    摘要: A decal which is adapted to decorate bottles, containers and similar devices of the type having surfaces with high wetting angles is fabricated without the use of wax. The decal can be printed upon utilizing various inks to provide aesthetic container surfaces as for example utilized in the cosmetic industry. The decal is free of wax and consists of a carrier layer as a plastic or paper having impressed thereon a base and a release layer which typically is a suitable plastic type material. The plastic type material as secured to the base layer has imprinted thereon a suitable pattern employing an ink which can contain metallic pigments or other piggments. The printed pattern has deposited thereon an adhesive layer which is relatively thin and which layer is secured to a desired surface of the container at low temperatures. After securing the decal to the surface of the container the release and base layers are removed thereby leaving the printed matter on the surface of the container.

    摘要翻译: 在不使用蜡的情况下,制造适于装饰具有高润湿角的表面的瓶子,容器和类似装置的贴花。 可以使用各种油墨来印刷贴花以提供例如在化妆品工业中使用的美学容器表面。 贴纸不含蜡,并且由作为塑料的载体层或其上印有基底的印刷层和通常为合适的塑料型材料的剥离层组成。 固定在基层上的塑料类材料上印有采用可含有金属颜料或其它配料的油墨的合适图案。 印刷图案上沉积有相对薄的粘合剂层,并且在低温下将层固定到容器的期望表面。 在将贴花固定到容器的表面之后,释放和基层被去除,从而将印刷物留在容器的表面上。

    Prepolymerization of monomer compositions containing diethylene glycol
bis(allyl carbonate)
    9.
    发明授权
    Prepolymerization of monomer compositions containing diethylene glycol bis(allyl carbonate) 失效
    含有二甘醇双(碳酸烯丙酯)的单体组合物的预聚

    公开(公告)号:US4623708A

    公开(公告)日:1986-11-18

    申请号:US707049

    申请日:1985-03-01

    CPC分类号: C08F263/06 C08F18/24 G02B1/04

    摘要: A prepolymerization step prior to casting reduces shrinkage during polymerization of a composition containing diethylene glycol bis(allyl carbonate) with up to 40% of a vinyl ester, preferably vinyl acetate, and one or more free radical type initiators. The prepolymerization step includes adding a small amount of free radical type initiator, which may be the same or different than that used just prior to casting, and heating to a temperature higher than one hour half-lifetime temperature of the initiator. In this manner, most of the added initiator is consumed and the prepolymerization produces the highest possible conversion while preventing overpolymerization. High yield of lenses of ophthalmic quality is obtained.

    摘要翻译: 浇铸之前的预聚合步骤减少含有二乙二醇双(碳酸烯丙酯)与高达40%乙烯基酯,优选乙酸乙烯酯和一种或多种自由基型引发剂的组合物聚合期间的收缩。 预聚合步骤包括加入少量的自由基型引发剂,其可以与刚刚铸造前相同或不同,并加热至高于引发剂的1小时半衰期温度。 以这种方式,大部分添加的引发剂被消耗,并且预聚合产生最高可能的转化率,同时防止过度聚合。 获得高产量的眼科质量的镜片。