Curable resin films
    1.
    发明授权
    Curable resin films 有权
    可固化树脂膜

    公开(公告)号:US08313825B2

    公开(公告)日:2012-11-20

    申请号:US12440488

    申请日:2007-09-19

    IPC分类号: H05K1/00

    摘要: A curable resin with at least one electrically conductive metal region on its surface formed by depositing on the surface a composition comprising activator, contacting the activator with a solution of a reducing agent and a solution of a metal ion, the reducing agent and metal ion undergoing chemical reaction activated by the activator to form an electrically conductive metal region on the surface, and method of forming is provided.

    摘要翻译: 在其表面上具有至少一个导电金属区域的可固化树脂,其通过在表面上沉积包含活化剂的组合物而形成,所述组合物包含活化剂,使活化剂与还原剂和经过金属离子,还原剂和金属离子的溶液的溶液接触 通过活化剂活化的化学反应在表面上形成导电金属区域,并且提供了形成方法。

    COMPOSITE MATERIAL
    2.
    发明申请
    COMPOSITE MATERIAL 有权
    复合材料

    公开(公告)号:US20100151214A1

    公开(公告)日:2010-06-17

    申请号:US12438392

    申请日:2007-08-23

    申请人: John Leslie Cawse

    发明人: John Leslie Cawse

    IPC分类号: B32B3/10 B05D5/12

    摘要: A composite material (1) comprising at least one prepreg (3), said prepreg comprising at least one polymeric resin and optionally at least one fibrous reinforcement; and a conducting ink (2) applied to at least one surface of said prepreg (3); where the conducting ink (2) has a surface tension lower than the surface energy of the at least one surface of said prepreg (3) to which the ink (2) is applied.

    摘要翻译: 一种复合材料(1),包括至少一个预浸料坯(3),所述预浸料坯包括至少一种聚合物树脂和任选的至少一种纤维增强材料; 和施加到所述预浸料坯(3)的至少一个表面的导电油墨(2); 其中导电油墨(2)的表面张力低于施加油墨(2)的所述预浸料坯(3)的至少一个表面的表面能。

    Method of making honeycomb panel structures
    3.
    发明授权
    Method of making honeycomb panel structures 有权
    制作蜂窝板结构的方法

    公开(公告)号:US06194477B1

    公开(公告)日:2001-02-27

    申请号:US09312134

    申请日:1999-05-14

    IPC分类号: C08J900

    摘要: Expanded cellular structures are formed from dense nonporous cellulose paper with an air permeance of less than 30 ml/min which cellular structure is provided with a shape retention of at least 90%. The shape stability is obtained by forming the cellular structure, spraying with an aqueous liquid and heating, the amount of liquid, time and temperature of heating being selected and sufficient to provide the desired shape retention. The minimum amount of water is at least 30 weight % of dry paper more usually at least 75% with minimum heating of 1 minute at 100° C.

    摘要翻译: 膨胀的细胞结构由致密的无孔纤维素纸形成,透气度小于30ml / min,其细胞结构具有至少90%的形状保持。 通过形成细胞结构,用水性液体喷雾和加热获得形状稳定性,选择液体的量,加热的时间和温度,并且足以提供所需的形状保持。 最少量的水是干纸的至少30重量%,更通常至少75%,在100℃下最少加热1分钟。

    Composite material
    4.
    发明授权
    Composite material 有权
    复合材料

    公开(公告)号:US08795820B2

    公开(公告)日:2014-08-05

    申请号:US12438392

    申请日:2007-08-23

    申请人: John Leslie Cawse

    发明人: John Leslie Cawse

    IPC分类号: B32B3/10

    摘要: A composite material (1) comprising at least one prepreg (3), said prepreg comprising at least one polymeric resin and optionally at least one fibrous reinforcement; and a conducting ink (2) applied to at least one surface of said prepreg (3); where the conducting ink (2) has a surface tension lower than the surface energy of the at least one surface of said prepreg (3) to which the ink (2) is applied.

    摘要翻译: 一种复合材料(1),包括至少一个预浸料坯(3),所述预浸料坯包括至少一种聚合物树脂和任选的至少一种纤维增强材料; 和施加到所述预浸料坯(3)的至少一个表面的导电油墨(2); 其中导电油墨(2)的表面张力低于施加油墨(2)的所述预浸料坯(3)的至少一个表面的表面能。

    Curing agents
    5.
    发明授权
    Curing agents 有权
    固化剂

    公开(公告)号:US6107437A

    公开(公告)日:2000-08-22

    申请号:US162074

    申请日:1998-09-28

    摘要: Curing agents for epoxy resins are provided in which an imidazole is substituted on the nitrogen atom by a long chain group. This provides greater latexing (stability) at ambient temperatures without adversely affecting curing properties at temperatures of 50.degree. C. upwards. Those components in which the chain is substituted by a hydroxy group on the 2 position are particularly preferred and are novel compounds.

    摘要翻译: 提供用于环氧树脂的固化剂,其中咪唑在氮原子上被长链基团取代。 这在环境温度下提供更好的胶乳(稳定性),而不会在50℃以上的温度下对固化性能产生不利影响。 其中链被2位上的羟基取代的那些成分是特别优选的,并且是新的化合物。