摘要:
Disclosed are hot-melt adhesives prepared from aromatic-aliphatic polyesters containing terephthalic acid in combination with adipic acid, glutaric acid, or a mixture thereof, as diacid components and a diol component containing 1,4-butanediol, 1,6-hexanediol, or a combination thereof. These adhesives set up rapidly within a well-defined temperature window. The hot-melt adhesives can be used in a variety of applications, but are especially suited as seaming adhesives for roll-applied labels. These adhesives have melting temperatures and crystallization properties that allow their application at temperatures cool enough to prevent curling and premature shrinkage of the shrink label during seaming, and yet produce strong label seams that can withstand the elevated temperatures of a shrink tunnel without sacrificing line speed. Also disclosed are labeled containers and a process for applying a roll-on, shrink label to a container using the hot-melt adhesives of the invention.
摘要:
Disclosed are hot-melt adhesives prepared from aromatic-aliphatic polyesters containing terephthalic acid in combination with adipic acid, glutaric acid, or a mixture thereof, as diacid components and a diol component containing 1,4-butanediol, 1,6-hexanediol, or a combination thereof. These adhesives set up rapidly within a well-defined temperature window. The hot-melt adhesives can be used in a variety of applications, but are especially suited as seaming adhesives for roll-applied labels. These adhesives have melting temperatures and crystallization properties that allow their application at temperatures cool enough to prevent curling and premature shrinkage of the shrink label during seaming, and yet produce strong label seams that can withstand the elevated temperatures of a shrink tunnel without sacrificing line speed. Also disclosed are labeled containers and a process for applying a roll-on, shrink label to a container using the hot-melt adhesives of the invention.
摘要:
Disclosed are hot-melt adhesives prepared from polyesters containing 1,4-cyclohexane-dicarboxylic acid as a diacid component and a diol component containing at least two diols chosen from 1,4-cyclohexanedimethanol, triethylene glycol, and diethylene glycol. These adhesives set up rapidly within a well-defined temperature window. The hot-melt adhesives can be used in a variety of applications, but are especially suited as seaming adhesives for roll-applied labels. These adhesives have melting temperatures and crystallization properties that allow their application at temperatures cool enough to prevent curling and premature shrinkage of the shrink label during seaming, and yet produce strong label seams that can withstand the elevated temperatures of a shrink tunnel without sacrificing line speed. Also disclosed are labeled containers and a process for applying a roll-on, shrink label to a container using the hot-melt adhesives of the invention.
摘要:
Disclosed are hot-melt adhesives prepared from polyesters containing 1,4-cyclohexane-dicarboxylic acid as a diacid component and a diol component containing at least two diols chosen from 1,4-cyclohexanedimethanol, triethylene glycol, and diethylene glycol. These adhesives set up rapidly within a well-defined temperature window. The hot-melt adhesives can be used in a variety of applications, but are especially suited as seaming adhesives for roll-applied labels. These adhesives have melting temperatures and crystallization properties that allow their application at temperatures cool enough to prevent curling and premature shrinkage of the shrink label during seaming, and yet produce strong label seams that can withstand the elevated temperatures of a shrink tunnel without sacrificing line speed. Also disclosed are labeled containers and a process for applying a roll-on, shrink label to a container using the hot-melt adhesives of the invention.
摘要:
Disclosed are blends of aliphatic-aromatic copolyesters with poly(ethylene-co-vinyl acetate) copolymers and shaped articles prepared therefrom. These blends have higher melt strength than the aliphatic-aromatic copolyester alone and exhibit increased melt strength and better processability. In addition, the blends and shaped articles show bio-disintegration and/or biodegradability in a composting environment.
摘要:
Disclosed are void-containing polyester shrink films which show excellent density retention upon exposures to high temperatures. The films have high shrinkage and retain their low density after processing under conditions of temperature and moisture used in typical recycling processes. The films are useful for sleeve label and other shrink film applications, and their lower density allows them to be readily separated from soft drink bottles, food containers and the like during recycling operations. Also disclosed is a process for void-containing polyester shrink films having high shrinkage and low density after exposure to elevated temperatures.
摘要:
Disclosed are void-containing polyester shrink films which show excellent density retention upon exposures to high temperatures. The films have high shrinkage and retain their low density after processing under conditions of temperature and moisture used in typical recycling processes. The films are useful for sleeve label and other shrink film applications, and their lower density allows them to be readily separated from soft drink bottles, food containers and the like during recycling operations. Also disclosed is a process for void-containing polyester shrink films having high shrinkage and low density after exposure to elevated temperatures.
摘要:
A compositional blend of from about 50 to about 99 weight percent of a polyester and from about 1 to about 50 weight percent of an essentially, linear, random aliphatic-aromatic copolyester or branched and/or chain extended copolyester thereof is useful as a heat-shrinkable film.
摘要:
A reactor grade copolyester composition, as well as a heat-shrinkable film made therefrom, unexpectedly has higher ductility than a multi-component blend of copolyesters with the same monomer concentrations. The reactor grade copolyester composition is made from a diacid component of at least about 90 mole percent and a diol component of (a) about 72 to about 88 mole percent ethylene glycol, about 10 to about 15 mole percent 1,4-cyclohexanedimethanol, and about 2 to about 13 mole percent diethylene glycol, or (b) about 59 to about 77.5 mole percent ethylene glycol, about 15 to about 28 mole percent 1,4-cyclohexane-dimethanol, and about 7.5 to about 13 mole percent diethylene glycol. Further, the heat-shrinkable film may be produced to closely match the shrink characteristics of polyvinyl chloride by varying the amounts of the diol components of the reactor grade copolyester composition. Furthermore, a reactor grade copolyester composition has a b* color value of −1.0 to less than 4.5, wherein the diacid component is at least about 90 mole percent terephthalic acid and the diol component is about 52 to about 88 mole percent ethylene glycol, about 10 to about 28 mole percent 1,4-cyclohexane-dimethanol, and about 2 to about 20 mole percent diethylene glycol.