Crosslinked pressure sensitive adhesive compositions
    1.
    发明授权
    Crosslinked pressure sensitive adhesive compositions 失效
    交联压敏粘合剂组合物

    公开(公告)号:US4069123A

    公开(公告)日:1978-01-17

    申请号:US300294

    申请日:1972-10-24

    IPC分类号: C09J133/06 C08F8/00

    摘要: Improved pressure sensitive adhesive compositions based on acrylate ester polymers and the substrates coated therewith. The improved adhesive and cohesive properties result from the addition to the polymer of specified quinone ultraviolet sensitizers and the subsequent crosslinking thereof by exposure to an ultraviolet source.

    摘要翻译: 改进的基于丙烯酸酯聚合物的压敏粘合剂组合物和其上涂覆的基材。 改进的粘合剂和内聚性质是通过加入特定的醌类紫外线敏化剂的聚合物和随后的通过暴露于紫外线源的交联而产生的。

    Removable hot melt pressure sensitive adhesive
    3.
    发明授权
    Removable hot melt pressure sensitive adhesive 失效
    可拆卸热熔压敏胶

    公开(公告)号:US4728572A

    公开(公告)日:1988-03-01

    申请号:US36618

    申请日:1987-04-10

    申请人: Irwin J. Davis

    发明人: Irwin J. Davis

    IPC分类号: C08K5/098 C09J153/02 C09J7/02

    摘要: Hot melt adhesive compositions prepared from styrene-isoprene-styrene block copolymers, a low softening point highly aliphatic resin and a metallic salt of a fatty acid exhibit a superior balance of properties in that they adhere well to a variety of substrates yet can be readily and cleanly removed when desired.

    摘要翻译: 由苯乙烯 - 异戊二烯 - 苯乙烯嵌段共聚物,低软化点高脂肪族树脂和脂肪酸的金属盐制备的热熔粘合剂组合物表现出优异的性能平衡,因为它们很好地粘附到各种基材上,但是可以容易地和 根据需要彻底清除。

    Neoprene latex contact adhesives
    5.
    发明授权
    Neoprene latex contact adhesives 失效
    氯丁橡胶胶乳接触胶

    公开(公告)号:US4342843A

    公开(公告)日:1982-08-03

    申请号:US237791

    申请日:1981-02-24

    IPC分类号: C09J111/02 C08L63/00 C08L9/10

    CPC分类号: C09J111/02

    摘要: The metal adhesion and heat and water resistance of conventional neoprene latex adhesives are improved by the addition thereto of a polyamine and an epoxy resin wherein for every 100 parts by weight of dry neoprene, the epoxy is added in an amount of 10-40 parts and the amine is added in an amount sufficient to provide 50-150% of the stoichiometric amount required to cure the epoxy.

    摘要翻译: 通过添加多胺和环氧树脂,改善了常规氯丁橡胶胶乳粘合剂的金属粘合性和耐热性和耐水性,其中对于每100重量份干氯丁橡胶,环氧树脂加入量为10-40份, 以足以提供固化环氧树脂所需化学计量的50-150%的量加入胺。

    Flexible laminates
    6.
    发明授权
    Flexible laminates 失效
    柔性层压板

    公开(公告)号:US5037700A

    公开(公告)日:1991-08-06

    申请号:US225916

    申请日:1981-01-19

    申请人: Irwin J. Davis

    发明人: Irwin J. Davis

    摘要: Flexible laminates are prepared using a room temperature curable, water-borne laminating adhesive. The adhesive consists essentially of a copolymer emulsion of an alkyl acrylate, alkyl methacrylate, styrene or vinyl ester, or mixtures thereof, and an ethylenically unsaturated carboxylic acid, and optional selected comonomers, combined with an epoxy resin emulsion and a polyfunctional amine. The flexible laminates are characterized by rapid room temperature curing, high bond strength, superior heat resistance and chemical and water resistance.

    摘要翻译: 使用室温可固化的水性层压粘合剂制备柔性层压材料。 粘合剂基本上由丙烯酸烷基酯,甲基丙烯酸烷基酯,苯乙烯或乙烯基酯,或其混合物和烯键式不饱和羧酸和任选的选择的共聚单体与环氧树脂乳液和多官能胺组合的共聚物乳液组成。 柔性层压板的特点是室温固化快,粘结强度高,耐热性优异,耐化学性和耐水性。

    Neoprene latex contact adhesives
    8.
    发明授权
    Neoprene latex contact adhesives 失效
    氯丁橡胶胶乳接触胶

    公开(公告)号:US4463110A

    公开(公告)日:1984-07-31

    申请号:US349803

    申请日:1982-02-18

    CPC分类号: C09J111/02

    摘要: The metal adhesion and heat and water resistance of conventional neoprene latex adhesives are improved by the addition thereto of a polyfunctional amine and an epoxy resin wherein for every 100 parts by weight of dry neoprene, the epoxy is added in an amount of 10-40 parts and the amine is added in an amount sufficient to provide 50-150% of the stoichiometric amount required to cure the epoxy.

    摘要翻译: 通过添加多官能胺和环氧树脂,改善了常规氯丁橡胶胶乳粘合剂的金属粘附性和耐热性和耐水性,其中对于每100重量份干氯丁橡胶,环氧树脂的加入量为10-40份 并且胺的加入量足以提供固化环氧树脂所需的化学计量量的50-150%。