Ferritic stainless steel sheet
    2.
    发明授权

    公开(公告)号:US11220732B2

    公开(公告)日:2022-01-11

    申请号:US16310956

    申请日:2017-06-15

    摘要: Provided is a ferritic stainless steel sheet excellent in shape of weld zone and corrosion resistance of a weld zone with a material of a different kind formed by performing welding with austenitic stainless steel.
    A ferritic stainless steel sheet having a chemical composition containing, by mass %, C: 0.003% to 0.020%, Si: 0.01% to 1.00%, Mn: 0.01% to 0.50%, P: 0.040% or less, S: 0.010% or less, Cr: 20.0% to 24.0%, Cu: 0.20% to 0.80%, Ni: 0.01% to 0.60%, Al: 0.01% to 0.08%, N: 0.003% to 0.020%, Nb: 0.40% to 0.80%, Ti: 0.01% to 0.10%, Zr: 0.01% to 0.10%, and the balance being Fe and inevitable impurities, in which relational expression (1) below is satisfied: 3.0≥Nb/(2Ti+Zr+0.5Si+5Al)≥1.5  (1), here, in relational expression (1), each of the atomic symbols denotes the content (mass %) of the corresponding chemical element.

    HIGH-STRENGTH GALVANIZED STEEL SHEET AND METHOD FOR MANUFACTURING THE SAME (AS AMENDED)
    3.
    发明申请
    HIGH-STRENGTH GALVANIZED STEEL SHEET AND METHOD FOR MANUFACTURING THE SAME (AS AMENDED) 审中-公开
    高强度钢化钢板及其制造方法(如修改)

    公开(公告)号:US20160047011A1

    公开(公告)日:2016-02-18

    申请号:US14779772

    申请日:2014-03-26

    摘要: A high-strength galvanized steel sheet has a chemical composition containing, by mass %, C: 0.16% or more and 0.24% or less, Si: 0.8% or more and 1.8% or less, Mn: 1.0% or more and 3.0% or less, P: 0.020% or less, S: 0.0040% or less, Al: 0.01% or more and 0.1% or less, N: 0.01% or less, Ca: 0.0001% or more and 0.0020% or less, and the balance including Fe and incidental impurities, and a microstructure, in which the total area ratio of a ferrite phase and a bainite phase with respect to the whole microstructure is 30% or more and 70% or less, in which the area ratio of a tempered martensite phase with respect to the whole microstructure is 20% or more and 40% or less, in which the area ratio of a retained austenite phase with respect to the whole microstructure is 10% or more and 20% or less, and in which the area ratio of a martensite phase with respect to the whole microstructure is 2% or more and 20% or less.

    摘要翻译: 高强度镀锌钢板具有以质量%计含有C:0.16%以上且0.24%以下,Si:0.8%以上且1.8%以下,Mn:1.0%以上3.0%以下的化学成分, 以下,P:0.020%以下,S:0.0040%以下,Al:0.01%以上且0.1%以下,N:0.01%以下,Ca:0.0001%以上且0.0020%以下, 余量包括Fe和杂质,以及相对于整个微观结构的铁素体相和贝氏体相的总面积比为30%以上且70%以下的微观结构,其中回火的面积比 相对于整个微观结构,马氏体相为20%以上且40%以下,残留奥氏体相相对于整个微观结构的面积比为10%以上且20%以下,其中 相对于整个微结构,马氏体相的面积比为2%以上且20%以下。

    FERRITIC STAINLESS STEEL SHEET
    4.
    发明申请

    公开(公告)号:US20200308677A1

    公开(公告)日:2020-10-01

    申请号:US16310956

    申请日:2017-06-15

    摘要: Provided is a ferritic stainless steel sheet excellent in shape of weld zone and corrosion resistance of a weld zone with a material of a different kind formed by performing welding with austenitic stainless steel.A ferritic stainless steel sheet having a chemical composition containing, by mass %, C: 0.003% to 0.020%, Si: 0.01% to 1.00%, Mn: 0.01% to 0.50%, P: 0.040% or less, S: 0.010% or less, Cr: 20.0% to 24.0%, Cu: 0.20% to 0.80%, Ni: 0.01% to 0.60%, Al: 0.01% to 0.08%, N:. 0.003% to 0.020%, Nb: 0.40% to 0.80%, Ti: 0.01% to 0.10%, Zr: 0.01% to 0.10%, and the balance being Fe and inevitable impurities, in which relational expression (1) below is satisfied: 3.0≥Nb/(2Ti+Zr+0.5 Si+5 Al)≥1.5   (1), here, in relational expression (1), each of the atomic symbols denotes the content (mass %) of the corresponding chemical element.

    High-strength galvanized steel sheet and method for manufacturing the same

    公开(公告)号:US10266906B2

    公开(公告)日:2019-04-23

    申请号:US14779772

    申请日:2014-03-26

    摘要: A high-strength galvanized steel sheet has a chemical composition containing, by mass %, C: 0.16% or more and 0.24% or less, Si: 0.8% or more and 1.8% or less, Mn: 1.0% or more and 3.0% or less, P: 0.020% or less, S: 0.0040% or less, Al: 0.01% or more and 0.1% or less, N: 0.01% or less, Ca: 0.0001% or more and 0.0020% or less, and the balance including Fe and incidental impurities, and a microstructure, in which the total area ratio of a ferrite phase and a bainite phase with respect to the whole microstructure is 30% or more and 70% or less, in which the area ratio of a tempered martensite phase with respect to the whole microstructure is 20% or more and 40% or less, in which the area ratio of a retained austenite phase with respect to the whole microstructure is 10% or more and 20% or less, and in which the area ratio of a martensite phase with respect to the whole microstructure is 2% or more and 20% or less.