摘要:
The present invention provides a method of producing a lithium mixed metal oxide, a lithium mixed metal oxide and a nonaqueous electrolyte secondary battery. The method includes a step of calcining a mixture of one or more compounds of M wherein M is one or more elements selected from the group consisting of nickel, cobalt and manganese, and a lithium compound, in the presence of one or more inactive fluxes selected from the group consisting of a fluoride of A, a chloride of A, a carbonate of A, a sulfate of A, a nitrate of A, a phosphate of A, a hydroxide of A, a molybdate of A and a tungstate of A, wherein A is one or more elements selected from the group consisting of Na, K, Rb, Cs, Ca, Mg, Sr and Ba. The lithium mixed metal oxide contains nickel, cobalt and manganese, has a BET specific surface area of from 3 m2/g to 15 m2/g, and has an average particle diameter within a range of 0.1 μm or more to less than 1 μm, the diameter determined by a laser diffraction scattering method.
摘要:
A lithium mixed metal oxide, shown by the following formula (A): Lix(Mn1−y−z−dNiyFezMd)O2 (A) wherein M is one or more elements selected from the group consisting of Al, Mg, Ti, Ca, Cu, Zn, Co, Cr, Mo, Si, Sn, Nb and V; x is 0.9 or more and 1.3 or less; y is 0.3 or more and 0.7 or less; z is more than 0 and 0.1 or less, and d is more than 0 and 0.1 or less. A positive electrode active material, including the lithium mixed metal oxide. A positive electrode, including the positive electrode active material. A nonaqueous electrolyte secondary battery, including the positive electrode.
摘要:
A lithium mixed metal oxide, shown by the following formula (A): Lix(Mn1-y-z-dNiyFezMd)O2 (A) wherein M is one or more elements selected from the group consisting of Al, Mg, Ti, Ca, Cu, Zn, Co, Cr, Mo, Si, Sn, Nb and V; x is 0.9 or more and 1.3 or less; y is 0.3 or more and 0.7 or less; z is more than 0 and 0.1 or less, and d is more than 0 and 0.1 or less. A positive electrode active material, including the lithium mixed metal oxide. A positive electrode, including the positive electrode active material. A nonaqueous electrolyte secondary battery, including the positive electrode.
摘要:
The present invention provides a positive electrode active material. The positive electrode active material is represented by the following formula (I) and has a BET specific surface area of larger than 5 m2/g and not larger than 15 m2/g: LixM1yM31-yO2 (I) wherein M1 is at least one transition metal element selected from Group 5 elements and Group 6 elements of the Periodic Table, M3 is at least one transition metal element other than M1 and selected from among transition metal elements excluding Fe, x is not less than 0.9 and not more than 1.3, and y is more than 0 and less than 1.
摘要:
The present invention provides a positive electrode active material. The positive electrode active material is represented by the following formula (I) and has a BET specific surface area of larger than 5 m2/g and not larger than 15 m2/g: LixM1yM31-yO2 (I) wherein M1 is at least one transition metal element selected from Group 5 elements and Group 6 elements of the Periodic Table, M3 is at least one transition metal element other than M1 and selected from among transition metal elements excluding Fe, x is not less than 0.9 and not more than 1.3, and y is more than 0 and less than 1.
摘要:
The present invention provides a positive electrode active material. The positive electrode active material is represented by the following formula (I) and has a BET specific surface area of larger than 5 m2/g and not larger than 15 m2/g: LixM1yM31-yO2 (I) wherein M1 is at least one transition metal element selected from Group 5 elements and Group 6 elements of the Periodic Table, M3 is at least one transition metal element other than M1 and selected from among transition metal elements excluding Fe, x is not less than 0.9 and not more than 1.3, and y is more than 0 and less than 1.
摘要:
The present invention provides a method of producing a lithium mixed metal oxide, a lithium mixed metal oxide and a nonaqueous electrolyte secondary battery. The method includes a step of calcining a mixture of one or more compounds of M wherein M is one or more elements selected from the group consisting of nickel, cobalt and manganese, and a lithium compound, in the presence of one or more inactive fluxes selected from the group consisting of a fluoride of A, a chloride of A, a carbonate of A, a sulfate of A, a nitrate of A, a phosphate of A, a hydroxide of A, a molybdate of A and a tungstate of A, wherein A is one or more elements selected from the group consisting of Na, K, Rb, Cs, Ca, Mg, Sr and Ba. The lithium mixed metal oxide contains nickel, cobalt and manganese, has a BET specific surface area of from 3 m2/g to 15 m2/g, and has an average particle diameter within a range of 0.1 μm or more to less than 1 μm, the diameter determined by a laser diffraction scattering method.
摘要:
A method of producing a layered structure lithium mixed metal oxide, including a step of calcining a lithium mixed metal oxide raw material containing a transition metal element and a lithium element in a molar ratio of the lithium element to the transition metal element of 1 or more and 2 or less, in the presence of an inactive flux containing one or more compounds selected from the group consisting of a carbonate of M, a sulfate of M, a nitrate of M, a phosphate of M, a hydroxide of M, a molybdate of M, and a tungstate of M, wherein M represents one or more elements selected from the group consisting of Na, K, Rb, Cs, Ca, Mg, Sr and Ba.
摘要:
A method for producing a layered lithium mixed metal oxide according to the present invention comprises a step of calcining, in the presence of an inert flux composed of a chloride, a lithium mixed metal oxide raw material containing a transition metal element and a lithium element so that the molar ratio of the lithium element to the transition metal element may fall within a range of 1 or more and 2 or less.
摘要:
A lithium mixed metal oxide comprising Ni, Mn and Fe and having a BET specific surface area of 2 m2/g or more and 30 m2/g or less. A method of producing a lithium mixed metal oxide, comprising bringing an aqueous solution containing Ni, Mn, Fe and Cl into contact with an alkali to obtain a coprecipitate, and calcining a mixture of the coprecipitate and a lithium compound by maintaining the mixture at a temperature of lower than 900° C. A positive electrode active material for nonaqueous electrolyte secondary battery, comprising the lithium mixed metal oxide described above or the lithium mixed metal oxide obtained by the method of producing a lithium mixed metal oxide described above as a main ingredient. A positive electrode for nonaqueous electrolyte secondary battery having the positive electrode active material for nonaqueous electrolyte secondary battery described above.