    申请日:1997-04-14

    摘要: The oxyhalide rare earth doped laser glass of the present invention comprises the substitution of fluorine for oxygen in glasses having the general molar batch composition of 50% SiO.sub.2, 25% CaO, 25% Al.sub.2 O.sub.3 to improve the distribution of rare earth dopants in the glass. The general molar batch composition of the invention ranges from approximately 45-70% SiO.sub.2, 15-35% CaO, 10-25% Al.sub.2 O.sub.3, 4-15% Al.sub.2 F.sub.6, and 0.001-2% Er.sub.2 O.sub.3. This substitution of fluorine into the 2SiO.sub.2. Al.sub.2 O.sub.3. CaO glass system provides erbium doped laser glasses having a Er.sub.2 O.sub.3 batch content of 0.01 mole % Er.sub.2 O.sub.3 to 1.2 mole % Er.sub.2 O.sub.3 (500 ppm Er.sub.2 O.sub.3 to 5.68 wt. % Er.sub.2 O.sub.3) which show little to no concentration quenching and exhibit useful fluorescence lifetimes of approximately 6 milliseconds (ms) or greater.

    摘要翻译: 本发明的卤氧化物稀土掺杂激光玻璃包括在具有一般摩尔批次组成为50%SiO 2,25%CaO,25%Al 2 O 3的玻璃中用氟代替氧,以改善玻璃中稀土掺杂剂的分布。 本发明的一般摩尔批次组合物的范围为约45-70%的SiO 2,15-35%的CaO,10-25%的Al 2 O 3,4-15%的Al 2 F 6和0.001-2%的Er 2 O 3。 氟取代为2SiO2。 Al2O3。 CaO玻璃系统提供具有Er2O3批次含量为0.01摩尔%Er 2 O 3至1.2摩尔%Er 2 O 3(500ppm Er 2 O 3至5.68重量%Er 2 O 3)的掺铒激光玻璃,其显示出很少至无浓度猝灭并且显示出约6毫秒的有用荧光寿命 (ms)以上。

    Phosphotellurite-containing glasses, process for making same and articles comprising same
    6.
    发明授权
    Phosphotellurite-containing glasses, process for making same and articles comprising same 有权
    含磷光辉石的玻璃,其制造方法和包含其的制品

    公开(公告)号:US07754629B2

    公开(公告)日:2010-07-13

    申请号:US11703363

    申请日:2007-02-07

    IPC分类号: C03C3/16 C03C3/12

    CPC分类号: G02B1/02 C03C3/16

    摘要: Disclosed are glass materials generally belonging to the P2O5—ZnO—TeO2 system and process for making the same. The glass may comprise Bi2O3 as well. The high refractive index and low Tg materials are particularly suitable for refractive lens elements for use in portable optical devices. The process involves the use of P2O5 source materials with reduced amounts of reducing agents or a step of removing the reducing agents from such source materials by an oxidizing step such as calcination.