FUEL PART AND PROCESS FOR PRODUCING OF A FUEL PART
    3.
    发明申请
    FUEL PART AND PROCESS FOR PRODUCING OF A FUEL PART 有权
    燃料部分和燃料部件生产过程

    公开(公告)号:US20130261245A1

    公开(公告)日:2013-10-03

    申请号:US13812195

    申请日:2011-07-21

    IPC分类号: C08L77/02

    摘要: This invention relates to a fuel part, comprising a polymer composition comprising: i. a polyamide A in which the ratio of terminal carboxy group concentration over terminal amino group concentration of the polyamide A is equal to 1 or higher, and ii. micro talcum in an amount of 0.001 to 1 weight percent with respect to the total amount of the polymer composition, and iii. an impact modifier in an amount of at least 1.0 weight percent with respect to the total amount of the polymer composition. This invention also relates to a process for producing a fuel part.

    摘要翻译: 本发明涉及燃料部分,其包括聚合物组合物,其包含:i。 其中末端羧基浓度与聚酰胺A的氨基末端浓度的比例等于1或更高的聚酰胺A,以及ii。 相对于聚合物组合物的总量,微滑石的量为0.001〜1重量%,iii。 相对于聚合物组合物的总量,抗冲改性剂的量为至少1.0重量%。 本发明还涉及燃料部件的制造方法。

    FUEL PART AND PROCESS FOR PREPARATION OF A FUEL PART
    4.
    发明申请
    FUEL PART AND PROCESS FOR PREPARATION OF A FUEL PART 有权
    燃料部分和燃料部分的制备过程

    公开(公告)号:US20130281599A1

    公开(公告)日:2013-10-24

    申请号:US13812314

    申请日:2011-07-21

    IPC分类号: C08K3/34 B29C49/00

    摘要: The present invention relates to a fuel part, comprising a polymer composition comprising: i. a polyamide A, and ii. micro talcum in an amount of 0.001 to 1 weight percent with respect to the total amount of the polymer composition, wherein the polymer composition has a melt volume flow rate (MVR) of at most 70 cm3/10 min at a weight of 21.6 kg and at a temperature of Tmeasure as measured according to ISO 1133. The invention also relates to a process for preparation of such fuel part wherein a blow-molding or roto-molding process is applied.

    摘要翻译: 本发明涉及一种燃料部件,其包括聚合物组合物,其包含:i。 聚酰胺A,和ii。 相对于聚合物组合物的总量为0.001〜1重量%的微滑石,其中聚合物组合物的熔体体积流动速率(MVR)为21.6千克的重量为70厘米3/10分钟以下, 在根据ISO 1133测量的Tmeasure温度下。本发明还涉及一种制备这种燃料部件的方法,其中应用吹塑或旋转成型方法。

    Fuel part and process for producing of a fuel part
    6.
    发明授权
    Fuel part and process for producing of a fuel part 有权
    燃料部件和燃料部件的制造方法

    公开(公告)号:US09309406B2

    公开(公告)日:2016-04-12

    申请号:US13812195

    申请日:2011-07-21

    摘要: This invention relates to a fuel part, comprising a polymer composition comprising: i. a polyamide A in which the ratio of terminal carboxy group concentration over terminal amino group concentration of the polyamide A is equal to 1 or higher, and ii. micro talcum in an amount of 0.001 to 1 weight percent with respect to the total amount of the polymer composition, and iii. an impact modifier in an amount of at least 1.0 weight percent with respect to the total amount of the polymer composition. This invention also relates to a process for producing a fuel part.

    摘要翻译: 本发明涉及燃料部分,其包括聚合物组合物,其包含:i。 其中末端羧基浓度与聚酰胺A的氨基末端浓度的比例等于1或更高的聚酰胺A,以及ii。 相对于聚合物组合物的总量,微滑石的量为0.001〜1重量%,iii。 相对于聚合物组合物的总量,抗冲改性剂的量为至少1.0重量%。 本发明还涉及燃料部件的制造方法。

    Process for preparing injection molded parts with decreased glass fiber read out
    7.
    发明授权
    Process for preparing injection molded parts with decreased glass fiber read out 有权
    制备玻璃纤维减少的注塑件的方法

    公开(公告)号:US09399314B2

    公开(公告)日:2016-07-26

    申请号:US13203522

    申请日:2010-02-08

    摘要: The present invention relates to a process for preparing an injection molded part, comprising the following steps: a preparing a glass fiber reinforced polyamide-6 composition with a relative viscosity of less than 2.4; b heating a such composition to obtain a viscous liquid; c filling a mold cavity with the viscous liquid with a filling time of at least 0.8 s; d leaving the viscous liquid in the mold under pressure until it cools to form a part; e opening the mold; f ejecting the part; wherein the polyamide-6 composition has a crystallization temperature under hyper DSC conditions of less than 168° C. The invention also relates to an injection molded part a having a maximum wall thickness of at least 2.5 mm; and/or b a part weight of at least 100 g per injection point; wherein the part consists of a glass fiber reinforced semi-crystalline polyamide-6 composition having a relative solution viscosity of less than 2.4, wherein the polyamide-6 composition has a crystallization temperature under hyper DSC conditions of less than 168° C.

    摘要翻译: 本发明涉及一种注射成型部件的制备方法,包括以下步骤:制备相对粘度小于2.4的玻璃纤维增​​强聚酰胺-6组合物; b加热这样的组合物以获得粘稠液体; c用粘稠液体填充模腔,填充时间至少为0.8s; d在压力下将粘性液体留在模具中直到其冷却以形成部件; 打开模具; f弹出零件; 其中所述聚酰胺-6组合物在超过DSC条件下的结晶温度低于168℃。本发明还涉及具有至少2.5mm的最大壁厚的注塑部分a; 和/或b每个注射点至少100g的部分重量; 其中该部分由相对溶液粘度小于2.4的玻璃纤维增​​强半结晶聚酰胺-6组合物组成,其中聚酰胺-6组合物在高DSC条件下的结晶温度小于168℃。

    PROCESS FOR PREPARING INJECTION MOLDED PARTS WITH DECREASED GLASS FIBER READ OUT
    9.
    发明申请
    PROCESS FOR PREPARING INJECTION MOLDED PARTS WITH DECREASED GLASS FIBER READ OUT 有权
    用玻璃纤维读出来制备注塑成型件的工艺

    公开(公告)号:US20120043700A1

    公开(公告)日:2012-02-23

    申请号:US13203522

    申请日:2010-02-08

    IPC分类号: B29C45/72 C08K7/14

    摘要: The present invention relates to a process for preparing an injection molded part, comprising the following steps: a preparing a glass fiber reinforced polyamide-6 composition with a relative viscosity of less than 2.4; b heating a such composition to obtain a viscous liquid; c filling a mold cavity with the viscous liquid with a filling time of at least 0.8 s; d leaving the viscous liquid in the mold under pressure until it cools to form a part; e opening the mold; f ejecting the part; wherein the polyamide-6 composition has a crystallization temperature under hyper DSC conditions of less than 168° C. The invention also relates to an injection molded part a having a maximum wall thickness of at least 2.5 mm; and/or b a part weight of at least 100 g per injection point; wherein the part consists of a glass fiber reinforced semi-crystalline polyamide-6 composition having a relative solution viscosity of less than 2.4, wherein the polyamide-6 composition has a crystallization temperature under hyper DSC conditions of less than 168° C.

    摘要翻译: 本发明涉及一种注射成型部件的制备方法,包括以下步骤:制备相对粘度小于2.4的玻璃纤维增​​强聚酰胺-6组合物; b加热这样的组合物以获得粘稠液体; c用粘稠液体填充模腔,填充时间至少为0.8s; d在压力下将粘性液体留在模具中直到其冷却以形成部件; 打开模具; f弹出零件; 其中所述聚酰胺-6组合物在超过DSC条件下的结晶温度低于168℃。本发明还涉及具有至少2.5mm的最大壁厚的注塑部分a; 和/或b每个注射点至少100g的部分重量; 其中该部分由相对溶液粘度小于2.4的玻璃纤维增​​强半结晶聚酰胺-6组合物组成,其中聚酰胺-6组合物在高DSC条件下的结晶温度小于168℃。