公开(公告)号:US20210139628A1
公开(公告)日:2021-05-13
申请号:US16887006
申请日:2020-05-29
Applicant: NAN YA PLASTICS CORPORATION
Inventor: TE-CHAO LIAO , SEN-HUANG HSU , CHUNG-CHI SU , CHUAN CHOU , Jui-Jung Lin
IPC: C08F283/01 , C09D167/00
Abstract: A curing agent composition and a curing agent coating formula thereof are provided. The curing agent composition includes 5 to 25 wt % of an ester group-containing amine end group adduct, 2 to 25 wt % of a C8-C22 hydrophobic saturated or unsaturated fatty amine, 2 to 25 wt % of a polyamine compound, 2 to 20 wt % of a silane compound, and 10 to 60 wt % of an ether solvent.
-
公开(公告)号:US20200270416A1
公开(公告)日:2020-08-27
申请号:US16678895
申请日:2019-11-08
Applicant: NAN YA PLASTICS CORPORATION
Inventor: TE-CHAO LIAO , CHUNG-CHI SU , Chia-Sheng Lai
Abstract: A recycled polyester fiber is provided. The recycled polyester fiber is made of a raw material by melt spinning The raw material includes 95.0 wt % to 99.99 wt % recycled polyester pellet formed from recycled bottle chip and 0.01 wt % to 5.0 wt % titanium dioxide slurry. Based on the total weight of the titanium dioxide slurry, the titanium dioxide slurry includes 20 wt % to 50 wt % bio-oil acting as carrier, 50 wt % to 80 wt % titanium dioxide powder, 0.1 wt % to 5 wt % dispersant, 0.01 wt % to 3 wt % antioxidant, and 0.001 wt % to 0.1 wt % dye.
-
公开(公告)号:US20220017771A1
公开(公告)日:2022-01-20
申请号:US17335257
申请日:2021-06-01
Applicant: NAN YA PLASTICS CORPORATION
Inventor: TE-CHAO LIAO , SEN-HUANG HSU , CHUNG-CHI SU
IPC: C09D175/04 , C09D183/04 , C09D7/47 , C09D7/45 , C09D7/43 , C09D7/65 , C09D7/63 , D06N3/14
Abstract: A water-based surface treatment agent is provided. The water-based surface treatment agent is suitable to be coated onto a surface of a synthetic leather. The water-based surface treatment agent at least includes waterborne polyurethane, silicone powder, and water. Based on 100 parts by weight of the water-based surface treatment agent, a content of the waterborne polyurethane is within 15 to 35 parts by weight, and a content of the silicone powder is within 3 to 20 parts by weight. A non-volatile matter content of the waterborne polyurethane is within a range from 20 wt % to 30 wt %. Each grain of the silicone powder has a particle size within a range from 0.2 μm to 15 μm, a specific gravity within a range from 0.9 to 1.5, a water content within a range from 0.1% to 0.5%, and a hardness (A) within a range from 30 to 90.
-
公开(公告)号:US20230126608A1
公开(公告)日:2023-04-27
申请号:US17874263
申请日:2022-07-26
Applicant: NAN YA PLASTICS CORPORATION
Inventor: TE-CHAO LIAO , JUNG-JEN CHUANG , CHUNG-CHI SU , ZHANG-JIAN HUANG
Abstract: A method for processing a waste fabric containing polyester and cotton fibers includes the following steps. The first step is providing a plurality of fabric scraps each containing polyester fibers and cotton fibers. The next step is allowing an acid catalyst aqueous solution to repeatedly contact and react with the fabric scraps at 130° C. to 160° C. in a circulation and backflow manner, so as to separate the cotton fibers from each of the fabric scraps. The last step is recycling the reacted acid catalyst aqueous solution and fabric scraps.
-
公开(公告)号:US20210122876A1
公开(公告)日:2021-04-29
申请号:US17007031
申请日:2020-08-31
Applicant: NAN YA PLASTICS CORPORATION
Inventor: TE-CHAO LIAO , SEN-HUANG HSU , CHUNG-CHI SU , CHUAN CHOU , Jui-Jung Lin
Abstract: A curing agent and method for producing the same are provided, the method includes: esterification reaction: reacting a polyhydric alcohol with a polybasic acid anhydride to obtain an ester-based emulsifier (A); chain extension reaction: reacting an ester-based emulsifier (A) with a bifunctional epoxy resin to obtain a polymer intermediate (B); and reacting the polymer intermediate (B) with a polyamine compound to obtain a curing agent (C).
-
公开(公告)号:US20230132013A1
公开(公告)日:2023-04-27
申请号:US17877827
申请日:2022-07-29
Applicant: NAN YA PLASTICS CORPORATION
Inventor: TE-CHAO LIAO , JUNG-JEN CHUANG , CHUNG-CHI SU
Abstract: A method for processing a waste fabric containing polyester and wool fibers includes the following steps. The method is to treat the waste fabric with an acid catalyst aqueous solution at 160° C. to 170° C. The wool fibers are degraded and completely separated from the polyester fibers in a treatment process. Afterwards, the polyester fibers are recycled.
-
公开(公告)号:US20220127453A1
公开(公告)日:2022-04-28
申请号:US17385918
申请日:2021-07-27
Applicant: NAN YA PLASTICS CORPORATION
Inventor: TE-CHAO LIAO , SEN-HUANG HSU , CHUNG-CHI SU
IPC: C08L67/06 , C08G63/183 , C08G63/21 , C08F12/08 , C08F220/20 , C08F222/10
Abstract: An unsaturated polyester resin composition with low styrene volatility and a molding article thereof are provided. The unsaturated polyester resin composition of includes: 30 to 60 parts by weight of unsaturated polyester resin and 2 to 30 parts by weight of comonomer, and the comonomer includes: (a) methyl styrene, (b) hydroxy acrylate monomer and (c) diallyl phthalate monomer, and the weight ratio of the content (a), (b), and (c) is 6:3:1 in the comonomer.
-
-
-
-
-
-