Thermoplastic compositions of polyurethanes and partly crosslinked alkyl
acrylate copolymers
    5.
    发明授权
    Thermoplastic compositions of polyurethanes and partly crosslinked alkyl acrylate copolymers 失效
    聚氨酯和部分交联丙烯酸酯共聚物的热塑性组合物

    公开(公告)号:US5237001A

    公开(公告)日:1993-08-17

    申请号:US713663

    申请日:1991-06-11

    摘要: The present invention is directed to a thermoplastic composition which is a blend of A) a thermoplastic polyurethane and B) an at least partly crosslinked alkyl acrylate copolymer of a C.sub.1-6 alkyl acrylate and a monomer selected from the group consisting of acrylonitrile, styrene, vinyl acetate, C.sub.1-6 alkyl methacrylates and mixtures thereof. The preferred compositions also contain copolymer selected from the group consisting ofC1) a thermoplastic graft product of a rubber component having a glass transition temperature below 0.degree. C., which serves as the graft base, and at least one graft monomer selected from the group consisting of styrene, .alpha.-methyl styrene, acrylonitrile an C.sub.1-6 alkyl methacrylate,C2) a rubber-free resin copolymer of styrene or .alpha.-methyl styrene with acrylonitrile,C3) mixtures thereof.

    摘要翻译: 本发明涉及一种热塑性组合物,其是A)热塑性聚氨酯和B)至少部分交联的丙烯酸C 1-6烷基酯与选自丙烯腈,苯乙烯, 乙酸乙烯酯,甲基丙烯酸C 1-6烷基酯及其混合物。 优选的组合物还包含共聚物,其选自C1)玻璃化转变温度低于0℃的橡胶组分的热塑性接枝产物,其用作接枝基质,和至少一种选自以下的接枝单体 由苯乙烯,α-甲基苯乙烯,丙烯腈和甲基丙烯酸C 1-6烷基酯组成,C2)苯乙烯或α-甲基苯乙烯与丙烯腈的无橡胶树脂共聚物,C3)其混合物。

    Mixtures of thermoplastic polymers in powder form
    6.
    发明授权
    Mixtures of thermoplastic polymers in powder form 失效
    粉末形式的热塑性聚合物的混合物

    公开(公告)号:US5112910A

    公开(公告)日:1992-05-12

    申请号:US743678

    申请日:1991-08-12

    摘要: Process for the preparation of mixtures of thermoplastic polymers in powder form from aqueous emulsions ofa) particulate, partly crosslinked rubber-like copolymers of a C.sub.2 -C.sub.8 -alkyl acrylate and/or butadiene with (based on the copolymer) up to 40 wt. % acrylonitrile, styrene or C.sub.1 -C.sub.4 -alkyl methacrylate,b) a thermoplastic resin, and if appropriatec) a rubber-rich graft polymer of styrene, .alpha.-methylstyrene, acrylonitrile, methyl methacrylate and/or alkyl acrylate on a diene or alkyl acrylate rubber having a rubber content of 50 to 95 wt. %,wherein aqueous emulsions of a) and b) and if appropriate c) having polymer contents of 15 to 50 wt. % are mixed with a coagulate solution simultaneously, but in separate streams, continuously or semi-continuously at 20.degree. to 100.degree. C., the polymers a) and b) and if appropriate c) being coagulated, the streams are combined and the polymer mixture is then separated off.

    摘要翻译: 制备粉末形式的热塑性聚合物的混合物的方法,该方法由以下混合物的水性乳液制备:a)丙烯酸C 2 -C 8烷基酯和/或丁二烯与(基于共聚物)的至少40重量%的颗粒部分交联的橡胶状共聚物。 丙烯腈,苯乙烯或甲基丙烯酸C 1 -C 4烷基酯,b)热塑性树脂,如果合适,c)在二烯或烷基上的苯乙烯,α-甲基苯乙烯,丙烯腈,甲基丙烯酸甲酯和/或丙烯酸烷基酯的富含橡胶的接枝聚合物 丙烯酸酯橡胶,其橡胶含量为50〜95重量% %,其中a)和b)和如果合适的水性乳液c)具有15至50重量%的聚合物含量。 %与凝固溶液同时混合,但在单独的流中,在20℃至100℃连续或半连续,聚合物a)和b),如果合适,c)凝结,将流合并,聚合物 混合物然后分离出来。

    Impact resistant polyamide moulding compounds modified with silicone
graft rubbers
    7.
    发明授权
    Impact resistant polyamide moulding compounds modified with silicone graft rubbers 失效
    用聚硅氧烷接枝橡胶改性的耐冲击聚酰胺模塑料

    公开(公告)号:US4945124A

    公开(公告)日:1990-07-31

    申请号:US294216

    申请日:1989-01-09

    摘要: This invention relates to polyamides which have been modified with special silicone graft rubbers to render them impact resistant and are tough at low temperatures and have high processing stability even at high temperatures and good surface properties.The moulding compounds, which are distinguished by excellent mechanical properties even at low temperatures, consist of at least 40% by weight of polyamide and special graft rubbers with a multishell core/sheath structure having a silicone-based core.

    摘要翻译: 本发明涉及用特殊硅氧烷接枝橡胶改性的聚酰胺,使其具有耐冲击性,并且在低温下是韧性的,即使在高温下也具有高的加工稳定性和良好的表面性能。 即使在低温下也被优异的机械性能区分的成型化合物由至少40重量%的聚酰胺和具有硅酮核的多壳芯/鞘结构的特殊接枝橡胶组成。

    Thermoplastic moulding compounds of polyamides and resin copolymers
    8.
    发明授权
    Thermoplastic moulding compounds of polyamides and resin copolymers 失效
    聚酰胺和树脂共聚物的热塑性模塑料

    公开(公告)号:US5340876A

    公开(公告)日:1994-08-23

    申请号:US88415

    申请日:1993-07-07

    IPC分类号: C08L77/00 C08L25/14 C08L33/06

    CPC分类号: C08L77/00

    摘要: This invention relates to thermoplastic moulding compounds with improved properties, in particular with reduced water absorption and rigidity and improved impact strength, from polyamides A and a thermoplastic resin copolymer B containing at least one (meth)acrylic acid ester of a tertiary alcohol in quantities of up to 35% by weight in addition to the other monomers such as styrene or (meth)acrylic esters. The invention also relates to rigid moulding compounds which are tough at low temperatures and are obtained from polyamides and the thermoplastic resin copolymers defined above and in addition contain a rubber polymer C in quantities of up to 35% by weight.

    摘要翻译: 本发明涉及具有改进的性能,特别是具有降低的吸水性和刚性以及改进的冲击强度的热塑性模塑料,其由聚酰胺A和含有至少一种叔醇的(甲基)丙烯酸酯的热塑性树脂共聚物B组成,其量为 除了其它单体如苯乙烯或(甲基)丙烯酸酯之外,还含有至多35重量%。 本发明还涉及在低温下韧性并且由聚酰胺和上述定义的热塑性树脂共聚物获得并且另外含有高达35重量%的橡胶聚合物C的刚性模塑料。

    High-impact dimensionally stable polyamide molding compositions
    9.
    发明授权
    High-impact dimensionally stable polyamide molding compositions 失效
    高冲击尺寸稳定的聚酰胺模塑组合物

    公开(公告)号:US4822852A

    公开(公告)日:1989-04-18

    申请号:US112532

    申请日:1987-10-26

    CPC分类号: C08L77/00 C08L51/04 C08L83/10

    摘要: The invention relates to thermoplastic molding compositions showing improved properties, more especially improved dimensional stability and notched impact strength, particularly at low temperatures, in the form of a mixture of at least 35% by weight of a copolyamide containing polydiorganosiloxane carbonamide units and/or of a mixture of partly crystalline polyamides and (co)polyamides containing polydiorganosiloxane carbonamide units and from 1 to 65% by weight of graft products of vinyl polymers on rubbers.The invention also relates to the dimensionally stable molding compositions tough at low temperatures characterized above which additionally contain amorphous siloxane-free polyamides added in quantities of up to 64% by weight.

    摘要翻译: 本发明涉及热塑性模塑组合物,其显示出改进的性能,特别是改进的尺寸稳定性和缺口冲击强度,特别是在低温下,以至少35重量%的含有聚二有机硅氧烷碳酰胺单元的共聚酰胺和/或 部分结晶聚酰胺和含有聚二有机硅氧烷碳酰胺单元的(共)聚酰胺的混合物和1至65重量%的橡胶上的乙烯基聚合物的接枝产物。 本发明还涉及在低温下韧性的尺寸稳定的模塑组合物,其特征在于其上另外含有以高达64重量%的量加入的无定形无硅氧烷聚酰胺。