摘要:
In a method for producing a hot strip of steel with material properties that are adjustable over the strip cross-section, a steel melt is fed onto a revolving casting belt of a horizontal strip casting facility and solidifies to form a pre-strip having a thickness between 6 and 20 mm, and the pre-strip is subjected to a hot rolling process after complete solidification. A gas jet or plasma jet composed of metallic and/or non-metallic elements that affect the material properties of the hot strip influences the steel melt that is still liquid and/or just about to start to solidify. The concentration of the elements introduced into the melt by the gas jet or plasma jet and diffusing into the melt is adjusted across the strip thickness and strip width by changing the influencing kinetic energy of the gas jet or plasma jet, the partial gas pressure and/or the applied temperature.
摘要:
In a method for producing a hot strip of steel with material properties that are adjustable over the strip cross-section, a steel melt is fed onto a revolving casting belt of a horizontal strip casting facility and solidifies to form a pre-strip having a thickness between 6 and 20 mm, and the pre-strip is subjected to a hot rolling process after complete solidification. A gas jet or plasma jet composed of metallic and/or non-metallic elements that affect the material properties of the hot strip influences the steel melt that is still liquid and/or just about to start to solidify. The concentration of the elements introduced into the melt by the gas jet or plasma jet and diffusing into the melt is adjusted across the strip thickness and strip width by changing the influencing kinetic energy of the gas jet or plasma jet, the partial gas pressure and/or the applied temperature.
摘要:
A transformable lightweight structural steel, which exhibits a resistance to hydrogen embrittlement, has TRIP and TWIP properties and contains the following elements (in wt.-%): C 0.05 to 0.05; Mn 9.0 to =25.0; H
摘要翻译:具有耐氢脆性的可变形轻质结构钢具有TRIP和TWIP性质,并含有以下元素(重量%):C 0.05至<= 1.0; Al 0.0〜<= 11.0; Si 0.0〜<= 6.0; Al + Si> 0.05; Mn 9.0〜= 25.0; H <20ppm,其余为铁,包括附带的钢伴侣元素,根据合金组成,存在不同的相。 轻质结构钢的特征在于使较高的C含量与较低的Mn含量相关联并使低C含量与较高的Mn含量相关联,C-Mn值对位于C-Mn坐标系中,大约在直接连接 远离C-Mn值对的连接线的线在奥氏体相和马氏体相之间处于平衡状态。
摘要:
The invention relates to a casting nozzle for a horizontal strip casting system, in particular for casting steel strip, wherein the nozzle is designed as a narrow rectangular hollow block having a bottom, top and two side walls and made of refractory material, the outflow region being located only slightly above a cooled continuous belt receiving the outflowing melt. Viewed in the flow direction, it is provided that the clear cross-section of the hollow block in the outflow region reduces uniformly in the direction toward the outflow and the end face of the bottom of the hollow block is designed with respect to the surface of the continuous belt such that the melt contacts the continuous belt perpendicularly.
摘要:
The invention relates to a casting nozzle for a horizontal strip casting system, especially for casting steel strip. The casting nozzle is connected to a feed channel and is designed as a rectangular refractory hollow block, the outlet region of which being only slightly above the cooled continuous belt which accommodates the outflowing melt. The hollow block is subdivided at least once in the direction of casting and a narrow sealing element is arranged on the partition side of the segments, the width of the remaining gaps in the partition area being selected as to close when the casting nozzle is operated.
摘要:
The invention relates to a casting nozzle for a horizontal strip casting system, in particular for casting steel strip, wherein the nozzle is designed as a narrow rectangular hollow block having a bottom, top and two side walls and made of refractory material, the outflow region being located only slightly above a cooled continuous belt receiving the outflowing melt. Viewed in the flow direction, it is provided that the clear cross-section of the hollow block in the outflow region reduces uniformly in the direction toward the outflow and the end face of the bottom of the hollow block is designed with respect to the surface of the continuous belt such that the melt contacts the continuous belt perpendicularly.
摘要:
The invention relates to a casting nozzle for a horizontal strip casting system, especially for casting steel strip. The casting nozzle is connected to a feed channel and is designed as a rectangular refractory hollow block, the outlet region of which being only slightly above the cooled continuous belt which accommodates the outflowing melt. The hollow block is subdivided at least once in the direction of casting and a narrow sealing element is arranged on the partition side of the segments, the width of the remaining gaps in the partition area being selected as to close when the casting nozzle is operated.
摘要:
The invention relates to a method for producing a hot strip from a triplex lightweight steel, wherein a melt is cast into a roughed strip and the latter is subsequently rolled into a hot strip. For this purpose, it is provided that the melt is cast in a horizontal strip casting facility under conditions of a calm flow and free of bending into a roughed strip in the range between 6 and 20 mm and is subsequently rolled into hot strip having a degree of deformation of at least 50%.
摘要:
The invention relates to a device for the horizontal continuous strip casting of steel, especially steel with high manganese content, for producing a pre-strip with a thickness ≦15 mm. The device includes a tundish containing the melt, a primary cooling zone having two deflection pulleys and a revolving cooled conveyor belt, and a secondary cooling zone which follows the primary cooling zone and has a housed roller table. A guide element having at least one roller is hereby arranged at the end of the primary cooling zone and before the start of the secondary cooling zone.
摘要:
The invention relates to a method for producing a hot strip from transformation-free ferritic steel, wherein a melt is cast into a roughed strip and the latter is subsequently rolled into a hot strip. For this purpose, it is provided that the melt is cast in a horizontal strip casting facility under conditions of a calm flow and free of bending into a roughed strip in the range between 6 and 20 mm and is subsequently rolled into hot strip having a degree of deformation of at least 50%.