Process for the preparation of thermoplastic aromatic
polyphosphonatocarbonates with improved heat-ageing resistance, and
their use
    5.
    发明授权
    Process for the preparation of thermoplastic aromatic polyphosphonatocarbonates with improved heat-ageing resistance, and their use 失效
    具有改善耐热老化性的热塑性芳族聚碳酸亚烃酯的制备方法及其用途

    公开(公告)号:US4401802A

    公开(公告)日:1983-08-30

    申请号:US224077

    申请日:1981-01-12

    CPC分类号: C08G64/00 C08G79/04

    摘要: Thermoplastic polyphosphonatocarbonates prepared by polycondensing at least one aromatic dihydroxy compound with a diaryl carbonate and a phosphonic acid diaryl ester in the presence of a catalyst selected from the group consisting of (a) tetra-C.sub.1 -C.sub.18 -alkyl titanates, (b) di-C.sub.2 -C.sub.4 -alkyl-tin oxides, (c) di-C.sub.2 -C.sub.4 -alkyl-di-C.sub.1 -C.sub.4 -alkoxy-tin compounds, (d) tetra-C.sub.3 -C.sub.18 -alkyl zirconates, (e) tri-C.sub.2 -C.sub.18 -alkyl vanadylates and (f) mixtures of germanium dioxide or titanium dioxide and at least one of (a) to (e) in a weight ratio of 1:3 to 3:1 at a temperature of from 80.degree.-340.degree. C. and under a pressure of 600 to 0.1 mm Hg in an inert gaseous atmosphere, the molar ratio of diaryl carbonate to phosphonic diaryl ester being from 5:95 to 95:5 and the molar ratio of aromatic dihydroxy compound to the sum of diaryl carbonates and phosphonic diaryl ester being from 0.91:1 to 0.99:1.

    摘要翻译: 在选自以下的催化剂存在下,将至少一种芳族二羟基化合物与碳酸二芳酯和膦酸二芳基酯缩聚制备的热塑性聚膦酸碳酸酯:(a)四-C1-烷基钛酸酯,(b)二 - (c)二-C2-C4-烷基 - 二-C1-C4烷氧基锡化合物,(d)四-C 3 -C 18烷基锆酸盐,(e)三-C2-烷基 - C18烷基氧钒酸酯和(f)二氧化锗或二氧化钛与至少一种(a)至(e)的混合物,重量比为1:3至3:1,温度为80-340℃ 并且在惰性气体气氛中在600至0.1mm Hg的压力下,碳酸二芳酯与膦酸二芳基酯的摩尔比为5:95至95:5,芳族二羟基化合物与碳酸二芳基酯的摩尔比 和膦酸二芳基酯为0.91:1至0.99:1。

    Process for the production of aromatic carboxylic acid chlorides
    7.
    发明授权
    Process for the production of aromatic carboxylic acid chlorides 失效
    芳香族羧酸氯化物的制备方法

    公开(公告)号:US4382898A

    公开(公告)日:1983-05-10

    申请号:US312224

    申请日:1981-10-19

    CPC分类号: C07C51/60

    摘要: A single-stage process for the production of pure, particularly sulphur-free, aromatic carboxylic acid chlorides by reacting an aromatic carboxylic acid containing from 1 to 3 carboxyl groups or a corresponding mixture of aromatic carboxylic acids with thionyl chloride in the presence of a catalyst, wherein tertiary phosphine oxides or their reaction products with thionyl chloride and/or the acid chloride to be formed are used as catalysts, and the use of the aromatic dicarboxylic acid dichlorides and tricarboxylic acid trichlorides obtained for the production of polycondensates.

    摘要翻译: 通过在催化剂存在下使含有1至3个羧基的芳族羧酸或芳族羧酸的相应混合物与亚硫酰氯反应生产纯的,特别是无硫的芳族羧酸氯化物的单阶段方法 其中使用叔膦氧化物或其与亚硫酰氯和/或酰氯的反应产物作为催化剂,并且使用获得的芳族二羧酸二氯化物和三羧酸三氯化物来制备缩聚物。

    Aromatic thermoplastic polyphosphonatocarbonate
    8.
    发明授权
    Aromatic thermoplastic polyphosphonatocarbonate 失效
    芳香族热塑性聚磷酸酯

    公开(公告)号:US4322520A

    公开(公告)日:1982-03-30

    申请号:US160644

    申请日:1980-06-18

    CPC分类号: C08G79/04 C08G64/083

    摘要: Thermoplastic polyphosphonatocarbonate prepared by polycondensing at least one aromatic dihydroxy compound with a diaryl carbonate and a phosphonic acid diaryl ester in the presence of a basic polycondensation catalyst at a temperature of from 80.degree. to 340.degree. and under a pressure of 600 to 0.1 mm Hg in an inert gaseous atmosphere, the molar ratio of diaryl carbonate to phosphonic diaryl ester being from 5:95 to 95:5 and the molar ratio of aromatic dihydroxy compound to the sum of diaryl carbonate and phosphonic acid diaryl ester being from 0.91:1 to 0.99:1, and following polycondensation, neutralizing said basic catalyst.

    摘要翻译: 在碱性缩聚催化剂存在下,在80〜340℃,600〜0.1mmHg的压力下,使至少一种芳族二羟基化合物与碳酸二芳基酯和膦酸二芳基酯缩聚而得到的热塑性聚磷酸酯 惰性气体气氛中,碳酸二芳酯与膦酸二芳基酯的摩尔比为5:95至95:5,芳族二羟基化合物与碳酸二芳基酯和膦酸二芳基酯的摩尔比为0.91:1至0.99 :1,并进行缩聚,中和所述碱性催化剂。

    Process for the preparation of thermoplastic aromatic
polyphosphonatocarbonates with improved heat-aging resistance, and
their use
    10.
    发明授权
    Process for the preparation of thermoplastic aromatic polyphosphonatocarbonates with improved heat-aging resistance, and their use 失效
    具有改善耐热老化性的热塑性芳族聚碳酸亚烃酯的制备方法及其用途

    公开(公告)号:US4508890A

    公开(公告)日:1985-04-02

    申请号:US493793

    申请日:1983-05-12

    CPC分类号: C08G64/00 C08G79/04

    摘要: Thermoplastic polyphosphonatocarbonates prepared by polycondensing at least one aromatic dihydroxy compound with a diaryl carbonate and a phosphonic acid diaryl ester in the presence of a catalyst selected from the group consisting of (a) tetra-C.sub.1 -C.sub.18 -alkyl titanates, (b) di-C.sub.2 -C.sub.4 -alkyl-tin oxides, (c) di-C.sub.2 -C.sub.4 -alkyl-di-C.sub.1 -C.sub.4 -alkoxy-tin compounds, (d) tetra-C.sub.3 -C.sub.18 -alkyl zirconates, (e) tri-C.sub.2 -C.sub.18 -alkyl vanadylates and (f) mixtures of germanium dioxide or titanium dioxide and at least one of (a) to (e) in a weight ratio of 1:3 to 3:1 at a temperature of from 80.degree.-340.degree. C. and under a pressure of 600 to 0.1 mm Hg in an inert gaseous atmosphere, the molar ratio of diaryl carbonate to phosphonic diaryl ester being from 5:95 to 95:5 and the molar ratio of aromatic dihydroxy compound to the sum of diaryl carbonates and phosphonic diaryl ester being from 0.91:1 to 0.99:1.

    摘要翻译: 在选自以下的催化剂存在下,将至少一种芳族二羟基化合物与碳酸二芳酯和膦酸二芳基酯缩聚制备的热塑性聚膦酸碳酸酯:(a)四-C1-烷基钛酸酯,(b)二 - (c)二-C2-C4-烷基 - 二-C1-C4烷氧基锡化合物,(d)四-C 3 -C 18烷基锆酸盐,(e)三-C2-烷基 - C18烷基氧钒酸酯和(f)二氧化锗或二氧化钛与至少一种(a)至(e)的混合物,重量比为1:3至3:1,温度为80-340℃ 并且在惰性气体气氛中在600至0.1mm Hg的压力下,碳酸二芳酯与膦酸二芳基酯的摩尔比为5:95至95:5,芳族二羟基化合物与碳酸二芳基酯的摩尔比 和膦酸二芳基酯为0.91:1至0.99:1。