Silicon-carbon Composite Anode Material for Lithium Ion Batteries and A Preparation Method Thereof
    1.
    发明申请
    Silicon-carbon Composite Anode Material for Lithium Ion Batteries and A Preparation Method Thereof 有权
    用于锂离子电池的碳 - 碳复合阳极材料及其制备方法

    公开(公告)号:US20140147751A1

    公开(公告)日:2014-05-29

    申请号:US14005791

    申请日:2012-03-17

    IPC分类号: H01M4/36 C23C18/12 C23C16/26

    摘要: Disclosed in the invention are a silicon-carbon composite anode material for lithium ion batteries and a preparation method thereof The material consists of a porous silicon substrate and a carbon coating layer. The preparation method of the material comprises preparing a porous silicon substrate and a carbon coating layer. The silicon-carbon composite anode material for lithium ion batteries has the advantages of high reversible capacity, good cycle performance and good rate performance. The material respectively shows reversible capacities of 1,556 mAh, 1,290 mAh, 877 mAh and 474 mAh/g at 0.2 C, 1 C, 4 C and 15 C rates; the specific capacity remains above 1,500 mAh after 40 cycles at the rate of 0.2 C and the reversible capacity retention rate is up to 90 percent.

    摘要翻译: 本发明公开了一种锂离子电池用碳 - 碳复合负极材料及其制备方法。该材料由多孔硅基材和碳涂层组成。 该材料的制备方法包括制备多孔硅衬底和碳涂层。 用于锂离子电池的硅碳复合阳极材料具有可逆容量大,循环性能好,速率性能好的优点。 该材料分别显示在0.2C,1C,4C和15C速率下1,556mAh,1,290mAh,877mAh和474mAh / g的可逆容量; 40次循环后的比容量以0.2C的比例保持在1500mAh以上,可逆容量保持率高达90%。

    ELECTRODE FOR LITHIUM ION BATTERIES AND THE METHOD FOR MANUFACTURING THE SAME
    7.
    发明申请
    ELECTRODE FOR LITHIUM ION BATTERIES AND THE METHOD FOR MANUFACTURING THE SAME 审中-公开
    锂离子电池用电极及其制造方法

    公开(公告)号:US20130316244A1

    公开(公告)日:2013-11-28

    申请号:US13989268

    申请日:2011-11-23

    IPC分类号: H01M4/36 H01M4/04

    摘要: An electrode is formed of a ternary composite of silicon, carbon, and carbon filter foil, for lithium ion batteries. Also described is a method for manufacturing silicon/carbon/carbon fiber foil composite electrode for lithium batteries, including: mixing silicon and an organic substance capable of forming carbon after heat treatment, in a solvent, to form a slurry; immersing the carbon fiber foil in said slurry until the slurry coats on and penetrates into the carbon fiber foil; and heating the carbon fiber foil, which has been coated and penetrated with the slurry, in an inert gas atmosphere or all inert gas atmosphere mixed with a reductive gas at a temperature of at least 400° C. for at least 2 hours.

    摘要翻译: 电极由用于锂离子电池的硅,碳和碳过滤箔的三元复合材料形成。 还描述了一种用于制造用于锂电池的硅/碳/碳纤维箔复合电极的方法,包括:在溶剂中将硅和能够在热处理后形成碳的有机物混合在一起形成浆料; 将碳纤维箔浸渍在所述浆料中直到浆料涂覆并渗透到碳纤维箔中; 并且在惰性气体气氛或与还原气体混合的所有惰性气体气氛中,在至少400℃的温度下加热已经用浆料涂覆和渗透的碳纤维箔至少2小时。

    ADJUSTING STRUCTURE AND STAND FOR PHOTOGRAPHIC APPARATUS

    公开(公告)号:US20240052967A1

    公开(公告)日:2024-02-15

    申请号:US17983667

    申请日:2022-11-09

    IPC分类号: F16M11/04 F16M11/32 G03B17/56

    摘要: The invention discloses an adjusting structure and a stand for photographic apparatus. The adjusting structure includes a first adjusting rod, a first connecting member, a second connecting member, a second adjusting rod, a first locking member and a supporting member. The first connecting member is fixedly connected with the first adjusting rod, the second connecting member is rotationally connected with the first connecting member and is provided with a first mounting hole, wherein the second connecting member can be rotated relative to the first connecting member to adjust an included angle with the first connecting member, the second adjusting rod is penetrated through the first mounting hole and movablely connected with the first adjusting rod, and can be moved relative to the first adjusting rod along a straight direction.