公开(公告)号:US12030297B2
公开(公告)日:2024-07-09
申请号:US17045816
申请日:2019-04-17
Applicant: NITTO DENKO CORPORATION
Inventor: Keisuke Sato , Takeshi Murashige , Junichi Inagaki , Atsushi Kishi
CPC classification number: B32B7/02 , B32B7/06 , B32B17/10 , B32B17/10018 , B32B17/10779 , B32B2457/202 , B32B2457/206
Abstract: Provided is a glass film-resin composite, which prevents the breakage of a glass film and enables the production of an elongated glass film. The glass film-resin composite of the present invention includes: an elongated glass film; a resin tape, which is arranged on at least one surface of the elongated glass film and is linearly arranged at least near each of both ends in a widthwise direction of the elongated glass film in one surface of the elongated glass film; a protective layer, which is arranged near each of both the ends in the widthwise direction of the surface of the elongated glass film having arranged thereon the resin tape and on an outside of the resin tape in the widthwise direction; and a resin layer arranged on one surface of the elongated glass film.
-
公开(公告)号:US12030281B2
公开(公告)日:2024-07-09
申请号:US17598357
申请日:2020-03-11
Applicant: Nitto Denko Corporation
Inventor: Keisuke Sato , Takeshi Murashige , Junichi Inagaki , Atsushi Kishi
CPC classification number: B32B17/10862 , B32B17/10 , B32B17/10018 , B32B37/0007 , B32B37/0053 , B32B37/10 , B32B37/12 , B32B37/26 , B32B2037/268 , B32B2250/05 , B32B2307/42 , B32B2457/20
Abstract: A method of manufacturing a glass resin laminated body includes a step of sticking a glass film on a resin film via an adhesive layer while holding the glass film and the resin film between a first roller that presses against the resin film and a second roller that is disposed opposite to the first roller and that presses against the glass film. A ratio of an elastic modulus P1 of a surface layer of the first roller to an elastic modulus P2 of the resin film P1/P2 satisfies a relation of 3×10−3≤P1/P2≤1.0.
-
公开(公告)号:US20230278318A1
公开(公告)日:2023-09-07
申请号:US18018982
申请日:2021-07-19
Applicant: Nitto Denko Corporation
Inventor: Takeshi Murashige , Junichi Inagaki , Keisuke Sato , Atsushi Kishi
CPC classification number: B32B17/10018 , B32B7/12 , B32B17/10862 , B32B2307/51 , B32B2307/7376 , B32B2307/546
Abstract: A multilayer structure includes one or more resin layers; and a glass layer laminated over the resin layers via bonding layers, wherein when ρ0 is a critical radius of curvature at which the glass layer does not break even though the multilayer structure being bent so that the glass layer is inside, a ratio t/ρ0 of a thickness t of the glass layer to the critical radius of curvature ρ0 is 0.001 or more and 0.02 or less.
-
公开(公告)号:US20230114553A1
公开(公告)日:2023-04-13
申请号:US17914374
申请日:2021-03-10
Applicant: NITTO DENKO CORPORATION
Inventor: Takeshi Murashige , Junichi Inagaki , Keisuke Sato , Atsushi Kishi
Abstract: A disclosed multilayer structure includes a resin layer, a glass layer laminated over the resin layer, and a tension applying portion configured to apply a tension in a direction in which the resin layer extends.
-
公开(公告)号:US20220219440A1
公开(公告)日:2022-07-14
申请号:US17442824
申请日:2020-02-10
Applicant: NITTO DENKO CORPORATION
Inventor: Junichi Inagaki , Takeshi Murashige , Keisuke Sato , Toshihiro Kanno
Abstract: Provided is a method of manufacturing a laminated film, the method including laminating a glass film and a resin film via an adhesive layer, by which peeling between the glass film and the resin film is prevented, and hence a laminated film excellent in appearance can be obtained. The method of manufacturing a laminated film of the present invention includes the steps of: laminating a glass film and a resin film via an adhesive to provide a precursor laminate; and curing the adhesive by applying an active energy ray to the precursor laminate, wherein the curing step includes nonuniformly applying the active energy ray in a surface of the precursor laminate.
-
公开(公告)号:US20220212448A1
公开(公告)日:2022-07-07
申请号:US17433398
申请日:2020-02-17
Applicant: NITTO DENKO CORPORATION
Inventor: Junichi Inagaki , Takeshi Murashige , Toshihiro Kanno
Abstract: Provided is an optical laminate in which optical defects is less likely to occur when used in an optical device such as a display. A laminate (101) includes a flexible glass film (10) having a thickness of 150 μm or less and a resin film (20) laminated on the glass film with an adhesive layer (50) interposed therebetween. The number of contaminants having a size of 100 μm or more in the adhesive layer is preferably 10/m2 or less. When the contaminants protrude from the surface of the adhesive layer (50), the height and inclination angle of protrusions is preferably small.
-
公开(公告)号:US10960610B2
公开(公告)日:2021-03-30
申请号:US16345010
申请日:2017-10-20
Applicant: NITTO DENKO CORPORATION
Inventor: Junichi Inagaki , Takeshi Murashige , Kazuhito Hosokawa , Toshihiro Kanno , Kota Nakai
Abstract: Provided is a production method for a film laminate by which a tough film can be bonded to a brittle film while the breakage of the brittle film is prevented. The production method for a film laminate of the present invention includes bonding a tough film having an elongated shape to a brittle film having an elongated shape while conveying the brittle film, wherein the method includes bonding the tough film and the brittle film to each other by bringing the tough film close to the brittle film, followed by blowing of a gas from a side of the tough film opposite to the brittle film.
-
公开(公告)号:US20180207906A1
公开(公告)日:2018-07-26
申请号:US15743414
申请日:2016-07-13
Applicant: c/o NITTO DENKO CORPORATION
Inventor: Junichi Inagaki , Takeshi Murashige , Kazuhito Hosokawa
CPC classification number: B32B7/02 , B32B7/12 , B32B17/064 , B32B17/10 , B32B27/08 , B32B2307/40 , C03B17/00 , C03B17/06 , C03B35/00 , H01L51/50 , H05B33/04
Abstract: Provided is a production method for an optical laminate, which is excellent in production efficiency even through use of a thin glass. The production method for an optical laminate includes: a thin glass production step of producing a thin glass having a thickness of 100 μm or less; and a lamination step of laminating an optical film on one surface, or each of both surfaces, of the thin glass, the thin glass production step and the lamination step being performed in an integrated line, the lamination step including applying an adhesive onto the optical film to form an application layer, and bonding the thin glass and the optical film through intermediation of the application layer, followed by curing the adhesive to form an adhesive layer between the optical film and the thin glass.
-
公开(公告)号:US12215972B2
公开(公告)日:2025-02-04
申请号:US17424429
申请日:2020-02-10
Applicant: NITTO DENKO CORPORATION
Inventor: Junichi Inagaki , Takeshi Murashige , Keisuke Sato
Abstract: Provided is a sensor device in which the sensitivity of a strain sensor is hardly inhibited despite the fact that a glass material is used as a protective material, and in which the glass material hardly breaks. The sensor device of the present invention includes: an optical laminate including a glass film, an adhesive layer, a resin layer, and a pressure-sensitive adhesive layer in the stated order; and a strain-sensing unit, wherein the glass film has a thickness of from 20 μm to 150 μm. In one embodiment, the strain-sensing unit is arranged on a pressure-sensitive adhesive layer side of the optical laminate.
-
公开(公告)号:US11639046B2
公开(公告)日:2023-05-02
申请号:US17045821
申请日:2019-04-17
Applicant: NITTO DENKO CORPORATION
Inventor: Takeshi Murashige , Junichi Inagaki , Atsushi Kishi , Kota Nakai , Toshihiro Kanno
Abstract: Provided is a glass film-resin composite, which prevents the breakage of a glass film and enables the production of an elongated glass film. The glass film-resin composite of the present invention includes: an elongated glass film; and a resin tape arranged on at least one surface of the elongated glass film, wherein the resin tape is linearly arranged at least near each of both ends in a widthwise direction of the elongated glass film in one surface of the elongated glass film, and wherein the resin tape includes an adhesive layer, and the adhesive layer is directly arranged on the elongated glass film.
-
-
-
-
-
-
-
-
-