公开(公告)号:US5891264A
公开(公告)日:1999-04-06
申请号:US956593
申请日:1997-10-23
申请人: Hisato Shinohara , Hisao Morooka , Izumi Ikeo , Akemi Takenouchi , Setsuo Nakajima , Yasuyuki Arai
发明人: Hisato Shinohara , Hisao Morooka , Izumi Ikeo , Akemi Takenouchi , Setsuo Nakajima , Yasuyuki Arai
IPC分类号: H01L31/04 , H01L31/0224
CPC分类号: H01L31/202 , H01L31/022425 , H01L31/0236 , H01L31/03685 , H01L31/03762 , H01L31/056 , H01L31/075 , H01L31/1804 , H01L31/1876 , Y02E10/52 , Y02E10/545 , Y02E10/547 , Y02E10/548 , Y02P70/521
摘要: An aluminum film is formed as a photoreflective electrode in the side opposite to the light incident side of a solar cell by sputtering at a substrate temperature of 50.degree. to 200.degree. C. using a target, aluminum containing silicon as an impurity element at 0.1 to 6.0 weight %. An aluminum film or a silver film into which an impurity element is not added is formed on the above aluminum film, to obtain a texture structure having convex and concave shapes. When an organic resin film substrate is used, components (released as a gas by heating and a vacuum atmosphere) such as water within the organic resin film is removed after the aluminum film is formed.
摘要翻译: 在50℃至200℃的基板温度下通过溅射在与太阳能电池的光入射侧相反的一侧形成铝膜作为光反射电极,使用目标,含铝硅作为杂质元素,在0.1〜 6.0重量%。 在上述铝膜上形成没有添加杂质元素的铝膜或银膜,以获得具有凸形和凹形的纹理结构。 当使用有机树脂膜基材时,在形成铝膜之后除去有机树脂膜内的水分等(通过加热气体和真空气体释放)。
-
公开(公告)号:US5711824A
公开(公告)日:1998-01-27
申请号:US579481
申请日:1995-12-27
申请人: Hisato Shinohara , Hisao Morooka , Izumi Ikeo , Akemi Takenouchi , Setsuo Nakajima , Yasuyuki Arai
发明人: Hisato Shinohara , Hisao Morooka , Izumi Ikeo , Akemi Takenouchi , Setsuo Nakajima , Yasuyuki Arai
IPC分类号: H01L31/04 , H01L31/0224
CPC分类号: H01L31/202 , H01L31/022425 , H01L31/0236 , H01L31/03685 , H01L31/03762 , H01L31/056 , H01L31/075 , H01L31/1804 , H01L31/1876 , Y02E10/52 , Y02E10/545 , Y02E10/547 , Y02E10/548 , Y02P70/521
摘要: An aluminum film is formed as a photoreflective electrode at the side opposite to the light incident side of a solar cell by sputtering at a substrate temperature of 50.degree. to 200.degree. C. using a target of aluminum containing silicon as an impurity element at 0.1 to 6.0 weight %. An aluminum film or a silver film in which an impurity element is not added is formed on the above aluminum film, to obtain a texture structure having convex and concave shapes. When an organic resin film substrate is used, components (released as a gas by heating in a vacuum atmosphere) such as water within the organic resin film are removed after the aluminum film is formed.
摘要翻译: 在50℃〜200℃的基板温度下通过溅射在与太阳能电池的光入射侧相反一侧的光反射电极上形成铝膜,使用含铝的硅作为杂质元素的目标为0.1〜 6.0重量%。 在上述铝膜上形成没有添加杂质元素的铝膜或银膜,以获得具有凸形和凹形的纹理结构。 当使用有机树脂膜基板时,在形成铝膜之后,除去有机树脂膜内的水分等(在真空气氛中,通过加热而被释放)。
-
公开(公告)号:US06722785B1
公开(公告)日:2004-04-20
申请号:US09599858
申请日:2000-06-23
申请人: Izumi Ikeo , Masatoshi Nakayama
发明人: Izumi Ikeo , Masatoshi Nakayama
IPC分类号: F16C3312
CPC分类号: F16C33/043 , F16C17/107 , F16C33/107 , F16C2370/12
摘要: A fluid dynamic bearing has a shaft (11) fitted in a sleeve (12) for rotation, with a fluid filled therebetween. The shaft (11) and/or sleeve (12) is formed with a pattern consisting of grooves (111g) and lands for generating a pressure distribution in the fluid and then covered with a diamond-like carbon film (11c) over the surface of the grooves and the surface of the lands.
摘要翻译: 流体动力轴承具有装配在套筒(12)中用于旋转的轴(11),其间填充有流体。 轴(11)和/或套筒(12)形成有由凹槽(111g)和平台组成的图案,用于在流体中产生压力分布,然后在金刚石状碳膜(11c)的表面上覆盖 凹槽和平台的表面。
-
-