摘要:
A Ni based alloy, which consists of by mass percent, C≦0.03%, Si: 0.01 to 0.5%, Mn: 0.01 to 1.0%, P≦0.03%, S≦0.01%, Cr: not less than 20% to less than 30%, Ni: more than 40% to not more than 60%, Cu: more than 2% to not more than 5.0%, Mo: 4.0 to 10%, Al: 0.005 to 0.5% and N: more than 0.02% to not more than 0.3%, with the balance being Fe and impurities, and the expression of “0.5 Cu+Mo≧6.5” is satisfied, has excellent corrosion resistance equivalent to that of Ni based alloys having high Mo contents, such as Hastelloy C22 and Hastelloy C276, in severe corrosive environments containing reducing acids, such as hydrochloric acid and sulfuric acid, together with excellent workability. Therefore, it can be suitably used as a low-cost material for various kinds of structural members.
摘要:
A Ni based alloy, which consists of by mass percent, C≦0.03%, Si: 0.01 to 0.5%, Mn: 0.01 to 1.0%, P≦0.03%, S≦0.01%, Cr: not less than 20% to less than 30%, Ni: more than 40% to not more than 60%, Cu: more than 2% to not more than 5.0%, Mo: 4.0 to 10%, Al: 0.005 to 0.5% and N: more than 0.02% to not more than 0.3%, with the balance being Fe and impurities, and the expression of “0.5 Cu+Mo≧6.5” is satisfied, has excellent corrosion resistance equivalent to that of Ni based alloys having high Mo contents, such as Hastelloy C22 and Hastelloy C276, in severe corrosive environments containing reducing acids, such as hydrochloric acid and sulfuric acid, together with excellent workability. Therefore, it can be suitably used as a low-cost material for various kinds of structural members.
摘要:
A Ni based alloy material consists of by mass percent, C≦0.03%, Si: 0.01 to 0.5%, Mn: 0.01 to 1.0%, P≦0.03%, S≦0.01%, Cr: not less than 20% to less than 30%, Ni: more than 40% to not more than 50%, Cu: more than 2.0% to not more than 5.0%, Mo: 4.0 to 10%, Al: 0.005 to 0.5%, W: 0.1 to 10% , N: more than 0.10% to not more than 0.35%, optionally one or more elements selected from Ca≦0.01% and Mg≦0.01%, with the balance being Fe and impurities, and the formula of “0.5Cu+Mo≧6.5” is satisfied. The material has a surface hardness of a Vickers hardness of not less than 350 at 500° C., a corrosion resistance equivalent to that of Ni based alloys having high Mo contents, and excellent erosion resistance in a severe environment.
摘要:
A Ni based alloy material consists of by mass percent, C≦0.03%, Si: 0.01 to 0.5%, Mn: 0.01 to 1.0%, P≦0.03%, S≦0.01%, Cr: not less than 20% to less than 30%, Ni: more than 40% to not more than 50%, Cu: more than 2.0% to not more than 5.0%, Mo: 4.0 to 10%, Al: 0.005 to 0.5%, W: 0.1 to 10%, N: more than 0.10% to not more than 0.35%, optionally one or more elements selected from Ca≦0.01% and Mg≦0.01%, with the balance being Fe and impurities, and the formula of “0.5Cu+Mo≧6.5” is satisfied. The material has a surface hardness of a Vickers hardness of not less than 350 at 500° C., a corrosion resistance equivalent to that of Ni based alloys having high Mo contents, and excellent erosion resistance in a severe environment.
摘要:
There is provided an austenitic stainless steel for high-pressure hydrogen gas consisting, by mass percent, of C: 0.10% or less, Si: 1.0% or less, Mn: 3% or more to less than 7%, Cr: 15 to 30%, Ni: 10% or more to less than 17%, Al: 0.10% or less, N: 0.10 to 0.50%, and at least one kind of V: 0.01 to 1.0% and Nb: 0.01 to 0.50%, the balance being Fe and impurities, wherein in the impurities, the P content is 0.050% or less and the S content is 0.050% or less, the tensile strength is 800 MPa or higher, the grain size number (ASTM E112) is No. 8 or higher, and alloy carbo-nitrides having a maximum diameter of 50 to 1000 nm are contained in the number of 0.4/μm2 or larger in cross section observation.
摘要翻译:提供了一种用于高压氢气的奥氏体不锈钢,其质量百分比为C:0.10%以下,Si:1.0%以下,Mn:3%以上至小于7%,Cr:15〜 30%,Ni:10%以上至小于17%,Al:0.10%以下,N:0.10〜0.50%,V:0.01〜1.0%,Nb:0.01〜0.50%中的至少一种, 余量为Fe和杂质,其中在杂质中,P含量为0.050%以下,S含量为0.050%以下,拉伸强度为800MPa以上,粒径数(ASTM E112)为8 以上,截面观察中最大直径为50〜1000nm的合金碳氮化物的含量为0.4 / m 2以上。
摘要:
There is provided an austenitic stainless steel for high-pressure hydrogen gas consisting, by mass percent, of C: 0.10% or less, Si: 1.0% or less, Mn: 3% or more to less than 7%, Cr: 15 to 30%, Ni: 10% or more to less than 17%, Al: 0.10% or less, N: 0.10 to 0.50%, and at least one kind of V: 0.01 to 1.0% and Nb: 0.01 to 0.50%, the balance being Fe and impurities, wherein in the impurities, the P content is 0.050% or less and the S content is 0.050% or less, the tensile strength is 800 MPa or higher, the grain size number (ASTM E112) is No. 8 or higher, and alloy carbo-nitrides having a maximum diameter of 50 to 1000 nm are contained in the number of 0.4/μm2 or larger in cross section observation.
摘要:
An austenitic stainless steel, which comprises by mass percent, C: not more than 0.10%, Si: 0.01 to 1.0%, Mn: 0.01 to 2%, Cr: 16 to 18%, Ni: more than 10% to less than 14%, Mo: more than 2.0% to not more than 3.0%, N: 0.03 to 0.10%, one or more elements selected from V, Nb and Ti satisfying the following formulas (1) and (2), 0.0013≦(V/51)+(Nb/93)+(Ti/48)≦0.0025 (1), {(C/12)+(N/14)}−{(V/51)+(Nb/93)+(Ti/48)}≦0.0058 (2), wherein each element symbol in the formulas (1) and (2) represents the content (by mass %) of the element concerned, with the balance being Fe and impurities, wherein the content of P is not more than 0.04% and the content of S is not more than 0.003% among the impurities, has excellent corrosion resistance, in particular, excellent intergranular corrosion resistance. The preferable contents of Nb and Ti are not more than 0.030% and not more than 0.050%, respectively.