Ethylene copolymer compositions
    4.
    发明授权
    Ethylene copolymer compositions 失效
    乙烯共聚物组合物

    公开(公告)号:US06506866B2

    公开(公告)日:2003-01-14

    申请号:US08857816

    申请日:1997-05-16

    IPC分类号: C08F21002

    摘要: Disclosed is a novel ethylene copolymer by copolymerizing an ethylene and at least one comonomer selected from a compound represented by the formula H2C═CHR wherein R is an alkyl group or an aryl group, and a diene, by slurry polymerization process in the presence of a solid catalyst system comprising a support, a transition metal compound and an activator capable of converting the transition metal compound into a catalytically active transition metal complex. The produced copolymer has a density of from 0.870 to 0.980 and a molecular weight distribution (Mw/Mn) of from 3 to 10, and exhibiting GPC/FT-IR characteristics and CFC characteristics, both of which define a comonomer content distribution, wherein, in one aspect, the lower the molecular weight of a copolymer fraction in a molecular weight distribution of an ethylene copolymer, the lower the comonomer content of the copolymer fraction; and, in the other aspect, the higher the molecular weight of a copolymer fraction, the higher the comonomer content of the copolymer fraction, so that ethylene copolymer exhibits high impact strength and excellent ESCR properties. Further, the ethylene copolymer contains substantially no impurites such as a wax, a gel and the like. Thus, the ethylene copolymer and blend compositions therefrom can be advantageously used for the production of film, fibers, foams or sheets including blown film, cast films, laminate films, blow-molded articles, injection molded articles, pipes, coating materials for cables, and the like.

    摘要翻译: 公开了一种新型乙烯共聚物,其通过在存在下通过淤浆聚合方法将乙烯和至少一种选自式H2C = CHR表示的化合物(其中R为烷基或芳基)和二烯的共聚单体共聚 固体催化剂体系,其包括载体,过渡金属化合物和能够将过渡金属化合物转化为催化活性的过渡金属络合物的活化剂。 制得的共聚物的密度为0.870〜0.980,分子量分布(Mw / Mn)为3〜10,表现出GPC / FT-IR特性和CFC特性,均为共聚单体含量分布, 在一个方面,共聚物部分在乙烯共聚物的分子量分布中的分子量越低,共聚物部分的共聚单体含量越低; 而在另一方面,共聚物部分的分子量越高,共聚物部分的共聚单体含量越高,使得乙烯共聚物表现出高的冲击强度和优异的ESCR性能。 此外,乙烯共聚物基本上不含蜡,凝胶等等。 因此,乙烯共聚物及其共混组合物可有利地用于制造膜,纤维,泡沫或片材,包括吹塑薄膜,流延薄膜,层压薄膜,吹塑制品,注塑制品,管道,电缆用涂料, 等等。

    Supported catalyst component, supported catalyst, their preparation, and
addition polymerization process
    5.
    发明授权
    Supported catalyst component, supported catalyst, their preparation, and addition polymerization process 失效
    负载催化剂组分,负载催化剂,其制备和加成聚合方法

    公开(公告)号:US6043180A

    公开(公告)日:2000-03-28

    申请号:US909236

    申请日:1997-08-11

    摘要: A supported catalyst component prepared from a support material and an alumoxane, containing 15-40 weight percent of aluminum from the alumoxane (based on the total weight of the support material and alumoxane), said supported catalyst component being obtained by heating said support material and alumoxane under an inert atmosphere at a temperature of from about 85 to about 250.degree. C. for a period sufficient to fix said alumoxane to the support material, to provide a supported catalyst component; wherein not more than about 10 percent aluminum from said alumoxane and present in the supported catalyst component is extractable in a one-hour extraction with toluene at 90.degree. C. using 10 ml toluene per gram of supported catalyst component; and a transition metal compound, and a process for the preparation of the supported catalyst.

    摘要翻译: 由支撑材料和铝氧烷制备的负载型催化剂组分,所述铝氧烷包含来自铝氧烷的15-40重量%的铝(基于载体材料和铝氧烷的总重量),所述负载的催化剂组分通过加热所述载体材料和 铝氧烷在惰性气氛下在约85至约250℃的温度下持续足够的时间以将所述铝氧烷固定到载体材料上,以提供负载型催化剂组分; 其中不超过约10%的来自所述铝氧烷并存在于负载型催化剂组分中的铝在90℃下用甲苯萃取1小时,每克载体催化剂组分为10ml甲苯; 和过渡金属化合物,以及制备负载型催化剂的方法。