摘要:
An antireflective coating is disclosed. The antireflective coating includes a first high index of refraction coating layer; a first low index of refraction coating layer over the first high index of refraction coating layer; a second high index of refraction coating layer over the first low index of refraction coating layer; and a second low index of refraction coating layer over the second high index of refraction coating layer, wherein the first high index of refraction coating layer has an optical thickness defined by the following equation within a range of ±25%: [−2.1643×(optical thickness of the second low index of refraction coating layer)2]+[4.6684×(optical thickness of the second low index of refraction coating layer)]−2.2187, or the first low index of refraction coating layer has an optical thickness defined by the following equation within a range of ±25%: [2.0567×(optical thickness of the second low index of refraction coating)2]−[3.5663×(optical thickness of the second low index of refraction coating)]+1.8467, or the second high index of refraction coating layer has an optical thickness defined by the following equation within a range of ±25%: [−0.3987×(optical thickness of the second low index of refraction coating layer)2]−[1.1576×(optical thickness of the second low index of refraction coating layer)]+2.7462.
摘要:
A colorant for a high redox glass composition comprising: total iron (Fe2O3) 0 to 1.1 weight percent; and from 0.0001 to 0.15 weight percent of at least one of the following: Cu nanostructures, Au nanostructures, or Ag nanostructures, wherein the weight percents are based on the total weight of the glass composition. The colorant of the invention can be used to make glass compositions having various colors.
摘要翻译:用于高氧化还原玻璃组合物的着色剂,其包含:0-1.1重量%的总铁(Fe 2 O 3 O 3); 和0.0001至0.15重量%的以下至少一种:Cu纳米结构,Au纳米结构或Ag纳米结构,其中重量百分比基于玻璃组合物的总重量。 本发明的着色剂可用于制备具有各种颜色的玻璃组合物。
摘要:
A glass composition for chemical tempering includes oxides in wt % ranges of: SiO2 60 to 75; Al2O3 18 to 28; Li2O 3 to 9; Na2O 0 to 3; K2O 0 to 0.5; CaO 0 to 3; MgO 0 to 3; ZrO2 0 to 3; where MgO+CaO is 0 to 6 wt %; Al2O3+ZrO2 is 18 to 28 wt %, and Na2O+K2O is 0.05 to 3.00 wt %. The glass has a log 10 viscosity temperature in the temperature range of 1328° F. (720° C.) to 1499° F. (815° C.); a liquidus temperature in the temperature range of 2437° F. (1336° C.) to 2575° F. (1413° C.), and a log 7.6 softening point temperature in the temperature range of 1544° F. (840° C.) to 1724° F. (940° C.). The chemically tempered glass has, among other properties, an abraded modulus of rupture of 72 to 78 KPSI, and a modulus of rupture of 76 to 112 KPSI.
摘要翻译:用于化学回火的玻璃组合物包括重量百分比范围为:SiO 2≤60至75的氧化物; Al 2 O 3→18→28; Li 2 O 3〜9; Na 2 O 0〜3; K 2 O 0至0.5; CaO 0〜3; MgO 0〜3; ZrO 2 0〜3; 其中MgO + CaO为0至6重量%; Al 2 O 3 + ZrO 2 2为18〜28重量%,Na 2 O + K 2 为0.05〜3.00重量%。 玻璃在1328°F(720°C)至1499°F(815°C)的温度范围内具有log 10粘度温度; 温度范围为2437°F(1336°C)至2575°F(1413°C)的液相线温度,以及1544°F温度范围内的log 7.6软化点温度(840°C 。)至1724°F(940℃)。 化学强化玻璃除其他性能之外还具有72至78KPSI的磨损模数和76至112KPSI的断裂模量。
摘要:
A colorant for a high redox glass composition comprising: total iron (Fe2O3) 0 to 1.1 weight percent; and from 0.0001 to 0.15 weight percent of at least one of the following: Cu nanostructures, Au nanostructures, or Ag nanostructures, wherein the weight percents are based on the total weight of the glass composition. The colorant of the invention can be used to make glass compositions having various colors.
摘要翻译:用于高氧化还原玻璃组合物的着色剂,其包含:0-1.1重量%的总铁(Fe 2 O 3 O 3); 和0.0001至0.15重量%的以下至少一种:Cu纳米结构,Au纳米结构或Ag纳米结构,其中重量百分比基于玻璃组合物的总重量。 本发明的着色剂可用于制备具有各种颜色的玻璃组合物。
摘要:
A glass composition that includes a base glass composition including: SiO2 from 65 to 75 weight percent, Na2O from 10 to 20 weight percent, CaO from 5 to 15 weight percent, MgO from 0 to 5 weight percent, Al2O3 from 0 to 5 weight percent, K2O from 0 to 5 weight percent, and a colorant and property modifying portion including total iron ranging from of equal to or less than 0.6 weight percent; and TiO2 ranging from 0.1 to 1.0 weight percent, wherein the redox ratio ranges from 0.33 to 0.45 and the weight percents are based on the total weight of the composition.
摘要翻译:一种玻璃组合物,其包含基础玻璃组合物,其包含:65〜75重量%的SiO 2,10〜20重量%的Na 2 O 3,5〜15重量%的CaO 0至5重量%的MgO,0至5重量%的Al 2 O 3,0至5重量%的K 2 O 3, 百分比,以及包含等于或小于0.6重量%的总铁的着色剂和性能改性部分; 和TiO 2范围为0.1至1.0重量%,其中氧化还原比范围为0.33至0.45,重量百分比基于组合物的总重量。
摘要:
A glass composition for forming a blue colored glass is disclosed. The glass composition is made up of a base glass portion, iron oxide, and at least one first additive compound selected from Nd2O3 in an amount up to 1 weight percent and/or CuO in an amount up to 0.5 weight percent. The base glass portion has the following components: SiO2 from 66 to 75 weight percent; Na2O from 10 to 20 weight percent; CaO from 5 to 15 weight percent; MgO from 0 to 5 weight percent; Al2O3 from 0 to 5 weight percent; B2O3 from 0 to 5 weight percent; and K2O from 0 to 5 weight percent. The total iron in the glass composition ranges from 0.3 to 1.2 weight percent, and the glass composition has a redox ratio ranging from 0.15 to 0.65.
摘要翻译:公开了一种用于形成蓝色玻璃的玻璃组合物。 玻璃组合物由基础玻璃部分,氧化铁和至少一种选自Nd 2 O 3 N 3的第一添加剂化合物组成,其量高达1重量% 和/或CuO,其量高达0.5重量%。 基础玻璃部分具有以下组分:66至75重量%的SiO 2; Na 2 O 2为10至20重量%; CaO为5〜15重量% 0〜5重量%的MgO; 0至5重量%的Al 2 O 3 O 3; B 2 O 3 O 3从0至5重量%; 和0-2重量%的K 2 O。 玻璃组合物中的总铁量为0.3〜1.2质量%,玻璃组合物的氧化还原比为0.15〜0.65。
摘要:
A glass composition that includes a base glass composition including: SiO2 from 65 to 75 weight percent, Na2O from 10 to 20 weight percent, CaO from 5 to 15 weight percent, MgO from 0 to 5 weight percent, Al2O3 from 0 to 5 weight percent, K2O from 0 to 5 weight percent and BaO 0 to 1 weight percent, and a colorant and property modifying portion including total iron from 0.25 to 0.9 weight percent, Cr2O3 from 6 PPM to 400 PPM, Er2O3 from 0.3 to 3.0 weight percent, and TiO2 from 0.1 to 0.8 weight percent, wherein the glass composition has a redox ratio ranging from 0.15 to 0.62.
摘要翻译:一种玻璃组合物,其包含基础玻璃组合物,其包含:65〜75重量%的SiO 2,10〜20重量%的Na 2 O 3,5〜15重量%的CaO 0至5重量%的MgO,0至5重量%的Al 2 O 3,0至5重量%的K 2 O 3, 百分比和BaO 0至1重量%,以及着色剂和性能改性部分,其包含0.25至0.9重量%的总铁,6PPM至400PPM的Cr 2 O 3 ,0.3-3.0重量%的Er 2 O 3,和0.1至0.8重量百分比的TiO 2,其中玻璃组合物具有氧化还原 比值范围从0.15到0.62。
摘要:
A colorant for a high redox glass composition comprising: total iron (Fe2O3) 0 to 1.1 weight percent; and from 0.0001 to 0.15 weight percent of at least one of the following: Cu nanostructures, Au nanostructures, or Ag nanostructures, wherein the weight percents are based on the total weight of the glass composition. The colorant of the invention can be used to make glass compositions having various colors.
摘要翻译:用于高氧化还原玻璃组合物的着色剂,其包含:总铁(Fe 2 O 3)0至1.1重量% 和0.0001至0.15重量%的以下至少一种:Cu纳米结构,Au纳米结构或Ag纳米结构,其中重量百分比基于玻璃组合物的总重量。 本发明的着色剂可用于制备具有各种颜色的玻璃组合物。
摘要:
A glass composition that includes a base glass composition including: SiO2 from 65 to 75 weight percent, Na2O from 10 to 20 weight percent, CaO from 5 to 15 weight percent, MgO from 0 to 5 weight percent, Al2O3 from 0 to 5 weight percent, K2O from 0 to 5 weight percent and BaO from 0 to 1 weight percent, and a colorant and property modifying portion including total iron from 0.5 to 0.8 weight percent, Er2O3 from 0.05 to 0.5 weight percent, Se from 1 PPM to 4 PPM, and CoO from 1 PPM to 15 PPM, wherein the glass composition has a redox ratio ranging from 0.25 to 0.35.
摘要翻译:一种玻璃组合物,其包含基础玻璃组合物,其包含:65〜75重量%的SiO 2,10〜20重量%的Na 2 O 3,5〜15重量%的CaO 0至5重量%的MgO,0至5重量%的Al 2 O 3,0至5重量%的K 2 O 3, 百分比和BaO为0至1重量%,以及着色剂和性能改性部分,其包含0.5至0.8重量%的总铁,0.05至0.5重量%的Er 2 O 3 O 3 百分比,Se从1PPM至4PPM,CoO从1PPM至15PPM,其中玻璃组合物的氧化还原比范围为0.25至0.35。
摘要:
A method for modifying the appearance of a substrate is disclosed. The method includes providing a substrate having first and second opposing surfaces and depositing a reflectance modifying coating on at least a portion of the first surface of the substrate, wherein the second surface has a visible light reflectance (R1) ranging from 5 to 20 percent.