PROCESS FOR PRODUCING FLUORESCENT SUBSTANCE AND FLUORESCENT SUBSTANCE PRODUCED THEREBY
    4.
    发明申请
    PROCESS FOR PRODUCING FLUORESCENT SUBSTANCE AND FLUORESCENT SUBSTANCE PRODUCED THEREBY 审中-公开
    生产荧光物质的方法和生产的荧光物质

    公开(公告)号:US20150001445A1

    公开(公告)日:2015-01-01

    申请号:US14453302

    申请日:2014-08-06

    IPC分类号: C09K11/77

    摘要: The present invention provides a fluorescent substance excellent both in quantum efficiency and in temperature characteristics, and also provides a process for producing the fluorescent substance. This fluorescent substance is an oxynitride phosphor having a low paramagnetic defect density and comprising aluminum, silicon, either or both of oxygen and nitrogen, and a metal element M, provided that the metal element M is partly replaced with an emission center element R. That phosphor can be produced by the steps of: subjecting a mixture of starting materials to heat treatment under a nitrogen atmosphere so as to obtain an intermediate fired product, and then further subjecting the intermediate fired product to heat treatment under an atmosphere of nitrogen-hydrogen mixed gas.

    摘要翻译: 本发明提供了在量子效率和温度特性方面优异的荧光物质,并且还提供了制造荧光物质的方法。 该荧光物质是具有低顺磁性缺陷密度的氧氮化物荧光体,并且包含铝,硅,氧和氮中的任一种或两者以及金属元素M,条件是金属元素M部分地被发射中心元素R替代。 可以通过以下步骤制造荧光体:在氮气气氛下对起始材料的混合物进行热处理,得到中间焙烧产物,然后在氮 - 氢混合气氛下进一步对中间焙烧产物进行热处理 加油站。

    RED LIGHT-EMITTING FLUORESCENT SUBSTANCE AND LIGHT-EMITTING DEVICE EMPLOYING THE SAME
    5.
    发明申请
    RED LIGHT-EMITTING FLUORESCENT SUBSTANCE AND LIGHT-EMITTING DEVICE EMPLOYING THE SAME 有权
    红色发光荧光物质和使用其的发光装置

    公开(公告)号:US20130214305A1

    公开(公告)日:2013-08-22

    申请号:US13775597

    申请日:2013-02-25

    IPC分类号: C09K11/77 H01L27/15

    摘要: The embodiment provides a red light-emitting fluorescent substance represented by the following formula (1): (M1-xECx)aM1bAlOcNd   (1). In the formula (1), M is an element selected from the group consisting of IA group elements, IIA group elements, IIIA group elements, IIIB group elements, rare earth elements and IVA group elements; EC is an element selected from the group consisting of Eu, Ce, Mn, Tb, Yb, Dy, Sm, Tm, Pr, Nd, Pm, Ho, Er, Cr, Sn, Cu, Zn, As, Ag, Cd, Sb, Au, Hg, TI, Pb, Bi and Fe; M1 is different from M and is selected from the group consisting of tetravalent elements; and x, a, b, c and d are numbers satisfying the conditions of 0

    摘要翻译: 本实施方案提供由下式(1)表示的红色发光荧光物质:(M1-xECx)aM1bAlOcNd(1)。 在式(1)中,M是选自IA族元素,IIA族元素,IIIA族元素,IIIB族元素,稀土元素和IVA族元素的元素; EC是选自Eu,Ce,Mn,Tb,Yb,Dy,Sm,Tm,Pr,Nd,Pm,Ho,Er,Cr,Sn,Cu,Zn,As,Ag,Cd, Sb,Au,Hg,TI,Pb,Bi和Fe; M1与M不同,选自四价元素; x,a,b,c和d分别是满足0

    LUMINESCENT MATERIAL
    7.
    发明申请
    LUMINESCENT MATERIAL 有权
    发光材料

    公开(公告)号:US20140092600A1

    公开(公告)日:2014-04-03

    申请号:US13837836

    申请日:2013-03-15

    IPC分类号: C09K11/77 F21K99/00

    摘要: According to one embodiment, the luminescent material exhibits a luminescence peak in a wavelength ranging from 490 to 580 nm when excited with light having an emission peak in a wavelength ranging from 250 to 500 nm. The luminescent material has a diffraction peak intensity of the largest peak detected at 2θ=30.1-31.1° that is higher than the diffraction peak intensity of the peak detected at 2θ=25.0-26.0° in X-ray diffraction by the Bragg-Brendano method using Cu-Kα line and its composition is represented by (Sr1−xEux)3−yAl3+zSi13−zO2+uN21−w (a part of the Sr may be substituted by at least one selected from Ba, Ca, Mg and Na, 0

    摘要翻译: 根据一个实施方案,当用波长范围为250-500nm的发光峰激发时,发光材料在490-580nm的波长范围内表现出发光峰。 发光材料具有在2θ时检测到的最大峰值的衍射峰强度; = 30.1-31.1°,高于在2θ时检测到的峰的衍射峰强度; = 25.0-26.0°,通过Bragg- 使用Cu-Kα线的Brendano方法及其组成由(Sr1-xEux)3-yAl3 + zSi13-zO2 + uN21-w(Sr的一部分可以被选自Ba,Ca,Mg中的至少一种或 Na,0