Method for Producing Methacrolein and/or Methacrylic Acid
    5.
    发明申请
    Method for Producing Methacrolein and/or Methacrylic Acid 有权
    生产甲基丙烯醛和/或甲基丙烯酸的方法

    公开(公告)号:US20090062564A1

    公开(公告)日:2009-03-05

    申请号:US12223494

    申请日:2007-03-30

    IPC分类号: C07C51/16 C07C45/29

    摘要: The present invention relates to a method for producing methacrolein and/or methacrylic acid characterized in that the catalyst filling length of a dehydration catalyst layer is 3 to 20% of the catalyst filling length of an oxidation catalyst layer in a method where raw material gas containing gaseous t-butanol is supplied to a fixed-bed multitubular reactor having a dehydration catalyst layer and an oxidation catalyst layer in this order, from the entrance for raw material gas toward the exit, to produce methacrolein and/or methacrylic acid by dehydration reaction and catalytic gas phase oxidation reaction, and the present invention can increase the conventional yield of approximately 80% to 81 to 82% even when a reaction bath temperature is relatively low (approximately 355° C.).

    摘要翻译: 本发明涉及甲基丙烯醛和/或甲基丙烯酸的制造方法,其特征在于,在含有原料气体的方法中,脱水催化剂层的催化剂填充长度为氧化催化剂层的催化剂填充长度的3〜20% 将气态叔丁醇从原料气体入口向出口依次供给具有脱水催化剂层和氧化催化剂层的固定床多管反应器,通过脱水反应生成甲基丙烯醛和/或甲基丙烯酸, 催化气相氧化反应,即使反应浴温度相对较低(约355℃),本发明也可将常规产率提高约80%至81%至82%。

    Process for producing catalyst for methacrylic acid production
    6.
    发明申请
    Process for producing catalyst for methacrylic acid production 审中-公开
    生产甲基丙烯酸催化剂的方法

    公开(公告)号:US20070010394A1

    公开(公告)日:2007-01-11

    申请号:US10558501

    申请日:2004-05-27

    IPC分类号: B01J27/24

    摘要: The object of the present invention is to provide a method for preparing a catalyst for producing methacrylic acid by subjecting methacrolein, isobutyl aldehyde or isobutyric acid to gas phase catalytic oxidation with high yield and high selectivity. A method for preparing a catalyst for producing methacrylic acid by subjecting methacrolein, isobutyl aldehyde or isobutyric acid to gas phase catalytic oxidation, the method comprising: (a) a step of blending compounds each containing any one of Mo, V, P, Cu, Cs or NH4 with water to prepare an aqueous solution or dispersion of the compounds (hereinafter referred to, both included, as a slurry); (b) a step of drying the slurry obtained in the step (a) to obtain a dried slurry; (c) a step of calcining the dried slurry obtained in..the step (b) to obtain a calcined body; (d) a step of filtering a mixture obtained by blending the calcined body obtained in the step (c) with water to separate an aqueous solution and water-insoluble matter; and (e) a step of drying the water-insoluble matter obtained in the step (d) to obtain a dried water-insoluble body.

    摘要翻译: 本发明的目的是提供一种通过以高产率和高选择性将甲基丙烯醛,异丁醛或异丁酸进行气相催化氧化来制备用于生产甲基丙烯酸的催化剂的方法。 一种通过使甲基丙烯醛,异丁醛或异丁酸进行气相催化氧化来制备甲基丙烯酸的催化剂的方法,所述方法包括:(a)将各自含有Mo,V,P,Cu, Cs或NH 4与水反应以制备化合物的水溶液或分散体(以下称为两者,均为浆料); (b)干燥步骤(a)中获得的浆料以获得干燥的浆料的步骤; (c)煅烧步骤(b)中获得的干燥浆料以获得煅烧体的步骤; (d)将通过将步骤(c)中获得的煅烧体与水混合而获得的混合物与水分离以分离水溶液和水不溶性物质的步骤; 和(e)干燥步骤(d)中获得的水不溶性物质以获得干燥的水不溶性体的步骤。