化,c)在还原介质中,在0和800℃之间的温度下,d1 )用水溶液浸渍,和d2)在低于200℃的温度下用至少一种氢供体化合物进行处理,e)将已经用铂浸渍的载体浸渍至少一个 含有所述第二族VIII族金属的前体的溶液,和f)在中性,还原性或氧化性气氛中在100〜800℃的温度下进行活化。

    Method for preparing multi-metal catalysts
    4.
    发明授权
    Method for preparing multi-metal catalysts 失效
    制备多金属催化剂的方法

    公开(公告)号:US5413984A

    公开(公告)日:1995-05-09

    申请号:US934515

    申请日:1992-10-13

    摘要: A method for preparing multi-metal catalysts including an active phase consisting of at least two metals, A and B, which are selected from groups VIII and IB of the periodic table, and a porous support. According to the method: firstly, at least a part of the porous support is impregnated with at least one precursor of metal A; secondly, activation is performed in a neutral or oxidizing atmosphere at a temperature of 120.degree.-800.degree. C. whereafter a treatment is carried out in a reduction medium at a temperature of 0.degree.-800.degree. C.; thirdly, at least a part of the support which was previously impregnated with the precursor of metal A is impregnated with at least one precursor of metal B; and fourthly, activation is performed in a neutral or oxidizing atmosphere at a temperature of 120.degree.-800.degree. C. The catalysts thereby obtained have improved stability, particularly when subjected to high temperatures, such as when they are used as post-combustion catalysts for exhaust gases from internal combustion engines, in which case metal A is platinum or palladium and metal B is platinum, palladium or rhodium, with the proviso that B is not the same as A.

    摘要翻译: PCT No.PCT / FR91 / 00969 Sec。 371日期:1992年10月13日 102(e)日期1992年10月13日PCT 1991年12月4日PCT PCT。 出版物WO92 / 11086 日期:1992年7月9日。一种制备多金属催化剂的方法,包括由至少两种选自元素周期表Ⅷ和IB的金属A和B组成的活性相和多孔载体。 根据该方法:首先,至少一部分多孔载体用至少一种金属A的前体浸渍; 其次,在中性或氧化性气氛中在120-800℃的温度下进行活化,然后在还原介质中在0-800℃的温度下进行处理。 第三,先前用金属A的前体浸渍的载体的至少一部分用至少一种金属B的前体浸渍; 第四,在中性或氧化性气氛中,在120-800℃的温度下进行活化。由此获得的催化剂具有改善的稳定性,特别是当经受高温时,例如当它们用作后燃催化剂 来自内燃机的废气,在这种情况下,金属A为铂或钯,金属B为铂,钯或铑,条件是B与A不同。